Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Styron Magnumâ„¢ 780HP ABS, High Heat, High Impact

Category Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), Heat Resistant, Molded
Manufacturer Styron
Trade Name Magnum™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Styron Magnumâ„¢ 780HP ABS, High Heat, High Impact.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM ABS resin are available in a wide range of melt flow rates, impact strength and heat resistance for both high and low gloss applications manufactured by injection molding, sheet or profile extrusion and thermoforming.MAGNUM® 780HP ABS resin is a low gloss, high heat, high impact grade designed for use in small household appliances. It offers a good balance of physical properties and excellent injection molding characteristics.Data provided by Dow Chemical.This product line was spun off from Dow Chemical to Styron in 2010.
Physical Properties Metric English Comments
Density 1.04 g/cc
0.0376 lb/in³
ASTM Data
Linear Mold Shrinkage 0.0055 cm/cm
0.0055 in/in
Melt Flow 3.0 g/10 min

@Load 3.80 kg,
Temperature 230 °C
3.0 g/10 min

@Load 8.38 lb,
Temperature 446 °F
ASTM Data
Mechanical Properties Metric English Comments
Hardness, Rockwell R 108
108
Tensile Strength, Yield 44.8 MPa
6500 psi
ASTM Data
Elongation at Yield 2.5 %
2.5 %
ISO Data
Tensile Modulus 2.07 GPa
300 ksi
ASTM Data
Izod Impact, Notched 2.40 J/cm
4.50 ft-lb/in
ASTM Data
Charpy Impact Unnotched NB
NB
ISO Data
NB
NB
ISO Data, Low Temp
Charpy Impact, Notched 0.700 J/cm²
3.33 ft-lb/in²
ISO Data, Low Temp
2.00 J/cm²
9.52 ft-lb/in²
ISO Data
Impact Test 45.0 J

@Temperature 23.0 °C
33.2 ft-lb

@Temperature 73.4 °F
Instrumented Dart Total Energy
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 78.0 µm/m-°C

@Temperature 20.0 °C
43.3 µin/in-°F

@Temperature 68.0 °F
ISO data
Deflection Temperature at 0.46 MPa (66 psi) 96.1 °C
205 °F
Unannealed; ASTM Data
Deflection Temperature at 1.8 MPa (264 psi) 83.0 °C
181 °F
Unannealed; 103°C (217°F) annealed; ASTM Data
Vicat Softening Point 111 °C
232 °F
Optical Properties Metric English Comments
Gloss 52.5 %
52.5 %
Gardner Gloss, 60°
Users viewing this material also viewed the following: