Material Notes:
Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Lubricant and Impact ModifierFeatures: Heat Stabilized, Lubricant and Impact ModifiedUL File Number: E157318Processing Method: Injection MoldingTPCI# 9170101Information provided by TP Composites, Inc.
Physical Properties Metric English Comments
Density 1.08 g/cc
0.0390 lb/in³
ASTM D792
Water Absorption 1.3 %

@Time 86400 sec
1.3 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.013 cm/cm

@Thickness 3.17 mm
0.013 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 110
110
ASTM D785
Tensile Strength 48.3 MPa
7000 psi
ASTM D638
Elongation at Yield 48 %
48 %
ASTM D638
Flexural Yield Strength 59.3 MPa
8600 psi
ASTM D790
Flexural Modulus 1.79 GPa
260 ksi
ASTM D790
Izod Impact, Notched 1.82 J/cm

@Thickness 3.17 mm,
Temperature -40.0 °C
3.40 ft-lb/in

@Thickness 0.125 in,
Temperature -40.0 °F
ASTM D256
8.01 J/cm

@Thickness 3.17 mm,
Temperature 22.8 °C
15.0 ft-lb/in

@Thickness 0.125 in,
Temperature 73.0 °F
ASTM D256
Izod Impact, Unnotched NB

@Thickness 3.17 mm
NB

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 79.2 µm/m-°C
44.0 µin/in-°F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 216 °C
420 °F
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 71.1 °C
160 °F
Unannealed; ASTM D648
Flammability, UL94 HB
HB
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+14 ohm-cm
1.00e+14 ohm-cm
ASTM D257
Dielectric Strength 17.3 kV/mm
440 kV/in
Method A (Short-Time); ASTM D149
Users viewing this material also viewed the following: