Mechanical Properties Metric English Comments
Izod Impact, Notched 1.82 J/cm

@Thickness 3.17 mm,
Temperature 22.8 °C
3.40 ft-lb/in

@Thickness 0.125 in,
Temperature 73.0 °F
ASTM-D256
Ineos ABS Lustran® 451 ABS, Injection Molding Grade
Lustran® ABS 451 is a soft flowing, medium impact injection molding resin designed with a unique balance of impact, heat resistance, flow, and gloss.
Izod Impact, Notched 1.82 J/cm

@Thickness 3.17 mm,
Temperature 22.8 °C
3.40 ft-lb/in

@Thickness 0.125 in,
Temperature 73.0 °F
ASTM D256
Techmer ES Elastoblend® PA6/6 GF13 IM HS BK 13% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 13% Filler by WeightAdditive: Heat Stabilizer, Impact Modifier and LubricantFeatures: Heat Stabilized, Impac..
Izod Impact, Notched 1.82 J/cm

@Thickness 3.17 mm,
Temperature -40.0 °C
3.40 ft-lb/in

@Thickness 0.125 in,
Temperature -40.0 °F
ASTM D256
Techmer ES Elastoblend® PA6/6 GF4 IM L LE
Availability: North AmericaForms: PelletsAdditive: Lubricant and Impact ModifierFeatures: Lubricant, Low Extractables and Impact ModifiedAppearance: Natural ColorInformation provided by TP Composite..
Izod Impact, Notched 1.82 J/cm

@Thickness 3.17 mm,
Temperature -40.0 °C
3.40 ft-lb/in

@Thickness 0.125 in,
Temperature -40.0 °F
ASTM D256
Techmer ES Elastoblend® PA6/6 HI BK Nylon 66
Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Lubricant and Impact ModifierFeatures: Heat Stabilized, Lubricant and Impact ModifiedUl File Number: E157318Appearance: BlackProce..
Izod Impact, Notched 1.82 J/cm

@Thickness 3.17 mm,
Temperature -40.0 °C
3.40 ft-lb/in

@Thickness 0.125 in,
Temperature -40.0 °F
ASTM D256
Techmer ES Elastoblend® PA6/6 IM L N Nylon 66
Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Lubricant and Impact ModifierFeatures: Heat Stabilized, Lubricant and Impact ModifiedUL File Number: E157318Processing Method: Inj..
Izod Impact, Notched 1.82 J/cm

@Thickness 3.17 mm,
Temperature -40.0 °C
3.40 ft-lb/in

@Thickness 0.125 in,
Temperature -40.0 °F
ASTM D256
Techmer ES Elastoblend® PA6/6 IM L W Nylon 66
Availability: North AmericaForms: PelletsAdditive: Lubricant and Impact ModifierFeatures: Lubricant and Impact ModifiedProcessing Method: Injection MoldingInformation provided by TP Composites, Inc...
Izod Impact, Notched 1.82 J/cm

@Thickness 3.17 mm,
Temperature 0.000 °C
3.40 ft-lb/in

@Thickness 0.125 in,
Temperature 32.0 °F
ASTM D256
Techmer ES Plastiblend® ABS 8004 UV
Availability: North AmericaForms: PelletsAdditive: UV StabilizerFeatures: Good UV Resistance and High Heat ResistanceInformation provided by TP Composites, Inc.
Izod Impact, Notched 1.82 J/cm

@Thickness 3.17 mm,
Temperature 0.000 °C
3.40 ft-lb/in

@Thickness 0.125 in,
Temperature 32.0 °F
ASTM D256
Techmer ES Plastiblend® ABS 8004 UV MB
Availability: North AmericaForms: PelletsAdditive: UV StabilizerFeatures: Good UV Resistance and High Heat ResistanceTPCI# 6816121Information provided by TP Composites, Inc.
Izod Impact, Notched 1.82 J/cm

@Thickness 3.17 mm,
Temperature 0.000 °C
3.40 ft-lb/in

@Thickness 0.125 in,
Temperature 32.0 °F
ASTM D256
Techmer ES Plastiblend® ABS 8012
Availability: North AmericaForms: PelletsProcessing Method: ExtrusionInformation provided by TP Composites, Inc.
Izod Impact, Notched 1.82 J/cm

@Thickness 3.17 mm,
Temperature 0.000 °C
3.40 ft-lb/in

@Thickness 0.125 in,
Temperature 32.0 °F
ASTM D256
Techmer ES Plastiblend® ABS 8014
Availability: North AmericaForms: PelletsProcessing Method: ExtrusionInformation provided by TP Composites, Inc.
Izod Impact, Notched 1.82 J/cm

@Thickness 3.17 mm,
Temperature -40.0 °C
3.40 ft-lb/in

@Thickness 0.125 in,
Temperature -40.0 °F
ASTM D256
Techmer ES Elastoblend® PA6/6 IM HS L BK Nylon 66
Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Lubricant and Impact ModifierFeatures: Heat Stabilized, Lubricant and Impact ModifiedProcessing Method: Injection MoldingInformati..
Izod Impact, Notched 1.82 J/cm

@Thickness 3.17 mm,
Temperature -40.0 °C
3.40 ft-lb/in

@Thickness 0.125 in,
Temperature -40.0 °F
ASTM D256
Techmer ES Elastoblend® PA6/6 IM L UV Nylon 66
Availability: North AmericaForms: PelletsAdditive: UV Stabilizer, Lubricant and Impact ModifierFeatures: Lubricant and Impact ModifiedProcessing Method: Injection MoldingInformation provided by TP C..
Izod Impact, Notched 1.82 J/cm

@Thickness 3.17 mm,
Temperature -40.0 °C
3.40 ft-lb/in

@Thickness 0.125 in,
Temperature -40.0 °F
ASTM D256
Techmer ES Elastoblend® PA6/6 IM X Nylon 66
Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Lubricant and Impact ModifierFeatures: Lubricant and Impact ModifiedProcessing Method: Injection MoldingInformation provided by TP..
Izod Impact, Notched 1.82 J/cm

@Thickness 3.17 mm,
Temperature 0.000 °C
3.40 ft-lb/in

@Thickness 0.125 in,
Temperature 32.0 °F
ASTM D256
Techmer ES Plastiblend® ABS 8004
Availability: North AmericaForms: PelletsFeatures: General Purpose and High Impact ResistanceInformation provided by TP Composites, Inc.
Izod Impact, Notched 1.82 J/cm

@Thickness 3.17 mm,
Temperature 0.000 °C
3.40 ft-lb/in

@Thickness 0.125 in,
Temperature 32.0 °F
ASTM D256
Techmer ES Plastiblend® ABS FR IM
Availability: North AmericaForms: PelletsFeatures: Flame Retardant and High Impact ResistanceProcessing Method: Injection MoldingInformation provided by TP Composites, Inc.
Izod Impact, Notched 1.82 J/cm

@Thickness 3.17 mm,
Temperature 0.000 °C
3.40 ft-lb/in

@Thickness 0.125 in,
Temperature 32.0 °F
ASTM D256
Techmer ES Plastiblend® ABS IM
Availability: North AmericaForms: PelletsFeatures: High Heat ResistanceInformation provided by TP Composites, Inc.