Teknor Apex APEX® 6500-70 Polyvinyl Chloride, Flexible

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Flexible Grade , PVC, Wire and Cable Grade
Manufacturer Teknor Apex Company
Trade Name APEX®
Port Ningbo port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Teknor Apex APEX® 6500-70 Polyvinyl Chloride, Flexible.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Notes: 60°C General Purpose; RoHS Compliant Uses: Connectors; Grommets; Plugs; Strain ReliefsForms: Pellets Processing Method: Injection Molding Agency Ratings: UL QMFZ2 .E54709 Wire Types: Molded Components Additional Information: Temperature Rating: 60°CInformation Provided by Teknor Apex
Physical Properties Metric English Comments
Specific Gravity 1.19 g/cc
1.19 g/cc
ASTM D792
Linear Mold Shrinkage 0.015 - 0.018 cm/cm
0.015 - 0.018 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Shore A 70
70
15 seconds; ASTM D2240
Tensile Strength at Break 13.1 MPa
1900 psi
ASTM D638
Elongation at Break 450 %
450 %
ASTM D638
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 60.0 °C
140 °F
Continuous Use; ASTM D794
UL RTI, Electrical 50.0 °C

@Thickness 1.50 mm
122 °F

@Thickness 0.0591 in
UL 746
UL RTI, Mechanical with Impact 50.0 °C

@Thickness 1.50 mm
122 °F

@Thickness 0.0591 in
UL 746
UL RTI, Mechanical without Impact 50.0 °C

@Thickness 1.50 mm
122 °F

@Thickness 0.0591 in
UL 746
Flammability, UL94 HB

@Thickness 1.50 mm
HB

@Thickness 0.0591 in
Processing Properties Metric English Comments
Melt Temperature 174 °C
345 °F
Processing Temperature
Descriptive Properties Value Comments
Appearance Clear/Transparent