Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 87.4 MPa | 12700 psi | ASTM D790 |
PolyOne Geon™ Vinyl Dry Blend E7130 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Flexural Strength | 87.6 MPa @Temperature 175 °C |
12700 psi @Temperature 347 °F |
ISO 178 |
Solvay Specialty Polymers Amodel® AFA-6133 V0 Z Polyphthalamide (PPA)
(Unverified Data**) Amodel AFA-6133 V0 Z is a 33% glass-fiber reinforced, flame retardant grade of polyphthalamide (PPA) resin specifically formulated for connector applications requiring compatibility with both infrar.. |
|||
Flexural Strength | 87.6 MPa | 12700 psi | clear casting |
TSE Industries EcoSPRAY® SS100 Aliphatic Polyurethane Resin TSE-EcoSPRAY® SS100 is an “Environmentally-Preferred Product” or EPP. It is an Aliphatic polyurethane resin free of Styrene, and is an “ultra-low” emitting resin during application. TSE-EcoSPRA.. |
|||
Flexural Strength | 87.6 MPa @Temperature 175 °C |
12700 psi @Temperature 347 °F |
4; ISO 178 |
Solvay Specialty Polymers Amodel® AFA-6133 V0 Z Polyphthalamide (PPA), 33% Glass Fiber (Dry) Amodel® AFA-6133 V0 Z is a 33% glass-fiber reinforced, flame retardant grade of polyphthalamide (PPA) resin specifically formulated for connector applications requiring compatibility with both in.. |
|||
Flexural Strength | 87.3 MPa | 12700 psi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Infino® NE-1030 PC/ABS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Flexural Strength | 87.3 MPa | 12700 psi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Starex® BF-0930 MABS, Unreinforced Scratch Resistant Scratch resistantInformation provided by Samsung Cheil Industries. |
|||
Flexural Strength | 87.3 MPa | 12700 psi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Infino® NE-1030 PC/ABS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Flexural Strength | 87.3 MPa | 12700 psi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Starex® BF-0930 MABS, Unreinforced Scratch Resistant Scratch resistantInformation provided by Samsung Cheil Industries. |
|||
Flexural Strength | 87.6 MPa | 12700 psi | clear casting |
TSE Industries EcoSPRAY® SS100 Aliphatic Polyurethane Resin TSE-EcoSPRAY® SS100 is an “Environmentally-Preferred Product” or EPP. It is an Aliphatic polyurethane resin free of Styrene, and is an “ultra-low” emitting resin during application. TSE-EcoSPRA.. |
|||
Flexural Strength | 87.9 MPa | 12700 psi | UNI EN ISO 14125: 2000 |
CRP Technology Windform® GT Polyamide Glass Composite Processed by selective laser sintering (SLS). Windform® GT is a deep and dark black composite material based on polyamide fiber glass. After hand finishing, the color becomes shining and brighter... |
|||
Flexural Strength | 87.5 MPa @Temperature 23.0 °C |
12700 psi @Temperature 73.4 °F |
EN ISO 178 |
Ensinger TECASINT™ 2031 Polyimide, 40% Graphite Filled (PI) TECASINT™ 2000 series of polyimide stock shapes provide a superior combination of high temperature and bearing and wear, properties that make it an ideal choice for the most demanding applications... |
|||
Flexural Strength | 87.6 MPa | 12700 psi | ASTM D790 |
Asahi Kasei Thermylene® P-20FG-1740 20% Glass Fiber Reinforced, Medium Impact Information provided by Asahi Thermofil |