Processing Properties | Metric | English | Comments |
---|---|---|---|
Gel Time | 30.0 - 60.0 min | 30.0 - 60.0 min | |
Resin Technology Group FDA-24N Two component Polyurethane Adhesive Resin Technology Group FDA-24N Two component Polyurethane AdhesiveFDA approvable, 1:1 ratio, general purpose adhesive |
|||
Gel Time | 40.0 - 60.0 min @Temperature 23.9 °C |
40.0 - 60.0 min @Temperature 75.0 °F |
when reacted at 1:1.3 by weight, based on the application |
TSE Industries EcoSPRAY® SS100 Aliphatic Polyurethane Resin TSE-EcoSPRAY® SS100 is an “Environmentally-Preferred Product” or EPP. It is an Aliphatic polyurethane resin free of Styrene, and is an “ultra-low” emitting resin during application. TSE-EcoSPRA.. |
|||
Gel Time | 40.0 - 60.0 min @Temperature 23.9 °C |
40.0 - 60.0 min @Temperature 75.0 °F |
when reacted at 1:1.3 by weight, based on the application |
TSE Industries EzNATE® SS100 Aliphatic Polyurethane Resin TSE-EcoSPRAY® SS100 is an “Environmentally-Preferred Product” or EPP. It is an Aliphatic polyurethane resin free of Styrene, and is an “ultra-low” emitting resin during application. TSE-EcoSPRA.. |
|||
Gel Time | 45.0 - 60.0 min @Temperature 60.0 °C |
45.0 - 60.0 min @Temperature 140 °F |
with 0.2%wt catalyst load |
Hybrid Plastics FireQuench® PM 1287 Resin FireQuench® PM1287 is an optically transparent, fire retardant hybrid nanocomposite resin that can serve as a replacement for standard epoxy-vinyl ester and related resins. It can be employed as .. |
|||
Gel Time | 40.0 - 60.0 min @Temperature 23.9 °C |
40.0 - 60.0 min @Temperature 75.0 °F |
when reacted at 1:1.3 by weight, based on the application |
TSE Industries EcoSPRAY® SS100 Aliphatic Polyurethane Resin TSE-EcoSPRAY® SS100 is an “Environmentally-Preferred Product” or EPP. It is an Aliphatic polyurethane resin free of Styrene, and is an “ultra-low” emitting resin during application. TSE-EcoSPRA.. |
|||
Gel Time | 40.0 - 60.0 min @Temperature 23.9 °C |
40.0 - 60.0 min @Temperature 75.0 °F |
when reacted at 1:1.3 by weight, based on the application |
TSE Industries EzNATE® SS100 Aliphatic Polyurethane Resin TSE-EcoSPRAY® SS100 is an “Environmentally-Preferred Product” or EPP. It is an Aliphatic polyurethane resin free of Styrene, and is an “ultra-low” emitting resin during application. TSE-EcoSPRA.. |