Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 152 MPa | 22100 psi | ASTM D638 |
Techmer ES Elastoblend® PA6 GF30 IM BK 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAdditive: Heat Stabilizer, Impact Modifier and LubricantFeatures: Heat Stabilized, Impac.. |
|||
Tensile Strength, Yield | 152 MPa | 22100 psi | ASTM D638 |
Techmer ES Elastoblend® PA6 GF33 IM2 BK 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Heat Stabilizer, Impact Modifier and LubricantFeatures: Heat Stabilized, Impac.. |
|||
Tensile Strength, Yield | 152 MPa | 22100 psi | ASTM D638 |
Techmer ES HiFill FR® PA6 GF33 FR HS L 33% Glass Filled (Dry) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Flame Retardant, Heat Stabilized and Lu.. |
|||
Tensile Strength, Yield | 152 MPa | 22100 psi | ASTM D638 |
Techmer ES HiFill® PA6 LGF30 HS L 12mm 30% Glass/Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass/Carbon Fiber Reinforcement, 35% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedIn.. |