Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 2.00e+13 ohm-cm | 2.00e+13 ohm-cm | Z direction; C96/35/90; ASTM D257 |
Rogers Corporation RT/duroid® 5870 Glass Microfiber Reinforced PTFE High Frequency Laminate RT/duroid® 5870 and 5880 glass microfiber reinforced PTFE composites are designed for exacting stripline and microstrip circuit applications. Glass reinforcing microfibers are randomly oriented to.. |
|||
Volume Resistivity | 2.00e+13 ohm-cm | 2.00e+13 ohm-cm | Z direction; C96/35/90; ASTM D257 |
Rogers Corporation RT/duroid® 5880 Glass Microfiber Reinforced PTFE High Frequency Laminate RT/duroid® 5870 and 5880 glass microfiber reinforced PTFE composites are designed for exacting stripline and microstrip circuit applications. Glass reinforcing microfibers are randomly oriented to.. |
|||
Volume Resistivity | 2.00e+13 ohm-cm | 2.00e+13 ohm-cm | Condition A; IPC 2.5.17.1 |
Rogers Corporation RT/duroid® 6006 Ceramic-PTFE Composite Microwave Laminate Features:High dielectric constant for circuit size reductionLow loss - Ideal for operating at X-band or belowTight dielectric constant and thickness control for repeatable circuit performanceLow moi.. |
|||
Volume Resistivity | 2.00e+13 ohm-cm | 2.00e+13 ohm-cm | ASTM D257 |
Permabond TA4310 Toughened Acrylic Adhesive PERMABOND® TA4310 is a 2-part, 1:1 toughened acrylic adhesive. Its toughening makes it ideal for bonding dissimilar materials where differential thermal expansion and contraction could be an issue... |
|||
Volume Resistivity | 2.00e+13 ohm-cm | 2.00e+13 ohm-cm | ASTM D257 |
Permabond TA435 Toughened Acrylic Adhesive & Initiator PERMABOND TA435 is a structural acrylic adhesive designed primarily for bonding metals, ferrites, ceramics and some thermoplastics. This adhesive may be used in a variety of structural bonding appli.. |
|||
Volume Resistivity | 2.00e+13 ohm-cm | 2.00e+13 ohm-cm | ASTM D257 |
Permabond TA440 Toughened Acrylic Adhesive PERMABOND TA440 is a two component structural acrylic adhesive suitable for bonding metals, glass, wood, ferrites, ceramics and some rigid plastics. This adhesive may be used in a variety of structu.. |
|||
Volume Resistivity | 2.00e+13 ohm-cm | 2.00e+13 ohm-cm | ASTM D257 |
Permabond TA4302 Toughened Acrylic Adhesive PERMABOND® TA4302 is a 2-part, 1:1 toughened acrylic adhesive. It can be used to bond a wide variety of materials including metals, plastics, GRP, ceramics, wood and other substrates. It is conveni.. |
|||
Volume Resistivity | 2.00e+13 ohm-cm | 2.00e+13 ohm-cm | ASTM D257 |
Techmer ES Elastoblend® PA6 GF30 IM BK 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAdditive: Heat Stabilizer, Impact Modifier and LubricantFeatures: Heat Stabilized, Impac.. |
|||
Volume Resistivity | 2.00e+13 ohm-cm | 2.00e+13 ohm-cm | ASTM D257 |
Techmer ES Elastoblend® PA6 GF30 IM L 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAdditive: Impact Modifier and LubricantFeatures: Impact Modified and LubricatedUL File N.. |
|||
Volume Resistivity | 2.00e+13 ohm-cm | 2.00e+13 ohm-cm | ASTM D257 |
Techmer ES Elastoblend® PA6 GF33 IM2 BK 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Heat Stabilizer, Impact Modifier and LubricantFeatures: Heat Stabilized, Impac.. |
|||
Volume Resistivity | 2.00e+13 ohm-cm | 2.00e+13 ohm-cm | ASTM D257 |
Techmer ES Elastoblend® PA6 GF33 IM3 BK 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Heat Stabilizer, Impact Modifier and LubricantFeatures: Heat Stabilized, Impac.. |
|||
Volume Resistivity | 2.00e+13 ohm-cm | 2.00e+13 ohm-cm | ASTM D257 |
Techmer ES Elastoblend® PA6 GF40 IM HS UV RD 40% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by WeightAdditive: Impact ModifierFeatures: Impact ModifiedUL File Number: E157318Processing Meth.. |
|||
Volume Resistivity | 2.00e+13 ohm-cm | 2.00e+13 ohm-cm | ASTM D257 |
Techmer ES Elastoblend® PA6 IM 407 L Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Impact Modifier and LubricantFeatures: Heat Stabilized, Impact Modified and LubricatedInformation provided by TP Composites, Inc. |
|||
Volume Resistivity | 2.00e+13 ohm-cm | 2.00e+13 ohm-cm | ASTM D257 |
Techmer ES Elastoblend® PA6 IM 409 L MB Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Impact Modifier and LubricantFeatures: Heat Stabilized, Impact Modified and LubricatedInformation provided by TP Composites, Inc. |
|||
Volume Resistivity | 2.00e+13 ohm-cm | 2.00e+13 ohm-cm | ASTM D257 |
Techmer ES Elastoblend® PA6 IM 435 HS L Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Impact Modifier and LubricantFeatures: Heat Stabilized, Impact Modified and LubricatedUses: Low Temperature ApplicationsInformatio.. |
|||
Volume Resistivity | 2.00e+13 ohm-cm | 2.00e+13 ohm-cm | ASTM D257 |
Techmer ES Elastoblend® PA6 IM L Availability: North AmericaForms: PelletsAdditive: Impact Modifier and LubricantFeatures: Impact Modified and LubricatedInformation provided by TP Composites, Inc. |
|||
Volume Resistivity | 2.00e+13 ohm-cm | 2.00e+13 ohm-cm | ASTM D257 |
Techmer ES Elastoblend® PA6 IM L W N Availability: North AmericaForms: PelletsAdditive: Impact Modifier and LubricantFeatures: Impact Modified and LubricatedAppearance: Natural ColorInformation provided by TP Composites, Inc. |
|||
Volume Resistivity | 2.00e+13 ohm-cm | 2.00e+13 ohm-cm | ASTM D257 |
Techmer ES Elastoblend® PA6 IM X Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Impact Modifier and LubricantFeatures: Heat Stabilized, Impact Modified and LubricatedProcessing Method: Injection MoldingInformat.. |
|||
Volume Resistivity | 2.00e+13 ohm-cm | 2.00e+13 ohm-cm | ASTM D257 |
Techmer ES Elastoblend® TPX-PA6/6 97058 BK 32% Mineral Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Mineral Fiber Reinforcement, 33% Filler by WeightAdditive: Impact Modifier and LubricantFeatures: Impact Modified and LubricatedUL File.. |
|||
Volume Resistivity | 2.00e+13 ohm-cm | 2.00e+13 ohm-cm | ASTM D257 |
Techmer ES Plastiblend® PA6/ABS 1120 B1 Availability: North AmericaForms: PelletsAdditive: Impact ModifierFeatures: Impact ModifiedUL File Number: E157318Information provided by TP Composites, Inc. |
|||
Volume Resistivity | 2.00e+13 ohm-cm | 2.00e+13 ohm-cm | ASTM D257 |
Techmer ES Plastiblend® PA6/ABS 1120 GF4 4% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 4% Filler by WeightAdditive: Impact ModifierFeatures: Impact ModifiedInformation provided by TP Composites, .. |
|||
Volume Resistivity | 2.00e+13 ohm-cm | 2.00e+13 ohm-cm | ASTM D257 |
Techmer ES HiFill® PA6 LGF30 HS L 12mm 30% Glass/Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass/Carbon Fiber Reinforcement, 35% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedIn.. |
|||
Volume Resistivity | 2.00e+13 ohm-cm | 2.00e+13 ohm-cm | IEC 60093 |
Unitika A1030GFL45 PA6, 45% Glass Fiber Reinforced, Dry Information provided by Unitika Ltd. |
|||
Volume Resistivity | 2.00e+13 ohm-cm | 2.00e+13 ohm-cm | ASTM D257 |
Toyobo PELPRENE™ S2004FS Polyester TPE, Flame Resistant Features: Polyester TPE, Flame ResistantInformation provided by Toyobo. |
|||
Volume Resistivity | >= 2.00e+13 ohm-cm | >= 2.00e+13 ohm-cm | |
Epoxy Technology EPO-TEK® 302 Fast Setting, Optical Epoxy Product Description: EPO-TEK® 302 is a two component, fast-gelling, room temperature curing epoxy, designed for electronic, optical, medical, and general applications. Advantages & Application No.. |
|||
Volume Resistivity | <= 2.00e+13 ohm-cm | <= 2.00e+13 ohm-cm | |
Epoxy Technology EPO-TEK® 360T High Temperature Epoxy Material Description: A two component, high-temperature grade, electrically and thermally insulating epoxy for semiconductor, electronics, fiber optics and medical applications. It is a thixotropic.. |
|||
Volume Resistivity | 2.00e+13 ohm-cm | 2.00e+13 ohm-cm | IEC 60093 |
Azoty Tarnow™ TARFLEN SM-S25 PTFE Tarflen SM1 reinforced with 25% glass fiber for standard compression molding.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A. |