Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 54.4 °C
130 °F
ASTM D648
RheTech Products FT5100-04 Thermoplastic Polyolefin, UV Stabilized, White
Applications: IP structural componentBody side moldingInjection molding conditions reported in table.Information provided by RheTech Products.
Deflection Temperature at 1.8 MPa (264 psi) 54.4 °C
130 °F
ASTM D648
RheTech Products FT5250-650UVA Thermoplastic Polyolefin, UV Stabilized, Exterior 848 Black
Applications: Cowl vent grillesExterior componentsBodyside moldingsInjection molding conditions reported in table.Information provided by RheTech Products.
Deflection Temperature at 1.8 MPa (264 psi) 54.4 °C
130 °F
ASTM D648
RheTech Products P252-00 Polypropylene Copolymer, Natural
Applications: Interior trimUnderhood componentsElectrical housingsInjection molding conditions reported in table.Information provided by RheTech Products.
Deflection Temperature at 1.8 MPa (264 psi) 54.4 °C
130 °F
ASTM D648
RheTech Products RCC220-01 20% Calcium Carbonate Reinforced Polypropylene Copolymer, Black, Recycled Content
Applications: I/P hush panelsSplash shieldsUnderhood componentsInjection molding conditions reported in table.Information provided by RheTech Products.
Deflection Temperature at 1.8 MPa (264 psi) 54.4 °C
130 °F
ASTM D 648
RTP Company RTP PP FR2 NAT Polypropylene (PP), Flame Retardant - Non-PBB/PBDE - UL94 - Value Product
Deflection Temperature at 1.8 MPa (264 psi) 54.4 °C
130 °F
ASTM D648
RTP Company RTP 200C TFE 10  Nylon 11 (PA 11) PTFE 10%  (discontinued **)
PTFE 10%Comments:PTFE LubricatedUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provided by RTP Company.Data for thi..
Deflection Temperature at 1.8 MPa (264 psi) 54.4 - 60.0 °C
130 - 140 °F
Average value: 56.8 °C Grade Count:3
Overview of materials for Nylon 11 with Graphite Filler
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11 with Graphite Filler". Each property range of values reported is minimum and maximum values of ..
Deflection Temperature at 1.8 MPa (264 psi) 54.4 °C
130 °F
ASTM D648
Kostat ICP-STAT ICS-1002 PP Sheet
KOSTATs ICP-STAT is a thermoplastic sheet coated with an inherently conductive polymer (ICP). ICP-STAT has distinctive advantages in ESD and cleanliness performances compared to other materials bas..
Deflection Temperature at 1.8 MPa (264 psi) 54.4 °C
130 °F
Unannealed (0.250"); ASTM D648
LTL Color Compounds ColorFast® PBT100 PBT
General purpose injection molding grade unfilled PBT with lubeAll information provided by LTL Color Compounders, Inc.
Deflection Temperature at 1.8 MPa (264 psi) 54.4 °C
130 °F
ASTM D648
Kostat ICP-STAT ICD-1002 PP Sheet
KOSTATs ICP-STAT is a thermoplastic sheet coated with an inherently conductive polymer (ICP). ICP-STAT has distinctive advantages in ESD and cleanliness performances compared to other materials bas..
Deflection Temperature at 1.8 MPa (264 psi) 54.4 °C
130 °F
Unannealed; ASTM D648
Techmer ES HiFill® PA12 CM40 40% Mineral Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Mineral Filler, 40% Filler by WeightAdditive: LubricantFeatures: LubricatedInformation provided by TP Composites, Inc.
Deflection Temperature at 1.8 MPa (264 psi) 54.4 °C
130 °F
ASTM D648
Spartech PP5110 Talc Filled Homopolymer
Offers an excellent balance of processing improvement and high levels of stiffness and heat deflection temperatureInformation provided by Spartech
Deflection Temperature at 1.8 MPa (264 psi) 54.4 °C
130 °F
Unannealed; ASTM D648
Techmer ES HiFill® PP 0096 S LE Polypropylene
Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/ReinforFeatures: Low ExtractablesInformation provided by TP Composites, Inc.
Deflection Temperature at 1.8 MPa (264 psi) 54.4 °C
130 °F
Unannealed; ASTM D648
Techmer ES HiFill® PP 0320 S1 Polypropylene
Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/ReinforFeatures: Good Corrosion ResistanceInformation provided by TP Composites, Inc.
Deflection Temperature at 1.8 MPa (264 psi) 54.4 °C
130 °F
Unannealed; ASTM D648
Techmer ES Luriblend® PE 5902
Availability: North AmericaForms: PelletsAdditive: LubricantFeatures: Lubricated, Good Wear Resistance and Low FrictionProcessing Method: Injection MoldingInformation provided by TP Composites, Inc...
Deflection Temperature at 1.8 MPa (264 psi) 54.4 °C
130 °F
Unannealed; ASTM D648
Techmer ES Statiblend® HDPE C BK
Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified FillerReinforFeatures: ConductiveUL File Number: E157318Appearance: BlackTPCI# 9411115Information provided by TP Composites..
Deflection Temperature at 1.8 MPa (264 psi) 54.4 °C
130 °F
Unannealed; ASTM D648
Techmer ES Electrablend® PA12 Stainless Steel Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: /Glass/Stainless Steel FiberFeatures: ConductiveTPCI# 9873105Information provided by TP Composites, Inc.
Deflection Temperature at 1.8 MPa (264 psi) 54.4 °C
130 °F
ASTM D648
Chase Plastics CP Pryme® NN200STL (DAM) Nylon 66, Super-Toughened, Internally Lubricated
Information provided by Chase Plastics.
Deflection Temperature at 1.8 MPa (264 psi) 54.4 °C
130 °F
ASTM D 648
RTP Company RTP 1000 TFE 10 Z Polybutylene Terephthalate (PBT), PTFE Lubricated - FDA Compliant Ingredients
Deflection Temperature at 1.8 MPa (264 psi) 54.4 °C
130 °F
ASTM D 648
RTP Company RTP 1000 TFE 20 Polybutylene Terephthalate (PBT), PTFE Lubricated
Deflection Temperature at 1.8 MPa (264 psi) 54.4 °C
130 °F
ASTM D 648
RTP Company RTP 100 TFE 20 Polypropylene (PP), PTFE Lubricated
Deflection Temperature at 1.8 MPa (264 psi) 54.4 °C
130 °F
ASTM D 648
RTP Company RTP 143 HI Polypropylene (PP), Impact Modified - Calcium Carbonate
Deflection Temperature at 1.8 MPa (264 psi) 54.4 °C
130 °F
ASTM D 648
RTP Company RTP 152 LF Polypropylene (PP), Low Flow - Flame Retardant - UL94 V-2
The RTP 152 family of compounds are flame retarded, unreinforced polypropylene materials. They offer excellent moldability, non-corrosive characteristics and the living-hinge effect.
Deflection Temperature at 1.8 MPa (264 psi) 54.4 °C
130 °F
ASTM D 648
RTP Company RTP 200 C Nylon 11 (PA); Unfilled - >99% Renewable Resource Content
Renewable Resource Content calculated based on % of total compound weight.
Deflection Temperature at 1.8 MPa (264 psi) 54.4 °C
130 °F
ASTM D648
1700FC PBT, Unfilled
Celanex 1700FC is a very high molecular weight extrusion grade of unreinforced polybutylene terephthalate for use in food contact applications.Information provided by Celanese
Deflection Temperature at 1.8 MPa (264 psi) 54.4 °C
130 °F
ASTM D648
2008 PBT, Unfilled
Celanex 2008 is a general purpose, unreinforced polybutylene terephthalate with a good balance of mechanical properties and processability for use in melt blown applications.Information provided by ..
Deflection Temperature at 1.8 MPa (264 psi) 54.4 °C
130 °F
ASTM D648
8000 PBT, Unfilled
Vandar 8000 polyester alloy is designed to meet UL94 V-0 requirements at 1/32 inch thickness while retaining excellent impact resistance. The product is characterized by excellent moldability and su..
Deflection Temperature at 1.8 MPa (264 psi) 54.4 - 185 °C
130 - 365 °F
Average value: 102 °C Grade Count:54
Overview of materials for Thermoplastic Polyurethane (TPUR), Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane (TPUR), Glass Fiber Reinforced". Each property range of values reported is mi..
Deflection Temperature at 1.8 MPa (264 psi) 54.4 °C
130 °F
ASTM D648
LookPolymers® 1400FC PBT  (Unverified Data**)
Celanex 1400FC is a general purpose, unreinforced polybutylene terephthalate with a good balance of mechanical properties and processability for use in food contact applications. Celanex 1400FC is a..
Deflection Temperature at 1.8 MPa (264 psi) 54.4 °C
130 °F
ASTM D648
Chase Plastics CP Pryme® PPC100-8M Polypropylene Copolymer
Information provided by Chase Plastics.