Material Notes:
Availability: North AmericaForms: PelletsFeatures: Flame RetardantInformation provided by TP Composites, Inc.
Physical Properties Metric English Comments
Density 0.980 g/cc
0.0354 lb/in³
ASTM D792
Water Absorption 0.020 %

@Time 86400 sec
0.020 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.018 cm/cm

@Thickness 3.17 mm
0.018 in/in

@Thickness 0.125 in
ASTM D955
Melt Flow 12 g/10 min

@Load 2.16 kg,
Temperature 190 °C
12 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 24.8 MPa
3600 psi
ASTM D638
Elongation at Break 100 %
100 %
ASTM D638
Flexural Strength 35.2 MPa
5100 psi
ASTM D790
Flexural Modulus 1.10 GPa
160 ksi
ASTM D790
Izod Impact, Notched 0.961 J/cm

@Thickness 3.17 mm
1.80 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Flammability, UL94 V-2
V-2