Material Notes:
Availability: North AmericaForms: PelletsFiller/Reinforcement: /Glass/Stainless Steel FiberFeatures: ConductiveTPCI# 9873105Information provided by TP Composites, Inc.
Physical Properties Metric English Comments
Density 1.08 g/cc
0.0390 lb/in³
ASTM D792
Water Absorption 0.25 %

@Time 86400 sec
0.25 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.010 cm/cm

@Thickness 3.17 mm
0.010 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Yield 51.0 MPa
7400 psi
ASTM D638
Elongation at Break 10 %
10 %
ASTM D638
Flexural Strength 81.4 MPa
11800 psi
ASTM D790
Flexural Modulus 1.21 GPa
175 ksi
ASTM D790
Izod Impact, Notched 1.33 J/cm

@Thickness 3.17 mm
2.50 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 16.2 µm/m-°C
9.00 µin/in-°F
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 54.4 °C
130 °F
Unannealed; ASTM D648
Electrical Properties Metric English Comments
Volume Resistivity 100 ohm-cm
100 ohm-cm
ASTM D257
Surface Resistance 1000 ohm
1000 ohm
ASTM D257
Users viewing this material also viewed the following: