Polymer Property : Izod Impact, Notched = 8.01 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 8.01 J/cm

@Temperature 23.0 °C
15.0 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
SABIC Innovative Plastics Lexan® 945ASR PC
Lexan* 945ASR Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating and is available in transparent and t..
Izod Impact, Notched 8.01 J/cm

@Temperature 23.0 °C
15.0 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
SABIC Innovative Plastics Lexan® 945ASR PC (Asia Pacific)
Lexan* 945ASR Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating and is available in transparent and t..
Izod Impact, Notched 8.01 J/cm

@Temperature 23.0 °C
15.0 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
SABIC Innovative Plastics Lexan® 945ASR PC (Europe-Africa-Middle East)
Lexan* 945ASR Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating and is available in transparent and t..
Izod Impact, Notched 8.01 J/cm

@Temperature 23.0 °C
15.0 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
SABIC Innovative Plastics Lexan® EXL1330 PC Copolymer (Europe-Africa-Middle East)
Lexan* EXL1330 polycarbonate (PC) siloxane copolymer resin is a UV stabilized opaque injection molding (IM) and sheet extrusion grade. This resin offers extreme low temperature (-60 C) ductility in ..
Izod Impact, Notched 8.01 J/cm

@Temperature 22.8 °C
15.0 ft-lb/in

@Temperature 73.0 °F
ASTM D256
Polymer Resources PC-IM2 Polycarbonate, Impact Modified, Medium Flow
Polycarbonate, Impact Modified, Medium FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided ..
Izod Impact, Notched 8.01 J/cm

@Temperature 22.8 °C
15.0 ft-lb/in

@Temperature 73.0 °F
ASTM D256
Polymer Resources PC-IM2-UV Polycarbonate, Impact Modified, Medium Flow, UV-stabilized
Polycarbonate, Impact Modified, Medium Flow, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inform..
Izod Impact, Notched 8.01 J/cm

@Temperature 23.0 °C
15.0 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
SABIC Innovative Plastics Lexan® EXL6414 PC (Europe-Africa-Middle East)
PC-Siloxane copolymer with excellent processability. Impact modified, medium flow, extreme low temp. ductility.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Izod Impact, Notched 8.01 J/cm

@Temperature 22.8 °C
15.0 ft-lb/in

@Temperature 73.0 °F
ASTM D256
Polymer Resources TP-IM1 Polybutylene Terephthalate, Low Temperature Impact Modified
Polybutylene Terephthalate, Low Temperature Impact ModifiedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Infor..
Izod Impact, Notched 8.01 J/cm

@Thickness 3.18 mm,
Temperature 23.0 °C
15.0 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Injection Molded; ASTM D256A
PolyOne Edgetek® XT XT-100-BW01 Natural PC+PBT  (discontinued **)
EDGETEK™ XT High Performance Polymers are polycarbonate and polyester alloys that combine strength, durability and chemical resistance. The Edgetek XT product family includes a complete line of gen..
Izod Impact, Notched 8.01 J/cm

@Thickness 3.18 mm,
Temperature 23.0 °C
15.0 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Injection Molded; ASTM D256A
PolyOne Edgetek® XT XT-100-CX01 PC+PBT  (discontinued **)
EDGETEK™ XT High Performance Polymers are polycarbonate and polyester alloys that combine strength, durability and chemical resistance. The Edgetek XT product family includes a complete line of gen..
Izod Impact, Notched 8.01 J/cm

@Thickness 3.18 mm,
Temperature 23.0 °C
15.0 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Injection Molded; ASTM D256A
PolyOne Edgetek® XT XT-500-CX01 PC+PBT  (discontinued **)
EDGETEK™ XT High Performance Polymers are polycarbonate and polyester alloys that combine strength, durability and chemical resistance. The Edgetek XT product family includes a complete line of gen..
Izod Impact, Notched 8.01 J/cm

@Temperature 22.8 °C
15.0 ft-lb/in

@Temperature 73.0 °F
ASTM D256
Polymer Resources PC/TP-GP3 PC/Polyester Alloy
High Impact, Superior Chemical ResistanceProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by..
Izod Impact, Notched 8.01 J/cm

@Thickness 3.17 mm,
Temperature 22.8 °C
15.0 ft-lb/in

@Thickness 0.125 in,
Temperature 73.0 °F
ASTM-D256
Ineos ABS Triax® 3050 ABS/Nylon Alloy, Injection Molding Grade (DAM)
Triax® 3050 resin is an ABS (Acrylonitrile Butadiene Styrene)/Nylon 6 alloy for injection molding. It is a semicrystalline thermoplastic with improved stability to light exposure, excellent proce..
Izod Impact, Notched 8.01 J/cm

@Thickness 3.17 mm,
Temperature 22.8 °C
15.0 ft-lb/in

@Thickness 0.125 in,
Temperature 73.0 °F
ASTM D256
Lucent Polymers PC/PBT-1550 Polycarbonate+PBT, Improved Impact Resistance, Injection Grade
Add "R" for Added ReleaseAdd "U" for UV StabilizerInformation provided by Lucent Polymers, Inc.
Izod Impact, Notched 8.01 J/cm

@Thickness 3.17 mm,
Temperature 22.8 °C
15.0 ft-lb/in

@Thickness 0.125 in,
Temperature 73.0 °F
ASTM-D256
Ineos ABS Triax® 3050 ABS/Nylon Alloy, Injection Molding Grade (Conditioned)
Triax® 3050 resin is an ABS (Acrylonitrile Butadiene Styrene)/Nylon 6 alloy for injection molding. It is a semicrystalline thermoplastic with improved stability to light exposure, excellent proce..
Izod Impact, Notched 8.01 J/cm

@Thickness 3.17 mm,
Temperature 22.8 °C
15.0 ft-lb/in

@Thickness 0.125 in,
Temperature 73.0 °F
ASTM D256
Techmer ES Elastoblend® PA6/6 IM L N Nylon 66
Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Lubricant and Impact ModifierFeatures: Heat Stabilized, Lubricant and Impact ModifiedUL File Number: E157318Processing Method: Inj..
Izod Impact, Notched 8.01 J/cm

@Thickness 3.17 mm,
Temperature 22.8 °C
15.0 ft-lb/in

@Thickness 0.125 in,
Temperature 73.0 °F
ASTM D256
Techmer ES Plastiblend® PC/PBT IM 1012
Availability: North AmericaForms: PelletsAdditive: Impact ModifierFeatures: Impact ModifiedAppearance: BlackInformation provided by TP Composites, Inc.
Izod Impact, Notched 8.01 J/cm

@Thickness 3.17 mm,
Temperature 22.8 °C
15.0 ft-lb/in

@Thickness 0.125 in,
Temperature 73.0 °F
ASTM D256
Techmer ES Elastoblend® PA6/6 IM HS L BK Nylon 66
Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Lubricant and Impact ModifierFeatures: Heat Stabilized, Lubricant and Impact ModifiedProcessing Method: Injection MoldingInformati..
Izod Impact, Notched 8.01 J/cm

@Thickness 3.17 mm,
Temperature 23.0 °C
15.0 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
ASTM D-256
Axiall 9211 Rigid PVC, Molding
Georgia Gulf 9211 is a food grade vinyl compound designed to maximize clarity. It is suitable for use in a variety of food, cosmetic and personal care products.Information provided by Georgia GulfG..
Izod Impact, Notched 8.01 J/cm

@Thickness 3.17 mm,
Temperature 23.0 °C
15.0 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
ASTM D-256
Axiall HF-6597 Rigid PVC, Molding
Georgia Gulf HF-6597 is a high flow PVC compound designed for thin wall parts and multi-cavity molds. It is ideally suited for a variety of electrical and appliance applications.Information provide..
Izod Impact, Notched 8.01 J/cm

@Thickness 3.17 mm,
Temperature 23.0 °C
15.0 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
ASTM D-256
Axiall SP-7107 Rigid PVC, Molding
Georgia Gulf SP-7107 is a general purpose, electrical grade rigid vinyl injection molding compound characterized by excellent flow, heat stability, color hold and surface appearance. This makes it ..
Izod Impact, Notched 8.01 J/cm

@Thickness 3.17 mm,
Temperature 22.8 °C
15.0 ft-lb/in

@Thickness 0.125 in,
Temperature 73.0 °F
ASTM D-256
Axiall Suprel® 9422 Rigid PVC, Molding
Georgia Gulf Suprel® 9422 Alloy is engineered for injection molding applications that require outstanding impact resistance or toughness, particularly at low temperatures. This alloy complies with..
Izod Impact, Notched 8.01 J/cm

@Thickness 3.17 mm,
Temperature 22.8 °C
15.0 ft-lb/in

@Thickness 0.125 in,
Temperature 73.0 °F
ASTM D-256
Axiall Suprel® SVA 9420 Rigid PVC, Molding
Georgia Gulf Suprel® SVA 9420 Alloy is engineered for injection molding applications that require outstanding impact resistance or toughness, particularly at low temperatures. This alloy complies ..
Izod Impact, Notched 8.01 J/cm

@Thickness 3.17 mm,
Temperature 22.8 °C
15.0 ft-lb/in

@Thickness 0.125 in,
Temperature 73.0 °F
ASTM D-256
Axiall Suprel® SVA 9412 Rigid PVC, Molding
Georgia Gulf Suprel® SVA 9412 injection molding alloy features excellent impact resistance, excellent processing characteristics and comprehensive UL listings. The UL listings of Suprel 9412 inclu..
Izod Impact, Notched 8.01 J/cm

@Thickness 3.18 mm,
Temperature 23.0 °C
15.0 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Injection Molded; ASTM D256A
PolyOne Edgetek® XT XT-100-CX00 PC+PBT  (discontinued **)
EDGETEK™ XT High Performance Polymers are polycarbonate and polyester alloys that combine strength, durability and chemical resistance. The Edgetek XT product family includes a complete line of gen..
Izod Impact, Notched 8.01 J/cm

@Thickness 3.18 mm,
Temperature 23.0 °C
15.0 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Injection Molded; ASTM D256A
PolyOne Edgetek® XT XT-500-CX00 PC+PBT  (discontinued **)
EDGETEK™ XT High Performance Polymers are polycarbonate and polyester alloys that combine strength, durability and chemical resistance. The Edgetek XT product family includes a complete line of gen..