Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 58.6 MPa | 8500 psi | ASTM D638 |
Multibase Multi-Pro® 2005 RCI Polypropylene Glass Fiber Reinforced, 20% by weight.Features:Heat Resistance, HighScratch ResistantStiffness, GoodForms:PelletsProcessing Methods:Injection MoldingUses:Automotive ApplicationsInformation provided .. |
|||
Tensile Strength, Yield | 58.6 MPa | 8500 psi | ASTM D638 |
Oxford Polymers 20GF 20% Glass Fiber Reinforced ABS, Flame Retardant 20% Glass Fiber Reinforced ABS, Flame RetardantInformation provided by Oxford Polymers. |
|||
Tensile Strength, Yield | 58.6 MPa | 8500 psi | ASTM D638 |
Oxford Polymers PC 10GF-V0 UL Listed Polycarbonate UL Listed PolycarbonateInformation provided by Oxford Polymers. |
|||
Tensile Strength, Yield | 58.6 MPa | 8500 psi | ASTM D638 |
Oxford Polymers PC GR912-V0 UL Listed Polycarbonate UL Listed PolycarbonateInformation provided by Oxford Polymers. |
|||
Tensile Strength, Yield | 58.6 MPa | 8500 psi | ASTM D638 |
Polymer Resources AH-GP2-TFE10 Acetal Homopolymer, 10% PTFE Process: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Polymer Resources Corporation. |
|||
Tensile Strength, Yield | 58.6 MPa @Thickness 3.17 mm |
8500 psi @Thickness 0.125 in |
ASTM D638 |
PTS Tristar® PC-06R 6.0 MFI Grade Polycarbonate, With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Tensile Strength, Yield | 58.6 MPa | 8500 psi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
PolyOne Lubri-Tech™ AT-15MCF/15T Acetal-Copolymer, Carbon Fiber Reinforced, PTFE Lubricated
(discontinued **) Description/Features:Milled Carbon Fiber ReinforcedPTFE LubricatedUL 94 HBPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Tensile Strength, Yield | 58.6 - 70.0 MPa | 8500 - 10200 psi | Average value: 63.7 MPa Grade Count:34 |
Overview of materials for Polycarbonate, Extruded This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Extruded". Each property range of values reported is minimum and maximum values of approp.. |
|||
Tensile Strength, Yield | 58.6 MPa | 8500 psi | oriented film, Yield Stress |
Honeywell Aegis™ OX High Barrier Nylon
(discontinued **) Description: Aegis OX is an oxygen-scavenging nylon. Oxygen barrier is comparable to a glass bottle with metal crown closure. In addition Aegis OX provides CO2 barrier and possesses glass-like cla.. |
|||
Tensile Strength, Yield | 58.6 MPa | 8500 psi | ASTM D638 |
MRC Polymers NAXALOYâ„¢ 780 PC+PBT Polyester Blend Good chemical resistance, impact and heat resistance.Information provided by MRC Polymers Inc. |
|||
Tensile Strength, Yield | 58.6 MPa | 8500 psi | ASTM D638 |
Kostat ICP-STAT ICS-1000 PC Sheet KOSTATs ICP-STAT is a thermoplastic sheet coated with an inherently conductive polymer (ICP). ICP-STAT has distinctive advantages in ESD and cleanliness performances compared to other materials bas.. |
|||
Tensile Strength, Yield | 58.6 MPa | 8500 psi | ASTM D638 |
Techmer ES Elastoblend® PC E IM Availability: North AmericaForms: PelletsAdditive: Impact ModifierFeatures: Impact Modified and High ViscosityProcessing Method: ExtrusionInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 58.6 MPa | 8500 psi | ASTM D638 |
Techmer ES Electrablend® PEI 04008 MB Availability: North AmericaForms: PelletsFeatures: Conductive and CopolymerInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 58.6 MPa | 8500 psi | ASTM D638 |
Techmer ES HiFill® PA6 1030 Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/ReinforFeatures: High Specific GravityInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 58.6 MPa | 8500 psi | ASTM D638 |
Star Plastics PC1212FR Molding Grade PC FR Information provided by Star Plastics, Inc. |
|||
Tensile Strength, Yield | 58.6 MPa | 8500 psi | ASTM D638 |
Star Plastics PC1212FRR Molding Grade PC FR Information provided by Star Plastics, Inc. |
|||
Tensile Strength, Yield | 58.6 MPa | 8500 psi | ASTM D638 |
Star Plastics PC1212FRUV Molding Grade PC FR Information provided by Star Plastics, Inc. |
|||
Tensile Strength, Yield | 58.6 MPa | 8500 psi | ASTM D638 |
Star Plastics PC1510UV Molding Grade PC Information provided by Star Plastics, Inc. |
|||
Tensile Strength, Yield | 58.6 MPa | 8500 psi | ASTM D638 |
Techmer ES Luriblend® PA12 TS18 Availability: North AmericaForms: PelletsAdditive: Silicone Lubricant(2%) and PTFE Lubricant(18%)Features: LubricatedInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 58.6 MPa | 8500 psi | ASTM D638 |
Techmer ES Luriblend® PA4/6 HS TL15 Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer and PTFE Lubricant (15%)Features: Heat Stabilized and LubricatedUL File Number: E157318Information provided by TP Composites, Inc... |
|||
Tensile Strength, Yield | 58.6 MPa | 8500 psi | ASTM D638 |
Techmer ES Luriblend® PA4/6 TL15 HS Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer and PTFE Lubricant (15%)Features: Heat Stabilized, Low Friction, Good Wear Resistance and LubricatedInformation provided by TP Com.. |
|||
Tensile Strength, Yield | 58.6 MPa | 8500 psi | ASTM D638 |
Techmer ES Luriblend® POM CO X MB Acetal Availability: North AmericaForms: PelletsAdditive: LubricantFeatures: Lubricated, Good Wear Resistance, Low Friction and CopolymerUL File Number: E157318Information provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 58.6 MPa | 8500 psi | ASTM D638 |
Styron EMERGEâ„¢ 7550 Polycarbonate (PC) / Acrylonitrile Butadiene Styrene (ABS) EMERGEâ„¢ PC/ABS 7550 advanced resin is an ignition-resistant PC/ABS blend that contains no chlorine or bromine additives. This resin is suitable for use in a wide variety of applications in the.. |
|||
Tensile Strength, Yield | 58.6 MPa | 8500 psi | ASTM D638 |
Star Plastics PC1212R Molding Grade PC with Release Information provided by Star Plastics, Inc. |
|||
Tensile Strength, Yield | 58.6 MPa | 8500 psi | chs 2.0 in/min; ASTM D638 |
Diamond Polymers ABSPC 8020 Very High Impact Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Tensile Strength, Yield | 58.6 MPa | 8500 psi | ASTM D638 |
Clariant Renol PBT1100 Black Polybutylene Terephthalate, General Purpose Data provided by Clariant Masterbatches |
|||
Tensile Strength, Yield | 58.6 MPa | 8500 psi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
PolyOne Lubri-Tech™ AT-10GF-10KV/000 Acetal-Copolymer, Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedAramid Fiber ReinforcedInformation provided by PolyOne Corporation. |
|||
Tensile Strength, Yield | 58.6 - 125 MPa | 8500 - 18100 psi | Average value: 88.7 MPa Grade Count:10 |
Overview of materials for Polybutylene Terephthalate (PBT), Glass + Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass + Mineral Filled". Each property range of values reported is min.. |