Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 58.6 MPa | 8500 psi | chs 2 in/min; ASTM D638 |
Network Polymers NPP 3514 Description: Black Polycarbonate Polyester AlloyInformation provided by Network Polymers Inc. |
|||
Tensile Strength, Yield | 58.6 MPa | 8500 psi | ASTM D638 |
Oxford Polymers 20GF 20% Glass Fiber Reinforced ABS, Flame Retardant 20% Glass Fiber Reinforced ABS, Flame RetardantInformation provided by Oxford Polymers. |
|||
Tensile Strength, Yield | 58.6 MPa | 8500 psi | ASTM D638 |
Oxford Polymers PC 10GF-V0 UL Listed Polycarbonate UL Listed PolycarbonateInformation provided by Oxford Polymers. |
|||
Tensile Strength, Yield | 58.6 MPa | 8500 psi | ASTM D638 |
Oxford Polymers PC GR912-V0 UL Listed Polycarbonate UL Listed PolycarbonateInformation provided by Oxford Polymers. |
|||
Tensile Strength, Yield | 58.6 MPa | 8500 psi | ASTM D638 |
Polymer Resources PC-GP1-TFE5 Polycarbonate, 5% PTFE, Wear Resistant, Low Flow Polycarbonate, 5% PTFE, General Purpose, Wear Resistant, Low FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.. |
|||
Tensile Strength, Yield | 58.6 MPa @Thickness 3.17 mm |
8500 psi @Thickness 0.125 in |
ASTM D638 |
PTS Tristar® PC-06 6 MFI Extrusion Grade Polycarbonate Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Tensile Strength, Yield | 58.6 MPa @Thickness 3.17 mm |
8500 psi @Thickness 0.125 in |
ASTM D638 |
PTS Tristar® PC-06R 6.0 MFI Grade Polycarbonate, With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Tensile Strength, Yield | 58.6 MPa @Thickness 3.17 mm |
8500 psi @Thickness 0.125 in |
ASTM D638 |
PTS Tristar® PC-10R-(V15) 15 MFI UV Stabilized Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Tensile Strength, Yield | 58.6 MPa | 8500 psi | oriented film, Yield Stress |
Honeywell Aegis™ OX High Barrier Nylon
(discontinued **) Description: Aegis OX is an oxygen-scavenging nylon. Oxygen barrier is comparable to a glass bottle with metal crown closure. In addition Aegis OX provides CO2 barrier and possesses glass-like cla.. |
|||
Tensile Strength, Yield | 58.6 MPa | 8500 psi | ASTM D638 |
Fiberfil® J-60/10/E Polypropylene Homopolymer, 10% Glass Reinforced, Chemically coupled Information provided by FIBERFIL Engineered Plastics |
|||
Tensile Strength, Yield | 58.6 MPa | 8500 psi | ASTM D638 |
Fiberfil® J-60/20 Polypropylene Homopolymer, 20% Glass Reinforced Information provided by FIBERFIL Engineered Plastics |
|||
Tensile Strength, Yield | 58.6 MPa | 8500 psi | ASTM D638 |
M. Holland Company PC402R Polycarbonate High clarityHigh heat resistanceHigh impact resistanceGood mold releaseApplications: AppliancesContainersTable products |
|||
Tensile Strength, Yield | 58.6 MPa | 8500 psi | ASTM D638 |
Fiberfil® J-60/10/E8 Polypropylene Homopolymer, 10% Glass Reinforced, Chemically coupled Information provided by FIBERFIL Engineered Plastics |
|||
Tensile Strength, Yield | 58.6 MPa | 8500 psi | ASTM D638 |
Fiberfil® J-61/30/FR Polypropylene Copolymer, 30% Glass Reinforced, Flame Retardant Information provided by FIBERFIL Engineered Plastics |
|||
Tensile Strength, Yield | 58.6 MPa | 8500 psi | ASTM D638 |
Techmer ES HiFill® PA6 1030 Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/ReinforFeatures: High Specific GravityInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 58.6 MPa | 8500 psi | ASTM D638 |
Star Plastics PC1212FRUV Molding Grade PC FR Information provided by Star Plastics, Inc. |
|||
Tensile Strength, Yield | 58.6 MPa | 8500 psi | ASTM D638 |
Star Plastics PC1510FR Molding Grade PC Information provided by Star Plastics, Inc. |
|||
Tensile Strength, Yield | 58.6 MPa | 8500 psi | ASTM D638 |
Star Plastics PC1510R Molding Grade PC Information provided by Star Plastics, Inc. |
|||
Tensile Strength, Yield | 58.6 MPa | 8500 psi | ASTM D638 |
Star Plastics PC1510RUV Molding Grade PC Information provided by Star Plastics, Inc. |
|||
Tensile Strength, Yield | 58.6 MPa | 8500 psi | ASTM D638 |
Techmer ES Luriblend® PA4/6 HS TL15 Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer and PTFE Lubricant (15%)Features: Heat Stabilized and LubricatedUL File Number: E157318Information provided by TP Composites, Inc... |
|||
Tensile Strength, Yield | 58.6 MPa | 8500 psi | ASTM D638 |
Techmer ES Luriblend® PA4/6 TL15 HS Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer and PTFE Lubricant (15%)Features: Heat Stabilized, Low Friction, Good Wear Resistance and LubricatedInformation provided by TP Com.. |
|||
Tensile Strength, Yield | 58.6 MPa | 8500 psi | ASTM D638 |
Techmer ES Luriblend® POM CO X MB Acetal Availability: North AmericaForms: PelletsAdditive: LubricantFeatures: Lubricated, Good Wear Resistance, Low Friction and CopolymerUL File Number: E157318Information provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 58.6 MPa | 8500 psi | ASTM D638 |
Techmer ES Plastiblend® PA6/6,6 IM 5050 BK Nylon 6/66 Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Impact Modifier and LubricantFeatures: Heat Stabilized, Copolymer, Impact Modified and LubricatedAppearance: BlackProcessing Metho.. |
|||
Tensile Strength, Yield | 58.6 MPa | 8500 psi | ASTM D638 |
Styron EMERGEâ„¢ 7550 Polycarbonate (PC) / Acrylonitrile Butadiene Styrene (ABS) EMERGEâ„¢ PC/ABS 7550 advanced resin is an ignition-resistant PC/ABS blend that contains no chlorine or bromine additives. This resin is suitable for use in a wide variety of applications in the.. |
|||
Tensile Strength, Yield | 58.6 MPa | 8500 psi | ASTM D638 |
Star Plastics PC1212R Molding Grade PC with Release Information provided by Star Plastics, Inc. |
|||
Tensile Strength, Yield | 58.6 MPa | 8500 psi | ASTM 638 |
PlastxWorld CEVIAN®-V 520 ABS Super High Rigid ABSThese are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc. |
|||
Tensile Strength, Yield | 58.6 MPa | 8500 psi | ASTM D638 |
Chase Plastics CP Pryme® PC310R Polycarbonate, 10% Glass Fiber Reinforced, Recycled Content Features: Good mold releaseRecycled contentForm: PelletsInformation provided by Chase Plastics. |
|||
Tensile Strength, Yield | 58.6 MPa | 8500 psi | ASTM D638 |
Clariant Renol PA2SP0010HW Nylon 6, Heavyweight Compound Data provided by Clariant Masterbatches |
|||
Tensile Strength, Yield | 58.6 MPa | 8500 psi | ASTM D638 |
Ex-Tech Plastics VersaTech™ APET Ex-Tech VersaTech™ APET has exceptional properties such as visual transparency high heat distortion and it has good resistance to mineral oils, solvents and acids.Characteristics:TransparentExcepti.. |
|||
Tensile Strength, Yield | 58.6 - 125 MPa | 8500 - 18100 psi | Average value: 88.7 MPa Grade Count:10 |
Overview of materials for Polybutylene Terephthalate (PBT), Glass + Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass + Mineral Filled". Each property range of values reported is min.. |