Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 54.4 °C | 130 °F | ASTM D648 |
RheTech Products FT5100-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural Applications: IP structural componentBody side moldingInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 54.4 °C | 130 °F | ASTM D648 |
RheTech Products FT5250-650UV Thermoplastic Polyolefin, UV Stabilized, Exterior 848 Black Applications: Cowl vent grillesExterior componentsBodyside moldingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 54.4 °C | 130 °F | ASTM D648 |
RheTech Products HP513-00 High Performance Polypropylene Copolymer, Non-UV Stabilized, Natural Applications: Interior trimI/P componentsCenter consolesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 54.4 °C | 130 °F | ASTM D648 |
RheTech Products P252-00 Polypropylene Copolymer, Natural Applications: Interior trimUnderhood componentsElectrical housingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 54.4 °C | 130 °F | Unannealed; ASTM D648 |
Ravago Manufacturing Americas Hylon® N2000THL Nylon 6 (DAM) Information provided by Ravago. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 54.4 °C | 130 °F | Unannealed; ASTM D648 |
M. Holland Company CP500 Polypropylene Copolymer Features: High Flow, High Impact Resistance, Good StiffnessUses: Automotive, Interior Parts Closures, Household Goods, ToysApprovals: FDA 21 CFR 177.1520Processing Method: Injection MoldingInformati.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 54.4 °C | 130 °F | ASTM D648 |
Kostat ICP-STAT ICS-1002 PP Sheet KOSTATs ICP-STAT is a thermoplastic sheet coated with an inherently conductive polymer (ICP). ICP-STAT has distinctive advantages in ESD and cleanliness performances compared to other materials bas.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 54.4 °C | 130 °F | ASTM D648 |
Kostat ICP-STAT ICD-1002 PP Sheet KOSTATs ICP-STAT is a thermoplastic sheet coated with an inherently conductive polymer (ICP). ICP-STAT has distinctive advantages in ESD and cleanliness performances compared to other materials bas.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 54.4 °C | 130 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PBT 620 Availability: North AmericaForms: PelletsFeatures: Medium FlowAppearance: Natural ColorInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 54.4 °C | 130 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PP 0096 S2 LE Polypropylene Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/ReinforFeatures: Low ExtractablesInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 54.4 °C | 130 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PP 0475 Polypropylene Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/ReinforInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 54.4 °C | 130 °F | Unannealed; ASTM D648 |
Techmer ES Luriblend® TPX-HDPE-99018 Availability: North AmericaForms: Pellets)Features: Good Wear Resistance and Low FrictionProcessing Method: Injection MoldingTPCI# 8869115Information provided by TP Composites, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 54.4 °C | 130 °F | Unannealed; ASTM D648 |
Techmer ES Statiblend® 02036 Polypropylene Availability: North AmericaForms: PelletsAdditive: AntistaticFeatures: Antistatic and ConductiveInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 54.4 °C | 130 °F | Unannealed; ASTM D648 |
Techmer ES Electrablend® PA12 Stainless Steel Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: /Glass/Stainless Steel FiberFeatures: ConductiveTPCI# 9873105Information provided by TP Composites, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 54.4 °C | 130 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PBT 0150 S Availability: North AmericaForms: PelletsFiller/Reinforcement: MetalInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 54.4 °C | 130 °F | ASTM D648 |
Westlake Plastics Propylux® CN-P Polypropylene (conductive) Carbon-powder-filled lightweight material with good chemical resistance, extremely low water absorption level, and high impact resistance (no break, notched or unnotched). Rated UL94 V-0.Informatio.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 54.4 - 185 °C | 130 - 365 °F | Average value: 102 °C Grade Count:54 |
Overview of materials for Thermoplastic Polyurethane (TPUR), Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane (TPUR), Glass Fiber Reinforced". Each property range of values reported is mi.. |