Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 174 - 179 °C | 345 - 354 °F | |
PolyOne Geon™ Vinyl Wire & Cable 1802-xx05FRD Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Melt Temperature | 174 - 179 °C | 345 - 354 °F | |
PolyOne Geon™ Vinyl Wire & Cable 1802-xx17FRD Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Melt Temperature | 174 - 182 °C | 345 - 360 °F | |
PolyOne Geon™ Vinyl Wire & Cable JAL110A Natural Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 174 - 182 °C | 345 - 360 °F | |
PolyOne Geon™ Vinyl Wire & Cable JJC32A Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Melt Temperature | 174 - 182 °C | 345 - 360 °F | |
PolyOne Geon™ Vinyl Wire & Cable W1604L-xx07FRD Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications. Provisional Product Information - Physical and Mechanical properties based on initial production.Information provide.. |
|||
Melt Temperature | 174 - 193 °C | 345 - 379 °F | |
PolyOne Geon™ HTX Ultra LA426 Gray 2382 Polyvinyl Chloride Alloy (PVC Alloy) Optimum for Black and Darker Colors between 50 and 70 L value. Also suitable for colors above 70 L value.Recommend drying material for a minimum of 2 hours at 160 degrees Farenheit. Physical propert.. |
|||
Melt Temperature | 174 - 193 °C | 345 - 379 °F | |
PolyOne Geon™ HTX Ultra LA426G Black 2880 Polyvinyl Chloride Alloy (PVC Alloy) Higher gloss version of Geon HTX Ultra LA426Recommend drying material for a minimum of 2 hours at 160 degrees Farenheit. Physical properties measured on LA426G Black 2880.Information provided by Pol.. |
|||
Melt Temperature | 174 - 179 °C | 345 - 354 °F | |
PolyOne Geon™ Vinyl Flexible A65M0 Polyvinyl Chloride, Flexible (PVC, Flexible) Recommended for interior applications.Information provided by PolyOne |
|||
Melt Temperature | 174 - 179 °C | 345 - 354 °F | |
PolyOne Geon™ Vinyl Flexible A8501 Polyvinyl Chloride, Flexible (PVC, Flexible) Recommended for interior applications.Information provided by PolyOne |
|||
Melt Temperature | 174 - 185 °C | 345 - 365 °F | |
PolyOne Geon™ Vinyl Flexible B9WF1 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 174 - 179 °C | 345 - 354 °F | |
PolyOne Geon™ Vinyl Flexible C8002 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 174 - 179 °C | 345 - 354 °F | |
PolyOne Geon™ Vinyl Flexible D7500 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 174 - 179 °C | 345 - 354 °F | |
PolyOne Geon™ Vinyl Flexible D8500 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 174 - 179 °C | 345 - 354 °F | |
PolyOne Geon™ Vinyl Flexible A80U0 Polyvinyl Chloride, Flexible (PVC, Flexible) Recommended for interior applications.Information provided by PolyOne |
|||
Melt Temperature | 174 - 179 °C | 345 - 354 °F | |
PolyOne Geon™ Vinyl Flexible B80MB Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 174 - 179 °C | 345 - 354 °F | |
PolyOne Geon™ Vinyl Flexible R158AE Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 174 - 179 °C | 345 - 354 °F | |
PolyOne Geon™ Vinyl Flexible R313AE Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 174 - 179 °C | 345 - 354 °F | |
PolyOne Geon™ Vinyl Flexible R4294Y Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 174 - 185 °C | 345 - 365 °F | |
Sylvin Technologies 9077-95 LMW Natural PVC for Injection Molding Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 174 - 185 °C | 345 - 365 °F | |
Sylvin Technologies 9915-95 Natural PVC Molding Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 174 - 185 °C | 345 - 365 °F | |
Sylvin Technologies 9925-95 Natural PVC Molding Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 174 - 185 °C | 345 - 365 °F | |
Sylvin Technologies 9940-95 Natural PVC Molding Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 174 - 185 °C | 345 - 365 °F | |
Sylvin Technologies 9950-95 Natural PVC Molding Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 174 °C | 345 °F | |
Teknor Apex APEX® 3201-70 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMUses-Automotive Applications, Non-specific Food Applications, General Purpose, Medical Applications, Modeling.. |
|||
Melt Temperature | 174 °C | 345 °F | |
Teknor Apex APEX® 3202-70 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMUses-Caps, Closure, Connectors, Food Service Applications, Safety Equipment, Valves/Valve Parts Appearance-Cl.. |
|||
Melt Temperature | 174 °C | 345 °F | |
Teknor Apex APEX® 3301-70 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Uses-Automotive Applications, Food Service Applications, General Purpose, Medical Applications, Profiles, To.. |
|||
Melt Temperature | 174 °C | 345 °F | Processing Temperature |
Teknor Apex APEX® 7500-70 Polyvinyl Chloride, Flexible Notes: 105°C General Purpose; RoHS Compliant Features: High Heat Resistance Uses: Connectors; Grommets; Plugs; Strain ReliefsForms: Pellets Processing Method: Injection Molding Agency Ratings: UL.. |
|||
Melt Temperature | 174 °C | 345 °F | |
Teknor Apex APEX® 85-J644-H Polyvinyl Chloride, Flexible Notes: 105°C Jacket; RoHS Compliant Features: Flame Retardant; High Heat Resistance; Low gloss Uses: Communication Wire Jacketing; Patch Cord Jacketing Forms: Pellets Agency Ratings: NEC Article .. |
|||
Melt Temperature | 174 °C | 345 °F | Processing Temperature |
Teknor Apex APEX® 6500-75 Polyvinyl Chloride, Flexible Notes: 60°C General Purpose; RoHS Compliant Uses: Connectors; Grommets; Plugs; Strain ReliefsForms: Pellets Processing Method: Injection Molding Agency Ratings: UL QMFZ2 .E54709 Wire Types: Molde.. |
|||
Melt Temperature | 174 °C | 345 °F | |
Axiall 8863 Moldings & Extrusions Flexible PVC A vinyl elastomer extrusion compound with rubber-like properties. Ideally suited for extruded profiles and tubings. Meets the requirements for LP Gas hose per UL21.Information provided by Georgia .. |