Techmer ES Electrablend® PC/ABS 033009

Category Polymer , Thermoplastic , ABS Polymer , Polycarbonate/ABS Alloy, Antistat/Conductive , Polycarbonate (PC)
Manufacturer Techmer ES
Trade Name Electrablend®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Techmer ES Electrablend® PC/ABS 033009.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/Reinfor.Features: Electrically Conductive and ESD ProtectionInformation provided by TP Composites, Inc.
Physical Properties Metric English Comments
Density 1.21 g/cc
0.0437 lb/in³
ASTM D792
Water Absorption 0.10 %

@Time 86400 sec
0.10 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0050 cm/cm

@Thickness 3.17 mm
0.0050 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Yield 55.8 MPa
8100 psi
ASTM D638
Elongation at Break 7.0 %
7.0 %
ASTM D638
Flexural Strength 88.9 MPa
12900 psi
ASTM D790
Flexural Modulus 3.03 GPa
440 ksi
ASTM D790
Izod Impact, Notched 0.641 J/cm

@Thickness 3.17 mm
1.20 ft-lb/in

@Thickness 0.125 in
ASTM D256
Izod Impact, Unnotched 5.87 J/cm

@Thickness 3.17 mm
11.0 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 39.6 µm/m-°C
22.0 µin/in-°F
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 98.9 °C
210 °F
Unannealed; ASTM D648
Flammability, UL94 HB

@Thickness 1.50 mm
HB

@Thickness 0.0591 in
Electrical Properties Metric English Comments
Volume Resistivity 1.0 - 100 ohm-cm
1.0 - 100 ohm-cm
ASTM D257
Surface Resistance 1.0 - 100 ohm
1.0 - 100 ohm
ASTM D257
Static Decay <= 0.10 sec
<= 0.10 sec
FTMS 101B
Shielding Effectiveness 50 dB
50 dB
ASTM D4935