Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 174 - 182 °C | 345 - 360 °F | |
PolyOne Geon™ Vinyl Wire & Cable 1604-xx07FRD Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Melt Temperature | 174 - 182 °C | 345 - 360 °F | |
PolyOne Geon™ Vinyl Wire & Cable EHB400A Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Melt Temperature | 174 - 182 °C | 345 - 360 °F | |
PolyOne Geon™ Vinyl Wire & Cable JJC32A Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Melt Temperature | 174 - 193 °C | 345 - 379 °F | |
PolyOne Geon™ HTX Ultra LA426 Black 2880 Polyvinyl Chloride Alloy (PVC Alloy) Recommend drying material for a minimum of 2 hours at 160 degrees Farenheit. Physical properties measured on LA426 Black 2880.Information provided by PolyOne |
|||
Melt Temperature | 174 - 193 °C | 345 - 379 °F | |
PolyOne Geon™ HTX Ultra LA426G Black 2880 Polyvinyl Chloride Alloy (PVC Alloy) Higher gloss version of Geon HTX Ultra LA426Recommend drying material for a minimum of 2 hours at 160 degrees Farenheit. Physical properties measured on LA426G Black 2880.Information provided by Pol.. |
|||
Melt Temperature | 174 - 193 °C | 345 - 379 °F | |
PolyOne Geon™ HTX Ultra LA436G Black 2880 Polyvinyl Chloride Alloy (PVC Alloy) Higher gloss, wider processing window version of Geon HTX Ultra LA426G.Recommend drying material for a minimum of 2 hours at 160 degrees Farenheit. Physical properties measured on LA436G Black 2880... |
|||
Melt Temperature | 174 - 179 °C | 345 - 354 °F | |
PolyOne Geon™ Vinyl Flexible 1351 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 174 - 179 °C | 345 - 354 °F | |
PolyOne Geon™ Vinyl Flexible A75G0 Polyvinyl Chloride, Flexible (PVC, Flexible) Recommended for interior applications.Information provided by PolyOne |
|||
Melt Temperature | 174 - 179 °C | 345 - 354 °F | |
PolyOne Geon™ Vinyl Flexible C75A0 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 174 - 179 °C | 345 - 354 °F | |
PolyOne Geon™ Vinyl Flexible R158AE Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 174 - 179 °C | 345 - 354 °F | |
PolyOne Geon™ Vinyl Flexible R313AE Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 174 - 185 °C | 345 - 365 °F | |
Huntsman PE 1302 EVA Film Extrusion
(discontinued **) 3% Vinyl Acetate EVA copolymer and FDA compliantFeatures: High clarity film with good low temperature toughness and heat seal characteristics.Applications: Film extrusion: food packaging, general pu.. |
|||
Melt Temperature | 174 - 185 °C | 345 - 365 °F | |
Sylvin Technologies 9077-95 LMW Natural PVC for Injection Molding Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 174 - 185 °C | 345 - 365 °F | |
Sylvin Technologies 916V0-95 Natural PVC for Injection Molding Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 174 - 185 °C | 345 - 365 °F | |
Sylvin Technologies 9950-95 Natural PVC Molding Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 174 - 185 °C | 345 - 365 °F | |
Sylvin Technologies 9999-95 Natural PVC Molding Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 174 °C | 345 °F | |
Teknor Apex APEX® 157-V Polyvinyl Chloride, Flexible Notes: 105°C Jacket; RoHS Compliant Features: Low to no Migration; Oil Resistant; Good UV Resistance; Sunlight Resistant (720 hours) Uses: Flexible Cord Jacketing; Wire and Cable ApplicationsForm.. |
|||
Melt Temperature | 174 °C | 345 °F | |
Teknor Apex APEX® 157V-4 Polyvinyl Chloride, Flexible Notes: 105°C Jacket; RoHS Compliant Features: Low to no Migration; Oil Resistant; Good UV Resistance; Sunlight Resistant (720 hours) Uses: Flexible Cord Jacketing; Wire and Cable Applications; Au.. |
|||
Melt Temperature | 174 °C | 345 °F | |
Teknor Apex APEX® 3201-70 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMUses-Automotive Applications, Non-specific Food Applications, General Purpose, Medical Applications, Modeling.. |
|||
Melt Temperature | 174 °C | 345 °F | |
Teknor Apex APEX® 3202-70 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMUses-Caps, Closure, Connectors, Food Service Applications, Safety Equipment, Valves/Valve Parts Appearance-Cl.. |
|||
Melt Temperature | 174 °C | 345 °F | |
Teknor Apex APEX® 3310-70 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-Sterilizable, RadiationUses-Automotive Applications, Food Service Applications, General Purpose, Med.. |
|||
Melt Temperature | 174 °C | 345 °F | |
Teknor Apex APEX® 90-A41R-70-NT Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Uses- Medical Applications, Tubing, Appearance-ClearForms-PelletsProcessing-ExtrusionInformation provided by.. |
|||
Melt Temperature | 174 °C | 345 °F | |
Teknor Apex APEX® 90-A472R-70-NT Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMUses-Medical Applications, Caps, Closures, Valves/Valve Parts Appearance-ClearForms-PelletsProcessing Method-.. |
|||
Melt Temperature | 174 °C | 345 °F | Processing Temperature |
Teknor Apex APEX® 1002 Polyvinyl Chloride, Flexible Notes: 60°C General Purpose; RoHS Compliant Uses: Connectors; Grommets; Plugs; Strain ReliefsForms: Pellets Processing Method: Injection Molding Agency Ratings: UL QMFZ2 .E54709 Wire Types: Molde.. |
|||
Melt Temperature | 174 °C | 345 °F | Processing Temperature |
Teknor Apex APEX® 6500-75 Polyvinyl Chloride, Flexible Notes: 60°C General Purpose; RoHS Compliant Uses: Connectors; Grommets; Plugs; Strain ReliefsForms: Pellets Processing Method: Injection Molding Agency Ratings: UL QMFZ2 .E54709 Wire Types: Molde.. |
|||
Melt Temperature | 174 °C | 345 °F | |
Axiall 2010 Wire & Cable Flexible PVC General purpose insulation and jacketing compound recommended for 75°C applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Melt Temperature | 174 - 182 °C | 345 - 360 °F | |
PolyOne Geon™ Vinyl Wire & Cable 0953-xx04D Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Melt Temperature | 174 - 179 °C | 345 - 354 °F | |
PolyOne Geon™ Vinyl Wire & Cable W1100L-xx92FRDA Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications. Provisional Product Information - Physical and Mechanical properties based on initial production.Information provide.. |
|||
Melt Temperature | 174 °C | 345 °F | |
Axiall 491 Wire & Cable Flexible PVC 60°C rated low temperature jacketing compound.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Melt Temperature | 174 - 185 °C | 345 - 365 °F | |
Sylvin Technologies 9604-95 LMW Clear PVC for Injection Molding Information provided by Sylvin Technologies Inc. |