Resin Technology Group UV-412 Medium Viscosity, High Clarity, UV Curable Adhesive

Category Polymer , Adhesive , Thermoset
Manufacturer Resin Technology Group
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Resin Technology Group UV-412 Medium Viscosity, High Clarity, UV Curable Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
UV 412 is a high clarity, fast setting UV adhesive. This solvent free adhesive is designed to bond a wide variety of transparent materials, (similar and dissimilar substrates). The high clarity provides an invisible bondline. UV 412 performs well in many glass coating and encapsulation applications and has outstanding moisture resistance.Applications: Glass to metal, Lens bonding, Glass repair, Fiber optic bonding, Medical devices, Window assembly.Processing: UV light cure: Intensity of 200 mw/cm2; Spectral output of 300 to 500 nanometers; Optimum wavelength of 375 nanometersRecommended Aurora UV light sources:Aurora 455-S 5x5 High Intensity FloodAurora 461-S 1x6 High Intensity BeamAurora 100-S Spot Light GuideInformation provided by Resin Technology Group.
Physical Properties Metric English Comments
Water Absorption 0.80 %
0.80 %
Cured
Viscosity 4200 - 5800 cP

@Temperature 25.0 °C
4200 - 5800 cP

@Temperature 77.0 °F
Uncured
Thickness <= 12700 microns
<= 500 mil
Cured film
Mechanical Properties Metric English Comments
Hardness, Shore D 85
85
Cured
Tensile Strength at Break 46.9 MPa
6800 psi
Cured
Elongation at Break 22 %
22 %
Cured
Thermal Properties Metric English Comments
Flash Point >= 93.3 °C
>= 200 °F
Uncured
Optical Properties Metric English Comments
Transmission, Visible 80 %
80 %
Mfr. Specifies clear but does not quantify
Electrical Properties Metric English Comments
Surface Resistance 1.20e+15 ohm
1.20e+15 ohm
Cured
Dielectric Strength 16.5 kV/mm
420 kV/in
Cured
Descriptive Properties Value Comments
Color Clear
Composition Urethane Oligomer/ (Meth) Acrylate Monomer Blend
Solubility Isopropyl Alcohol, Chlorinated solvents
Toxicity Low