Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Chevron Phillips mPact™ D143SA m-LLDPE Linear Low Density Polyethylene  (discontinued **)

Category Polymer , Film , Thermoplastic , Polyethylene (PE) , LLDPE , Linear Low Density Polyethylene (LLDPE), Film Grade
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chevron Phillips mPact™ D143SA m-LLDPE Linear Low Density Polyethylene  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Low Density PolyethyleneCustomer Benefits: This metallocene LLDPE film resin possesses the typical physical properties of metallocene polyethylenes with the added potential benefit of improved processability (bubble stability, down gauging, and melt fracture resistance). Applications: Can liners, general purpose packaging, S/AProperty Comments: LLDPE line, 2.5:1 BUR, .08" diegap, 8" die, 56" FLH, 250 lbs/hr, 400°FData provided by Chevron Phillips Chemical Company LP.
Physical Properties Metric English Comments
Density 0.916 g/cc
0.0331 lb/in³
ASTM D1505
Melt Flow 1.3 g/10 min
1.3 g/10 min
Condition 190/2.16; ASTM D1238
Mechanical Properties Metric English Comments
Secant Modulus, MD 0.150 GPa
21.8 ksi
at 1%; ASTM D882
Secant Modulus, TD 0.170 GPa
24.7 ksi
at 1%; ASTM D882
Coefficient of Friction, Dynamic 0.20
0.20
ASTM D1894
Coefficient of Friction, Static 0.17
0.17
ASTM D1894
Elmendorf Tear Strength MD 225 g
225 g
ASTM D1922
Elmendorf Tear Strength TD 375 g
375 g
ASTM D1922
Dart Drop Test 650 g
1.43 lb
26 in; ASTM D1709
Optical Properties Metric English Comments
Haze 14 %
14 %
ASTM D1003