3M Scotch® 70 HDT Self-Fusing Silicone Rubber Electrical Tape with Tapered Edge

Category Polymer , Adhesive , Thermoset , Silicone , Silicone Rubber
Manufacturer 3M
Trade Name Scotch®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M Scotch® 70 HDT Self-Fusing Silicone Rubber Electrical Tape with Tapered Edge.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Scotch® Silicone Rubber Electrical Tape 70 HDT is a high-temperature arc-and track-resistant tape composed of self-fusing, inorganic silicone rubber and easy-tear and easy-strip liner. The 70 HDT product also has a triangular (tapered edge) profile and blue guidelines to make half-lapping application easier.Information provided by 3M
Physical Properties Metric English Comments
Thickness 203 microns
8.00 mil
Edge
508 microns
20.0 mil
Peak
Mechanical Properties Metric English Comments
Tensile Strength at Break 6.89 MPa
999 psi
ASTM D412
Elongation at Break 300 %
300 %
ASTM D412
Electrical Properties Metric English Comments
Volume Resistivity 7.00e+14 ohm-cm
7.00e+14 ohm-cm
ASTM D1458
Dielectric Constant 2.5

@Temperature 150 °C
2.5

@Temperature 302 °F
ASTM D150
2.6

@Temperature 130 °C
2.6

@Temperature 266 °F
ASTM D150
2.9

@Temperature 90.0 °C
2.9

@Temperature 194 °F
ASTM D150
3.0

@Temperature 23.0 °C
3.0

@Temperature 73.4 °F
ASTM D150
Dielectric Strength 23.6 kV/mm
600 kV/in
ASTM D2148
Dissipation Factor 0.50

@Temperature 130 °C
0.50

@Temperature 266 °F
ASTM D150
0.70

@Temperature 150 °C
0.70

@Temperature 302 °F
ASTM D150
Arc Resistance >= 60 sec
>= 60 sec
ASTM D495
Descriptive Properties Value Comments
Appearance Sky Blue Gray