ATI Allegheny Ludlum Stainless Steel Chromium-Nickel-Molybdenum 317LX™ (UNS S31725)

Category Metal , Ferrous Metal , Stainless Steel , T 300 Series Stainless Steel
Manufacturer ATI Allegheny Ludlum
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ATI Allegheny Ludlum Stainless Steel Chromium-Nickel-Molybdenum 317LX™ (UNS S31725).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Allegheny Ludlum's 317LX™ is molybdenum-bearing austenitic stainless steel with greatly increased resistance to chemical attack as compared to the conventional chromium-nickel austenitic stainless steels such as Type 304. AL 317LX™ alloy also offers higher creep, stress-to-rupture, and tensile strength at elevated temperatures than conventional stainless steels. The alloy has low carbon to provide resistance to sensitization during welding and other thermal processes. Increased levels of molybdenum enhance resistance to pitting and crevice corrosion especially in process steams containing acids, chlorides and sulfur compounds at elevated temperatures. This alloy is intended for severe service conditions such as flue gas desulfurization (FGD) systems.Information provided by Allegheny Ludlum Corporation.
Physical Properties Metric English Comments
Density 8.00 g/cc
0.289 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate >= 515 MPa
>= 74700 psi
ASTM A240
Tensile Strength, Yield >= 205 MPa
>= 29700 psi
ASTM A240
Elongation at Break >= 40 %
>= 40 %
ASTM A240
Modulus of Elasticity 200 GPa
29000 ksi
Thermal Properties Metric English Comments
CTE, linear 16.5 µm/m-°C

@Temperature 25.0 - 100 °C
9.17 µin/in-°F

@Temperature 77.0 - 212 °F
18.2 µm/m-°C

@Temperature 25.0 - 500 °C
10.1 µin/in-°F

@Temperature 77.0 - 932 °F
19.5 µm/m-°C

@Temperature 25.0 - 1000 °C
10.8 µin/in-°F

@Temperature 77.0 - 1830 °F
Specific Heat Capacity 0.460 J/g-°C
0.110 BTU/lb-°F
Thermal Conductivity 14.6 W/m-K
101 BTU-in/hr-ft²-°F
Melting Point 1320 - 1400 °C
2410 - 2550 °F
Solidus 1320 °C
2410 °F
Liquidus 1400 °C
2550 °F
Maximum Service Temperature, Air 899 °C
1650 °F
oxidation resistance is excellent and low scaling rate at this temp
Component Elements Properties Metric English Comments
Carbon, C <= 0.030 %
<= 0.030 %
Chromium, Cr 18 - 20 %
18 - 20 %
Iron, Fe 60 %
60 %
as balance
Manganese, Mn <= 2.0 %
<= 2.0 %
Molybdenum, Mo 4.0 - 5.0 %
4.0 - 5.0 %
Nickel, Ni 13.5 - 17.5 %
13.5 - 17.5 %
Nitrogen, N <= 0.10 %
<= 0.10 %
Phosphorous, P <= 0.040 %
<= 0.040 %
Silicon, Si <= 0.75 %
<= 0.75 %
Sulfur, S <= 0.030 %
<= 0.030 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.0000790 ohm-cm
0.0000790 ohm-cm
Magnetic Permeability 1.0028
1.0028
fully annealed 0.5" plate; 1.0028 65% cold-worked 0.5" plate