Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 78.0 µm/m-°C @Temperature 20.0 °C |
43.3 µin/in-°F @Temperature 68.0 °F |
ASTM data |
Americas Styrenics Styron® 8100 MFD High Impact Polystyrene
(discontinued **) STYRON 8100 MFD high impact polystyrene is designed for microfloppy diskettes (MFD) applications. It offers easy processing, coloring, abrasion resistance, impact strength, and high heat resistance... |
|||
CTE, linear, Parallel to Flow | 78.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
43.3 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP LUBRICOMP DP003EH PC LNP LUBRICOMP* DP003EH is a compound based on Polycarbonate resin containing 15% PTFE/Silicone. Added features of this material include: Easy Molding, Internally Lubricated, Healthcare. |
|||
CTE, linear, Parallel to Flow | 78.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
43.3 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP LUBRICOMP ZP001XXP PPE+PS LNP* LUBRICOMP* ZP001XXP is a compound based on PPE+PS resin containing 5% PTFE/Silicone. Added features of this material include: Wear Resistant. |
|||
CTE, linear, Parallel to Flow | 78.0 µm/m-°C @Temperature 20.0 °C |
43.3 µin/in-°F @Temperature 68.0 °F |
ISO data |
Styron Magnum™ 2642 ABS, Impact Grade MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
CTE, linear, Parallel to Flow | 78.0 µm/m-°C @Temperature 20.0 °C |
43.3 µin/in-°F @Temperature 68.0 °F |
ISO data |
Styron Magnum™ 342EZ ABS, Medium Impact MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
CTE, linear, Parallel to Flow | 78.0 µm/m-°C @Temperature 20.0 °C |
43.3 µin/in-°F @Temperature 68.0 °F |
ISO data |
Styron Magnum™ 780HP ABS, High Heat, High Impact MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
CTE, linear, Parallel to Flow | 78.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
43.3 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP STAT-KON KD000EI Acetal Copolymer (Europe-Africa-Middle East) LNP* Stat-Kon* KD000EI is a compound based on Acetal Copolymer resin containing Carbon Powder. Added features include: Electrically Conductive, Impact Modified. |
|||
CTE, linear, Parallel to Flow | 78.0 µm/m-°C @Temperature 20.0 °C |
43.3 µin/in-°F @Temperature 68.0 °F |
ISO data |
Styron Magnum™ 344HP ABS MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
CTE, linear, Parallel to Flow | 78.0 µm/m-°C @Temperature 20.0 °C |
43.3 µin/in-°F @Temperature 68.0 °F |
|
Eastman Eastar DN001 PCTG Copolyester ISO data as provided by the manufacturer, Eastman Chemical |
|||
CTE, linear, Parallel to Flow | 78.0 µm/m-°C @Temperature 20.0 °C |
43.3 µin/in-°F @Temperature 68.0 °F |
|
Covestro Bayblend® FR 3001 Polycarbonate + ABS Blend Key Features:Flame retarding agentUnfilledFlame retardantSuitable processing methods:Injection moldingInformation provided by Bayer Polymers.As of 1 September 2015, Bayer MaterialScience was separat.. |