Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 77.0 °C | 171 °F | ISO 11357-3 |
Total Evatane® 24 - 03 HDPE vinyl acetate copolymer, blown film, injection molding
(discontinued **) EVA Copolymer made by high pressure tubular process. Temperature profile (°C) for injection molding: 130 to 160.Information provided provided by Total Petrochemicals.Total Petrochemicals includes f.. |
|||
Melting Point | 77.0 °C | 171 °F | Exxon Method |
ExxonMobil Escorene® LD-737 EVA Copolymer for Specialty Applications
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 19.5% vinyl acetate copolymer.Applications: Compound viscosity modifier; High flow applications. |
|||
Melting Point | 77.0 °C | 171 °F | Exxon Method |
ExxonMobil Escorene® LD-740 High EVA Film and Compounding Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A high vinyl acetate copolymer resin for specialty film and compounding applications. Outstanding heat sealability along with excellent strength pr.. |
|||
Melting Point | 77.0 - 82.0 °C | 171 - 180 °F | |
Indium Corp. Indalloy 28 Bismuth Solder Alloy Information Provided by Indium Corporation |
|||
Melting Point | 77.0 °C | 171 °F | Freezing Point via DSC/ASTM D3418 |
DuPont Elvax® 3135SB Ethylene-Vinyl Acetate Copolymer Resin for Blown Film 12 wt% Vinyl Acetate.Elvax® 3135SB is an extrudable ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene resi.. |
|||
Melting Point | 77.0 °C | 171 °F | Freezing Point; DSC; ASTM-D3418 |
Westlake EF532 12% EVA Copolymer (Experimental Product) Westlake EF532 resin is a 12.0% EVA copolymer designed for use as a sealant / lamination layer in monolayer or coextruded flexible film structures. It has very low seal initiation temperature, excel.. |
|||
Melting Point | 77.0 °C | 171 °F | Freezing Point |
Westlake Elevate™ DA532 Ethylene Vinyl Acetate Copolymer Experimental ProductDescription: Westlake DA532 resin is a 12.0% EVA copolymer designed for use as a sealant / lamination layer in monolayer or coextruded flexible film structures. It has very low .. |
|||
Melting Point | 77.0 °C | 171 °F | by DSC; ASTM D3418 |
Westlake EMAC® SP2260 24% Ethylene-Methyl Acrylate Copolymer Westlake EMAC® SP2260 is a 24% EMA copolymer designed for blown or cast film, tie-layers, and extrusions where flexibility, compatibility, or low heat seal temperatures are required. SP2260 provide.. |
|||
Melting Point | 77.0 °C | 171 °F | Upon Melting via DSC/ASTM D3418 |
DuPont Elvax® 3190 Ethylene-Vinyl Acetate Copolymer Resin for Coextrusion 25 wt% Vinyl Acetate.Elvax® 3190 is an extrudable ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene resins.. |
|||
Melting Point | 77.0 °C | 171 °F | Freezing Point; ASTM D3418 |
DuPont™ Bynel® 30E783 Anhydride Modified Ethylene Vinyl Acetate BYNEL® Series 3000 resins are anhydride-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process p.. |
|||
Melting Point | 77.2 °C | 171 °F | Peak Melting Temperature; ExxonMobil Method |
ExxonMobil OPTEMA™ TC 120 Molding Ethylene Methyl Acrylate Product Description: Optema TC 120 is an ethylene methyl acrylate copolymer, which can be used as an impact modifier or compatibilizer in polymer compounds. TC 120 has been processed on typical LDPE.. |
|||
Melting Point | 77.2 °C | 171 °F | Dow Method (DSC) |
Dow Primacor® 5986 Ethylene acrylic acid copolymer Low heat seal temperature High gloss, excellent clarity Excellent grease and oil resistance and excellent product resistance for flexible packaging applications Complies with U.S. FDA 21 CFR 177.131.. |
|||
Melting Point | 77.0 °C | 171 °F | D.S.C. method |
Arkema Group Orevac® 9304 Film EVA-MAH Terpolymer EVA Terpolymers based Main Applications: Extrusion coating Thermo-adhesive filmsInformation provided by Arkema Group |
|||
Melting Point | 77.0 °C | 171 °F | ASTM-D3418 |
Braskem Evateno® HM 728 EVA Hot Melt Copolymer Evateno® HM 728 is a copolymer of Ethylene-Vinyl Acetate (EVA) with high vinyl-acetate content, medium molecular weight, and good compatibility with other thermoplastic and elastomeric resins. Evat.. |
|||
Melting Point | 77.0 °C | 171 °F | DSC |
Arkema Group LOTADER® 4403 Terpolymer Ethylene - Acrylic Ester - Maleic Anhydride LOTADER 4403 is a random terpolymer of Ethylene, Acrylic Ester and Maleic Anhydride, polymerized by high pressure autoclave process. LOTADER 4403 is a versatile adhesive for extrusion lamination, de.. |
|||
Melting Point | 77.0 - 78.0 °C | 171 - 172 °F | |
BASF 2-Ethyl Imidazole Formula: C5H8N2CAS: 1072-62-4Description: 2-Ethyl Imidazole is a colorless to yellowish solid with an amine-like odor.Synonyms: 2EIApplications: It is used as a Pharmaceuticals, Crop protection agen.. |
|||
Melting Point | 77.0 °C | 171 °F | Freezing point via DSC/ASTM D3418 |
DuPont Bynel® 20E482 Acid-Modified Ethylene Terpolymer Adhesive Resin
(discontinued **) Bynel® Series 2000 resins are acid-modified ethylene terpolymers with medium to high acid comonomer contents. They contain a temperature stable ester that makes them functional in high-temperature .. |
|||
Melting Point | 77.0 °C | 171 °F | Freezing Point; ASTM D3417 |
DuPont Elvax® 3135B Ethylene Vinyl Acetate
(discontinued **) DuPont™ Elvax® 3135B is an extrudable ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene resins. Additive:.. |
|||
Melting Point | 77.0 °C | 171 °F | Upon Melting via DSC/ASTM D3418 |
DuPont Elvax® 3190LG Ethylene-Vinyl Acetate Copolymer Resin for Coextrusion
(discontinued **) 25 wt% Vinyl Acetate.Elvax® 3190 is an extrudable ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene resins.. |