Techmer ES Plaslube® J-4/30/TF/15 Nylon 612, 30% GFR, 15% PTFE

Category Polymer , Thermoplastic , Nylon , Nylon 612 , Nylon 612, Glass Fiber Filler
Manufacturer Techmer ES
Trade Name Plaslube®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Techmer ES Plaslube® J-4/30/TF/15 Nylon 612, 30% GFR, 15% PTFE.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Plaslube glass fiber reinforced polytetrafluoroethylene (PTFE) lubricated nylon 612 grades offer a unique balance of excellent wear and friction performance with good dimensional stability and mechanical strength. These characteristics are typical of gear train, pulley, and other bearing applications. Further wear and friction performance can be achieved by utilizing both PTFE and silicone. For less dimensionally critical applications, our nylon 6 grades offer similar performance characteristics.
Physical Properties Metric English Comments
Density 1.45 g/cc
0.0524 lb/in³
ASTM D792
Water Absorption 0.13 %
0.13 %
24 hrs. ASTM D570
Linear Mold Shrinkage 0.0020 cm/cm

@Thickness 3.17 mm
0.0020 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 138 MPa
20000 psi
ASTM D638
Flexural Yield Strength 214 MPa
31000 psi
ASTM D790
Flexural Modulus 8.27 GPa
1200 ksi
ASTM D790
Izod Impact, Notched 1.60 J/cm

@Thickness 3.17 mm
3.00 ft-lb/in

@Thickness 0.125 in
ASTM D256
Coefficient of Friction, Dynamic 0.25
0.25
Coefficient of Friction, Static 0.20
0.20
K (wear) Factor 141 x 10-8 mm³/N-M
70.0 x 10-10 in³-min/ft-lb-hr
Thrust washer at 2000 PV
Limiting Pressure Velocity 0.701 MPa-m/sec
20000 psi-ft/min
at 100 FPM, ambient temperature, thrust washer.
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 199 °C
390 °F
ASTM D648