Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, 30% Glass Fiber Filled , Nylon 6, Heat Stabilized , Nylon 6, Impact Grade
Manufacturer Techmer ES
Trade Name Elastoblend®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Techmer ES Elastoblend® PA6 GF30 IM BK 30% Glass Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAdditive: Heat Stabilizer, Impact Modifier and LubricantFeatures: Heat Stabilized, Impact Modified and LubricatedAppearance: BlackInformation provided by TP Composites, Inc.
Physical Properties Metric English Comments
Density 1.34 g/cc
0.0484 lb/in³
ASTM D792
Water Absorption 1.5 %

@Time 86400 sec
1.5 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0035 cm/cm

@Thickness 3.17 mm
0.0035 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 120
120
ASTM D785
Tensile Strength, Yield 152 MPa
22100 psi
ASTM D638
Elongation at Break 4.0 %
4.0 %
ASTM D638
Flexural Strength 234 MPa
34000 psi
ASTM D790
Flexural Modulus 8.27 GPa
1200 ksi
ASTM D790
Izod Impact, Notched 1.01 J/cm

@Thickness 3.17 mm,
Temperature -40.0 °C
1.90 ft-lb/in

@Thickness 0.125 in,
Temperature -40.0 °F
ASTM D256
2.03 J/cm

@Thickness 3.17 mm,
Temperature 22.8 °C
3.80 ft-lb/in

@Thickness 0.125 in,
Temperature 73.0 °F
ASTM D256
Izod Impact, Unnotched 13.9 J/cm

@Thickness 3.17 mm
26.0 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 36.0 µm/m-°C
20.0 µin/in-°F
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 210 °C
410 °F
Unannealed; ASTM D648
Flammability, UL94 HB

@Thickness 1.50 mm
HB

@Thickness 0.0591 in
Electrical Properties Metric English Comments
Volume Resistivity 2.00e+13 ohm-cm
2.00e+13 ohm-cm
ASTM D257
Dielectric Strength 15.4 kV/mm
390 kV/in
Method A (Short-Time); ASTM D149