Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 1.82 J/cm @Thickness 3.17 mm, Temperature 22.8 °C |
3.40 ft-lb/in @Thickness 0.125 in, Temperature 73.0 °F |
ASTM-D256 |
Ineos ABS Lustran® 451 ABS, Injection Molding Grade Lustran® ABS 451 is a soft flowing, medium impact injection molding resin designed with a unique balance of impact, heat resistance, flow, and gloss. |
|||
Izod Impact, Notched | 1.82 J/cm @Thickness 3.17 mm, Temperature 22.8 °C |
3.40 ft-lb/in @Thickness 0.125 in, Temperature 73.0 °F |
ASTM D256 |
Techmer ES Elastoblend® PA6/6 GF13 IM HS BK 13% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 13% Filler by WeightAdditive: Heat Stabilizer, Impact Modifier and LubricantFeatures: Heat Stabilized, Impac.. |
|||
Izod Impact, Notched | 1.82 J/cm @Thickness 3.17 mm, Temperature -40.0 °C |
3.40 ft-lb/in @Thickness 0.125 in, Temperature -40.0 °F |
ASTM D256 |
Techmer ES Elastoblend® PA6/6 GF4 IM L LE Availability: North AmericaForms: PelletsAdditive: Lubricant and Impact ModifierFeatures: Lubricant, Low Extractables and Impact ModifiedAppearance: Natural ColorInformation provided by TP Composite.. |
|||
Izod Impact, Notched | 1.82 J/cm @Thickness 3.17 mm, Temperature -40.0 °C |
3.40 ft-lb/in @Thickness 0.125 in, Temperature -40.0 °F |
ASTM D256 |
Techmer ES Elastoblend® PA6/6 HI BK Nylon 66 Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Lubricant and Impact ModifierFeatures: Heat Stabilized, Lubricant and Impact ModifiedUl File Number: E157318Appearance: BlackProce.. |
|||
Izod Impact, Notched | 1.82 J/cm @Thickness 3.17 mm, Temperature -40.0 °C |
3.40 ft-lb/in @Thickness 0.125 in, Temperature -40.0 °F |
ASTM D256 |
Techmer ES Elastoblend® PA6/6 IM L N Nylon 66 Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Lubricant and Impact ModifierFeatures: Heat Stabilized, Lubricant and Impact ModifiedUL File Number: E157318Processing Method: Inj.. |
|||
Izod Impact, Notched | 1.82 J/cm @Thickness 3.17 mm, Temperature -40.0 °C |
3.40 ft-lb/in @Thickness 0.125 in, Temperature -40.0 °F |
ASTM D256 |
Techmer ES Elastoblend® PA6/6 IM L W Nylon 66 Availability: North AmericaForms: PelletsAdditive: Lubricant and Impact ModifierFeatures: Lubricant and Impact ModifiedProcessing Method: Injection MoldingInformation provided by TP Composites, Inc... |
|||
Izod Impact, Notched | 1.82 J/cm @Thickness 3.17 mm, Temperature 0.000 °C |
3.40 ft-lb/in @Thickness 0.125 in, Temperature 32.0 °F |
ASTM D256 |
Techmer ES Plastiblend® ABS 8004 UV Availability: North AmericaForms: PelletsAdditive: UV StabilizerFeatures: Good UV Resistance and High Heat ResistanceInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 1.82 J/cm @Thickness 3.17 mm, Temperature 0.000 °C |
3.40 ft-lb/in @Thickness 0.125 in, Temperature 32.0 °F |
ASTM D256 |
Techmer ES Plastiblend® ABS 8004 UV MB Availability: North AmericaForms: PelletsAdditive: UV StabilizerFeatures: Good UV Resistance and High Heat ResistanceTPCI# 6816121Information provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 1.82 J/cm @Thickness 3.17 mm, Temperature 0.000 °C |
3.40 ft-lb/in @Thickness 0.125 in, Temperature 32.0 °F |
ASTM D256 |
Techmer ES Plastiblend® ABS 8012 Availability: North AmericaForms: PelletsProcessing Method: ExtrusionInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 1.82 J/cm @Thickness 3.17 mm, Temperature 0.000 °C |
3.40 ft-lb/in @Thickness 0.125 in, Temperature 32.0 °F |
ASTM D256 |
Techmer ES Plastiblend® ABS 8014 Availability: North AmericaForms: PelletsProcessing Method: ExtrusionInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 1.82 J/cm @Thickness 3.17 mm, Temperature -40.0 °C |
3.40 ft-lb/in @Thickness 0.125 in, Temperature -40.0 °F |
ASTM D256 |
Techmer ES Elastoblend® PA6/6 IM HS L BK Nylon 66 Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Lubricant and Impact ModifierFeatures: Heat Stabilized, Lubricant and Impact ModifiedProcessing Method: Injection MoldingInformati.. |
|||
Izod Impact, Notched | 1.82 J/cm @Thickness 3.17 mm, Temperature -40.0 °C |
3.40 ft-lb/in @Thickness 0.125 in, Temperature -40.0 °F |
ASTM D256 |
Techmer ES Elastoblend® PA6/6 IM L UV Nylon 66 Availability: North AmericaForms: PelletsAdditive: UV Stabilizer, Lubricant and Impact ModifierFeatures: Lubricant and Impact ModifiedProcessing Method: Injection MoldingInformation provided by TP C.. |
|||
Izod Impact, Notched | 1.82 J/cm @Thickness 3.17 mm, Temperature -40.0 °C |
3.40 ft-lb/in @Thickness 0.125 in, Temperature -40.0 °F |
ASTM D256 |
Techmer ES Elastoblend® PA6/6 IM X Nylon 66 Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Lubricant and Impact ModifierFeatures: Lubricant and Impact ModifiedProcessing Method: Injection MoldingInformation provided by TP.. |
|||
Izod Impact, Notched | 1.82 J/cm @Thickness 3.17 mm, Temperature 0.000 °C |
3.40 ft-lb/in @Thickness 0.125 in, Temperature 32.0 °F |
ASTM D256 |
Techmer ES Plastiblend® ABS 8004 Availability: North AmericaForms: PelletsFeatures: General Purpose and High Impact ResistanceInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 1.82 J/cm @Thickness 3.17 mm, Temperature 0.000 °C |
3.40 ft-lb/in @Thickness 0.125 in, Temperature 32.0 °F |
ASTM D256 |
Techmer ES Plastiblend® ABS FR IM Availability: North AmericaForms: PelletsFeatures: Flame Retardant and High Impact ResistanceProcessing Method: Injection MoldingInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 1.82 J/cm @Thickness 3.17 mm, Temperature 0.000 °C |
3.40 ft-lb/in @Thickness 0.125 in, Temperature 32.0 °F |
ASTM D256 |
Techmer ES Plastiblend® ABS IM Availability: North AmericaForms: PelletsFeatures: High Heat ResistanceInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 1.82 J/cm @Thickness 3.17 mm |
3.41 ft-lb/in @Thickness 0.125 in |
|
TPI Porene® ABS-AN450 Flame Retardant ABS Resin Information provided by US distributor Polymer Technology and Services, LLC (PTS). |