Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 2.72 J/cm @Temperature -29.0 °C |
5.10 ft-lb/in @Temperature -20.2 °F |
3.2 mm (0.125 in) notch |
Kraton® G1657 + PA-6,6 blend (8/12/80) Blending KRATON D and G polymers with PA significantly improves the toughness at both room and low temperatures. KRATON polymers are block segments of styrene and rubber monomers (A-B, A-B-A, or [A.. |
|||
Izod Impact, Notched | 2.72 J/cm @Temperature 22.8 °C |
5.10 ft-lb/in @Temperature 73.0 °F |
1/8" x 1/2" bar; ASTM-D256 (Method A) |
Ineos ABS Lustran® Guardian™ 620 ABS, Extrusion Grade Lustran® Guardian™ ABS 620 is a high modulus, HFC 134a and HCFC 22 resistant extrusion grade resin designed for refrigerator door and food liners. Lustran® ABS 620 offers good melt streng.. |
|||
Izod Impact, Notched | 2.72 J/cm @Thickness 3.17 mm, Temperature -40.0 °C |
5.10 ft-lb/in @Thickness 0.125 in, Temperature -40.0 °F |
ASTM D256 |
Techmer ES Elastoblend® PC E IM Availability: North AmericaForms: PelletsAdditive: Impact ModifierFeatures: Impact Modified and High ViscosityProcessing Method: ExtrusionInformation provided by TP Composites, Inc. |