Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 2.67 GPa | 387 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics Cycolac® MG8000SR ABS This data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Modulus | 2.67 GPa | 387 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics Cycolac® MG8000SR ABS (Asia Pacific) This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Tensile Modulus | 2.67 GPa | 387 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics Cycolac® MG8000SR ABS (Europe-Africa-Middle East) This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Tensile Modulus | 2.67 GPa | 387 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Cycoloy® CY2010 PC+ABS (Europe-Africa-Middle East) Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering hydrolytic stability and excellent flow for a wide variety of thin wall or large size applicat.. |
|||
Tensile Modulus | 2.67 GPa | 387 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Cycoloy® CY5000 PC+ABS Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering hydrolytic stability and excellent flow for a wide variety of thin wall or large size applicat.. |
|||
Tensile Modulus | 2.67 GPa | 387 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Cycoloy® CY5000 PC+ABS (Asia Pacific) Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering hydrolytic stability and excellent flow for a wide variety of thin wall or large size applicat.. |
|||
Tensile Modulus | 2.67 GPa | 387 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Cycoloy® CY5000 PC+ABS (Europe-Africa-Middle East) Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering hydrolytic stability and excellent flow for a wide variety of thin wall or large size applicat.. |
|||
Tensile Modulus | 2.67 GPa | 387 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Cycoloy® CY5005 PC+ABS Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering hydrolytic stability and excellent flow for a wide variety of thin wall or large size applicat.. |
|||
Tensile Modulus | 2.67 GPa | 387 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Cycoloy® CY6010 PC+ABS Cycoloy CY6010 resin is a flame retardant PC/ABS blend featuring excellent flow together with good impact and UL-94 V0 listing at 1.5mm. Its excellent flow combined with balanced heat and good pract.. |
|||
Tensile Modulus | 2.67 GPa | 387 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Cycoloy® CY6010 PC+ABS (Asia Pacific) Cycoloy CY6010 resin is a flame retardant PC/ABS blend featuring excellent flow together with good impact and UL-94 V0 listing at 1.5mm. Its excellent flow combined with balanced heat and good pract.. |
|||
Tensile Modulus | 2.67 GPa | 387 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Cycoloy® CY6010 PC+ABS (Europe-Africa-Middle East) Cycoloy CY6010 resin is a flame retardant PC/ABS blend featuring excellent flow together with good impact and UL-94 V0 listing at 1.5mm. Its excellent flow combined with balanced heat and good pract.. |
|||
Tensile Modulus | 2.67 GPa | 387 ksi | 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Geloy EXGY30CP ASA Pearlescent GELOY ASA resin with copper-look for capstock extrusion. Outstanding weatherability.This data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Modulus | 2.67 GPa | 387 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® BPL1000 PC Lexan* BPL1000 Polycarbonate (PC) resin is an injection moldable grade featuring high flow and good impact peroformance. It contains non-chlorinated and non-brominated flame retardant systems with U.. |
|||
Tensile Modulus | 2.67 GPa | 387 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® BPL1000 PC (Asia Pacific) Lexan* BPL1000 Polycarbonate (PC) resin is an injection moldable grade featuring high flow and good impact peroformance. It contains non-chlorinated and non-brominated flame retardant systems with U.. |
|||
Tensile Modulus | 2.67 GPa | 387 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® BPL1000 PC (Europe-Africa-Middle East) Lexan* BPL1000 Polycarbonate (PC) resin is an injection moldable grade featuring high flow and good impact peroformance. It contains non-chlorinated and non-brominated flame retardant systems with U.. |
|||
Tensile Modulus | 2.67 GPa | 387 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics Lexan® ML7677A PC (Asia Pacific) Commercial grade for Polycarbonate in only nature color. Excellent processability, super high flow, flame retardant, UL rated V-1 at 2.0mm.This data was supplied by SABIC-IP for the Asia Pacific reg.. |
|||
Tensile Modulus | 2.67 GPa | 387 ksi | 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Geloy FXTW30CP ASA Pearlescent GELOY ASA resin with copper-look for capstock extrusion. Outstanding weatherability.This data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Modulus | 2.67 GPa | 387 ksi | clear casting |
TSE Industries EcoSPRAY® SS100 Aliphatic Polyurethane Resin TSE-EcoSPRAY® SS100 is an “Environmentally-Preferred Product” or EPP. It is an Aliphatic polyurethane resin free of Styrene, and is an “ultra-low” emitting resin during application. TSE-EcoSPRA.. |
|||
Tensile Modulus | 2.67 GPa | 387 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® SLDM310 PC (Asia Pacific) Mineral filled Antistatic Polycarbonate, HDT110degC type |
|||
Tensile Modulus | 2.67 GPa | 387 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL PX6120 PPE+PS (Asia Pacific) Noryl PX6120 is an unfilled material with good flow, high Impact and chemical resistance against cleaners. Noryl PX6120 is developed for personal care appplications. |
|||
Tensile Modulus | 2.67 GPa | 387 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL PX6120 PPE+PS (Europe-Africa-Middle East) Noryl PX6120 is an unfilled material with good flow, high Impact and chemical resistance against cleaners. Noryl PX6120 is developed for personal care appplications. |
|||
Tensile Modulus | 2.67 GPa | 387 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics NORYL SE1X PPE+PS PPE+PS blend. Unfilled. Non-brominated, non-chlorinated FR system. UL94 V1, UL746C F1. Dielectric strength. Suitable for E/E market indoor/outdoor applications. |
|||
Tensile Modulus | 2.67 GPa | 387 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP IBP34 PA6.12 LNP* LUBRICOMP* IBP34 is a compound based on Nylon 6/12 containing 20% Glass Bead, 15% PTFE/Silicone. Added features include: Wear Resistant. |
|||
Tensile Modulus | 2.67 GPa | 387 ksi | 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Valox® 295 PBT Unreinforced PBTThis data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Modulus | 2.67 GPa | 387 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL PVX0800 PPE NORYL* PVX0800 resin is a high flow, V0 = 1.5 mm grade, suitable for a variety of electronics applications. |
|||
Tensile Modulus | 2.67 GPa | 387 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP STAT-KON DX09301C PC (Asia Pacific) Low Ionic, Low Outgassing, Low LPC and ESD safe Polycarbonate compound suitable for Semiconductor and Hard Disk Drive (HDD) application.Added features of this material include: Clean Compounding Sys.. |
|||
Tensile Modulus | 2.67 GPa | 387 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics NORYL GTX GTX673 PPE+PA Conductive Noryl GTX* resin designed for profile extrusion. This grade can be electrostatic or powder coat painted without the need for a primer. In addition, its high heat capability allows it to .. |
|||
Tensile Modulus | 2.67 GPa | 387 ksi | clear casting |
TSE Industries EcoSPRAY® SS100 Aliphatic Polyurethane Resin TSE-EcoSPRAY® SS100 is an “Environmentally-Preferred Product” or EPP. It is an Aliphatic polyurethane resin free of Styrene, and is an “ultra-low” emitting resin during application. TSE-EcoSPRA.. |
|||
Tensile Modulus | 2.67 GPa | 388 ksi | Storage |
Epoxy Technology EPO-TEK® 323LP Epoxy Material Description: Longer pot life version of EPO-TEK® 353ND designed for semiconductor, hybrid, fiber-optic, hard-disk drive and medical applications.Information Provided by Epoxy Technology |
|||
Tensile Modulus | 2.67 GPa | 388 ksi | Storage |
Epoxy Technology EPO-TEK® OM125 Optical Epoxy Product Description: EPO-TEK® OM125 is two component, high Tg, optical epoxy designed for bonding multi-mode fiber optic connectors. Advantages & Application Notes: Color coded blue for easy operat.. |