Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.0055 - 0.010 cm/cm | 0.0055 - 0.010 in/in | ASTM D955 |
Multibase Multi-Pro® 3010 X Black Polypropylene Forms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase |
|||
Linear Mold Shrinkage | 0.0055 cm/cm | 0.0055 in/in | |
Plastcom SLOVAMID 6 GF 30 006/1M PA6 reinforced with 30% glass fibre Features: PA 6 for injection moulding, chemically strengthened with 30% of milled glass fibre, for mouldings with high strength and toughness used in the automotive, electrical, engineering and cons.. |
|||
Linear Mold Shrinkage | 0.0055 cm/cm | 0.0055 in/in | |
Plastcom SLOVAMID 6 GF 33 PA6, 33% glass fibre FeaturesPA 6 for injection moulding, chemically strengthened with 33% of glass fibre, for mouldings with high strength and toughness used in the automotive, electrical, engineering and consumer-good.. |
|||
Linear Mold Shrinkage | 0.0055 cm/cm | 0.0055 in/in | STN 64 0808 |
Plastcom SLOVASTER® B GF 30 FRK 3 Polybutylene Terephthalate, 30% Chemically Coupled Glass Fiber, Red Phosphorus Flame Retardant FeaturesPBT with the content of 30% chemically coupled glass fiber and flame retardant based on red phosphorus. Anisotropy of shrinkage enables injection moulding of round, cylindrical or other hol.. |
|||
Linear Mold Shrinkage | 0.0055 cm/cm | 0.0055 in/in | |
Plastcom SLOVASTER® B1 GF 45 PBT, 45% glass fibre FeaturesPBT for injection moulding, chemically reinforced with 45% glass fibre. Characterised by excellent properties also at minus temperatures like eg. modulus of elasticity in tension and bending.. |
|||
Linear Mold Shrinkage | 0.0055 cm/cm | 0.0055 in/in | STN 64 0808 |
Plastcom SLOVAMID 6 GF 30 Polyamide 6, 30% Glass Fiber FeaturesPA 6 for injection moulding, chemically strengthened with 30% of glass fiber, for mouldings with high strength and toughness used in the automotive, electrical, engineering and consumer-good.. |
|||
Linear Mold Shrinkage | 0.0055 cm/cm | 0.0055 in/in | Isotropy |
Solvay TECHNYL® A 218 V50 PA66, 50% glass fiber, DRY Description: TECHNYL® A 218 V50 is a polyamide 66, reinforced with 50% of glass fiber, heat stabilized, for injection molding. This product is available in natural and black colors.Benefits: The .. |
|||
Linear Mold Shrinkage | 0.0055 cm/cm | 0.0055 in/in | ASTM Data; MD |
Styrolution Luran® S 777 K ASA Luran S 777 K is an easy flowing injection molding ASA grade with good toughness and heat distorsion resistance. |
|||
Linear Mold Shrinkage | 0.0055 cm/cm | 0.0055 in/in | ASTM Data; MD |
Styrolution Terluran® GP-22 ABS Terluran GP-22 is an easy flowing grade of ABS for injection molding with high resistance to impact and heat deflection.Information provided by STYROLUTION, which is a joint venture between BASF and.. |
|||
Linear Mold Shrinkage | 0.0055 cm/cm | 0.0055 in/in | ASTM Data; MD |
Styrolution Terluran® GP-35 ABS Terluran GP-35 is a very high flow grade of ABS for injection molding with good resistance to impact and heat deflection.Information provided by STYROLUTION, which is a joint venture between BASF an.. |
|||
Linear Mold Shrinkage | 0.0055 cm/cm | 0.0055 in/in | ASTM Data; MD |
Styrolution Terluran® HH-106 ABS Terluran HH-106 is an injection molding ABS grade with high resistance to heat deformation and impact.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS. |
|||
Linear Mold Shrinkage | 0.0055 cm/cm | 0.0055 in/in | |
Styron Magnum™ 2642 ABS, Impact Grade MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Linear Mold Shrinkage | 0.0055 cm/cm | 0.0055 in/in | |
Styron Magnum™ 4455 ABS MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Linear Mold Shrinkage | 0.0055 cm/cm | 0.0055 in/in | |
Styron Magnum™ 545 ABS, General Purpose MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Linear Mold Shrinkage | 0.0055 cm/cm | 0.0055 in/in | |
Styron Magnum™ 9010 ABS, High Gloss MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Linear Mold Shrinkage | 0.0055 cm/cm | 0.0055 in/in | |
Styron Magnum™ 941 ABS MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Linear Mold Shrinkage | 0.0055 cm/cm | 0.0055 in/in | |
Styron Magnum™ 9555 ABS, High Impact MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Linear Mold Shrinkage | 0.0055 cm/cm | 0.0055 in/in | |
Styron Magnumâ„¢ FG960 ABS, High Impact MAGNUM ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM ABS .. |
|||
Linear Mold Shrinkage | 0.0055 cm/cm | 0.0055 in/in | |
Styron Magnum™ SPD 214 ABS MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Linear Mold Shrinkage | 0.0055 cm/cm | 0.0055 in/in | |
Styron Magnum™ 213 ABS, General Purpose MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Linear Mold Shrinkage | 0.0055 cm/cm | 0.0055 in/in | |
Styron Magnum™ 347EZ ABS MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Linear Mold Shrinkage | 0.0055 cm/cm | 0.0055 in/in | |
Styron Magnum™ 357HP ABS, High Heat MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Linear Mold Shrinkage | 0.0055 cm/cm | 0.0055 in/in | ASTM D955 |
Adell BL-18 Nylon 6, 40% Glass Reinforced; Mineral Filled Data provided by Adell Plastics, Inc. |
|||
Linear Mold Shrinkage | 0.0055 cm/cm | 0.0055 in/in | ASTM D955 |
Adell AT-34 Nylon 66, 20% Glass Reinforced; Impact Modified Data provided by Adell Plastics, Inc. |
|||
Linear Mold Shrinkage | 0.0055 cm/cm | 0.0055 in/in | restricted |
BASF Ultramid® A3HG6 HR BK 23591 30% Glass Filled PA66 (Dry) Description: 30% glass-fiber reinforced injection-molding grade with enhanced hydrolysis resistance, e.g., for applications in vehicle cooling systems.Information provided by BASF |
|||
Linear Mold Shrinkage | 0.0055 cm/cm | 0.0055 in/in | |
BASF Ultramid® A3WG5 25% Glass Filled PA66 (Conditioned) Ultramid A3WG5 is a 25% glass fiber reinforced and heat resistance injection molding PA66 grade. |
|||
Linear Mold Shrinkage | 0.0055 cm/cm | 0.0055 in/in | restricted |
BASF Ultramid® B35EG3 15% Glass Filled PA6 (Dry) Description: 15% glass-fiber reinforced injection-molding grade for gIT applications such as, for example, steering column switches, vehicle mirror housings and the wheels of mountain bikes.Informat.. |
|||
Linear Mold Shrinkage | 0.0055 cm/cm | 0.0055 in/in | restricted |
BASF Ultramid® B35EG3 BK 00564 15% Glass Filled PA6 (Dry) Description: 15% glass-fiber reinforced injection-molding grade for gIT applications such as, for example, steering column switches, vehicle mirror housings and the wheels of mountain bikes.Informat.. |
|||
Linear Mold Shrinkage | 0.0055 cm/cm | 0.0055 in/in | ASTM D955 |
Adell RR-14 Copolymer Polypropylene, 20% Glass Reinforced Data provided by Adell Plastics, Inc. |
|||
Linear Mold Shrinkage | 0.0055 cm/cm | 0.0055 in/in | |
Styron Magnum™ 9020 ABS, High Gloss MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM AB.. |