Material Notes:
TSE-EcoSPRAY® SS100 is an “Environmentally-Preferred Product” or EPP. It is an Aliphatic polyurethane resin free of Styrene, and is an “ultra-low” emitting resin during application. TSE-EcoSPRAY® SS100 is designed for the manufacturing of solid surfaces. This polyurethane is aliphatic. Therefore, solid surface technology manufactured using TSE-EcoSPRAY® SS100 exhibit excellent weather ability and good chemical resistance against weak acids and bases.All information provided by TSE Industries
Physical Properties Metric English Comments
Specific Gravity 1.08 g/cc

@Temperature 23.9 °C
1.08 g/cc

@Temperature 75.0 °F
Viscosity 2000 cP

@Temperature 23.9 °C
2000 cP

@Temperature 75.0 °F
Mechanical Properties Metric English Comments
Hardness, Barcol 45 - 48
45 - 48
clear casting
Tensile Strength, Yield 70.3 MPa
10200 psi
Clear Casting
Tensile Modulus 2.67 GPa
387 ksi
clear casting
Flexural Strength 87.6 MPa
12700 psi
clear casting
Flexural Modulus 2.51 GPa
364 ksi
clear casting
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 58.0 °C
136 °F
clear casting; unspecified load
Processing Properties Metric English Comments
Gel Time 40.0 - 60.0 min

@Temperature 23.9 °C
40.0 - 60.0 min

@Temperature 75.0 °F
when reacted at 1:1.3 by weight, based on the application
Shelf Life 6.00 Month

@Temperature 23.9 °C
6.00 Month

@Temperature 75.0 °F
Sealed containers should be stored between 75ºF and 95ºF