Indorama Auriga Polymers Polyclearâ„¢ Splash 3301 PET Resin

Category Polymer , Thermoplastic , Polyester, TP , Polyethylene Terephthalate (PET) , Polyethylene Terephthalate (PET), Unreinforced
Manufacturer Indorama Auriga Polymers
Trade Name Polyclear™ Splash
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Indorama Auriga Polymers Polyclearâ„¢ Splash 3301 PET Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Polyclear® Splash PET 3301 is a copolymer packaging resin with a nominal intrinsic viscosity of 0.74 dl/g. Polyclear® Splash PET 3301 is designed to provide very low regenerated acetaldehyde levels in injection molding, and is noted for its excellent color and clarity. Polyclear® Splash PET 3301 resin been used successfully in water bottles, as well as in custom container applications. The polymer complies with the Federal Food, Drug and Cosmetic Act for certain food applications. Please contact Auriga Polymers Inc. for specific FDA clearances. Polyclear® Splash PET 3301 offers excellent performance in maximum through put injection molding and stretch-blow molding applications. Containers made from Auriga Polymers Inc. PET are lightweight, have excellent clarity, and are shatterproof. With the important advantage of being totally recyclable, PET is the packaging material of choice.
Physical Properties Metric English Comments
Bulk Density >= 0.833 g/cc
>= 0.0301 lb/in³
Density >= 1.39 g/cc
>= 0.0502 lb/in³
Pycnometer
Particle Mesh Size 28 Mesh
28 Mesh
0.05% through; Gravimetric determination as manufactured
Viscosity Measurement 0.72 - 0.76
0.72 - 0.76
Intrinsic; 1% Solution in Dichloroacetic Acid
Crystallinity >= 50 %
>= 50 %
Pycnometer
Thermal Properties Metric English Comments
Melting Point <= 248 °C
<= 478 °F
DSC
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
clear; thickness not quantified
Chemical Properties Metric English Comments
Acetaldehyde <= 1.00 ppm
<= 1.00 ppm
Gas Chromatography
Diethylene Glycol <= 2.3 %
<= 2.3 %
Gas Chromatography
Carboxyl End Groups <= 45 meq/kg
<= 45 meq/kg
Titration
Processing Properties Metric English Comments
Moisture Content <= 0.10 %
<= 0.10 %
Karl Fisher Titration as manufactured
Descriptive Properties Value Comments
Chip Size < 2 grams/100 chips
Process Blow Molding
Injection Molding