Material Notes:
Availability: North AmericaForms: PelletsAdditive: Impact ModifierFeatures: Impact Modified and High ViscosityProcessing Method: ExtrusionInformation provided by TP Composites, Inc.
Physical Properties Metric English Comments
Density 1.19 g/cc
0.0430 lb/in³
ASTM D792
Water Absorption 0.14 %

@Time 86400 sec
0.14 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0060 cm/cm

@Thickness 3.17 mm
0.0060 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 114
114
ASTM D785
Tensile Strength, Yield 58.6 MPa
8500 psi
ASTM D638
Elongation at Yield 14 %
14 %
ASTM D638
Flexural Yield Strength 82.7 MPa
12000 psi
ASTM D790
Flexural Modulus 2.48 GPa
360 ksi
ASTM D790
Izod Impact, Notched 2.72 J/cm

@Thickness 3.17 mm,
Temperature -40.0 °C
5.10 ft-lb/in

@Thickness 0.125 in,
Temperature -40.0 °F
ASTM D256
2.94 J/cm

@Thickness 6.35 mm,
Temperature 22.8 °C
5.50 ft-lb/in

@Thickness 0.250 in,
Temperature 73.0 °F
ASTM D256
8.54 J/cm

@Thickness 3.17 mm,
Temperature 22.8 °C
16.0 ft-lb/in

@Thickness 0.125 in,
Temperature 73.0 °F
ASTM D256
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 68.4 µm/m-°C
38.0 µin/in-°F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 132 °C
270 °F
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 127 °C
260 °F
Unannealed; ASTM D648
Flammability, UL94 V-2

@Thickness 1.50 mm
V-2

@Thickness 0.0591 in
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+17 ohm-cm
1.00e+17 ohm-cm
ASTM D257
Dielectric Strength 15.0 kV/mm
380 kV/in
Method A (Short-Time); ASTM D149