Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Limiting Pressure Velocity | 0.7006 MPa-m/sec | 20000 psi-ft/min | 4:1 safety factor; QTM 55007 |
Quadrant EPP Fluorosint® HPV Mica-filled PTFE (ASTM Product Data Sheet) |
|||
Limiting Pressure Velocity | 0.701 MPa-m/sec | 20000 psi-ft/min | 4:1 safety factor; QTM 55007 |
Quadrant EPP Ketron® HPV PEEK High Pressure Velocity Polyetherether Ketone (ASTM Product Data Sheet) This bearing grade of extruded Ketron PEEK offers the lowest coefficient of friction and best machinability of all Ketron grades. It is ideal for low wear, high PV parts that require chemical resis.. |
|||
Limiting Pressure Velocity | 0.701 MPa-m/sec | 20000 psi-ft/min | 4:1 safety factor; QTM 55007 |
Quadrant EPP Duratron® PAI T5530 Compression Molded Glass Reinforced Polyamide-imide (ASTM Product Data Sheet) |
|||
Limiting Pressure Velocity | 0.701 MPa-m/sec | 20000 psi-ft/min | 100 fpm |
Techmer ES Luriblend® PA6/6 GF30 TL15 BK 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 30% Filler by WeightAdditive: Heat Stabilizer and PTFE Lubricant(15%)Features: Lubricated, Good Wear Resistance, Low Frict.. |
|||
Limiting Pressure Velocity | 0.701 MPa-m/sec | 20000 psi-ft/min | 100 fpm |
Techmer ES Luriblend® PA6/6 GF30 TL15 UV 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 30% Filler by WeightAdditive: Heat Stabilizer, UV Stabilizer and PTFE Lubricant(15%)Features: Lubricated, Good Wear Resist.. |
|||
Limiting Pressure Velocity | 0.701 MPa-m/sec | 20000 psi-ft/min | 100 fpm |
Techmer ES Luriblend® PA6/6 GF30 TL5 LE 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 30% Filler by WeightAdditive: PTFE Lubricant(15%)Features: Lubricated, Good Wear Resistance, Low Friction and Low Extracta.. |
|||
Limiting Pressure Velocity | 0.701 MPa-m/sec | 20000 psi-ft/min | 100 fpm |
Techmer ES Luriblend® PA6/6 GF33 TL15 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 33% Filler by WeightAdditive: Heat Stabilizer and PTFE Lubricant(15%)Features: Lubricated, Good Wear Resistance, Heat Stab.. |
|||
Limiting Pressure Velocity | 0.701 MPa-m/sec | 20000 psi-ft/min | at 100 FPM, ambient temperature, thrust washer. |
Techmer ES Plaslube® J-1850/30/TF/15 PBT, 30% GFR, 15% PTFE |
|||
Limiting Pressure Velocity | 0.701 MPa-m/sec | 20000 psi-ft/min | at 100 FPM, ambient temperature, thrust washer. |
Techmer ES Plaslube® J-3/30/TF/15 Nylon 6, 30% GFR, 15% PTFE Plaslube glass fiber reinforced polytetrafluoroethylene (PTFE) lubricated nylon 612 grades offer a unique balance of excellent wear and friction performance with good dimensional stability and mecha.. |
|||
Limiting Pressure Velocity | 0.701 MPa-m/sec | 20000 psi-ft/min | at 100 FPM, ambient temperature, thrust washer. |
Techmer ES Plaslube® J-4/30/TF/15 Nylon 612, 30% GFR, 15% PTFE Plaslube glass fiber reinforced polytetrafluoroethylene (PTFE) lubricated nylon 612 grades offer a unique balance of excellent wear and friction performance with good dimensional stability and mecha.. |
|||
Limiting Pressure Velocity | 0.701 MPa-m/sec | 20000 psi-ft/min | Unlubricated |
TriStar FCJ Composite Bearing This family of materials offers the combination of high compressive strength, low coefficient of friction, and excellent abrasion and corrosion resistance while running without lubrication. They are.. |
|||
Limiting Pressure Velocity | 0.700 MPa-m/sec | 20000 psi-ft/min | |
A. Schulman ComAlloy Lubrilon® 629 Nylon 6/6, Glass Fiber/PTFE Filled, Flow Enhanced Data provided by the manufacturer, ComAlloy International Company. High performance and excellent lubricity with minimal surface wear.The ComAlloy product line has been integrated into the A Schulma.. |
|||
Limiting Pressure Velocity | 0.701 MPa-m/sec | 20000 psi-ft/min | |
Saint-Gobain Rulon® FCJ Grade Bearing/Seal PTFE
(discontinued **) Saint Gobain Rulon® CJ is now produced as a part of the TriStar Plastics Corp. product line under the CJ Bearings trade name.Description: Rulon® is the Saint-Gobain trade name for their family of .. |