Styron Magnumâ„¢ 1040 ABS, Very High impact

Category Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded
Manufacturer Styron
Trade Name Magnum™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Styron Magnumâ„¢ 1040 ABS, Very High impact.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM ABS resin are available in a wide range of melt flow rates, impact strength and heat resistance for both high and low gloss applications manufactured by injection molding, sheet or profile extrusion and thermoforming.The Automotive grades of MAGNUM ABS resins offer a wide range of gloss, viscosity, impact strength and heat properties for use in numerous automotive applications. Melt flow rates from 1 to 12 g/10 min, impact strengths from 130 to 590 J/m and heat distortion temperatures from 77.C to 90.C are available. Available primarily as natural plus concentrates, MAGNUM ABS resins are used in a wide variety of automotive applications including structural instrument panels, consoles, pillars and exterior trim parts requiring painting and plating.MAGNUM 1040 ABS resin is often suitable for applications requiring Izod impact strengths of 530 J/m. This low gloss, very high impact grade is one of the more viscous resins having a melt flow rate of about 2.2 g/10 min. and is often used in door sills and glove boxes.Data provided by Dow Chemical.This product line was spun off from Dow Chemical to Styron in 2010.
Physical Properties Metric English Comments
Density 1.04 g/cc
0.0376 lb/in³
ASTM Data
Linear Mold Shrinkage 0.0055 cm/cm
0.0055 in/in
Melt Flow 2.2 g/10 min

@Load 3.80 kg,
Temperature 230 °C
2.2 g/10 min

@Load 8.38 lb,
Temperature 446 °F
ASTM Data
Mechanical Properties Metric English Comments
Tensile Strength, Yield 41.4 MPa
6000 psi
ASTM Data
Elongation at Yield 2.8 %
2.8 %
ISO Data
Tensile Modulus 2.00 GPa
290 ksi
ASTM Data
Izod Impact, Notched 5.34 J/cm
10.0 ft-lb/in
ASTM Data
Charpy Impact Unnotched NB
NB
ISO Data
NB
NB
ISO Data, Low Temp
Charpy Impact, Notched 1.60 J/cm²
7.61 ft-lb/in²
ISO Data, Low Temp
6.30 J/cm²
30.0 ft-lb/in²
ISO Data
Impact Test 54.0 J

@Temperature 23.0 °C
39.8 ft-lb

@Temperature 73.4 °F
Instrumented Dart Total Energy
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 80.0 µm/m-°C

@Temperature 20.0 °C
44.4 µin/in-°F

@Temperature 68.0 °F
ISO data
Deflection Temperature at 0.46 MPa (66 psi) 93.0 °C
199 °F
Unannealed; ASTM Data
Deflection Temperature at 1.8 MPa (264 psi) 79.4 °C
175 °F
Unannealed; ASTM Data
Vicat Softening Point 107 °C
225 °F
Optical Properties Metric English Comments
Gloss 52.5 %
52.5 %
Gardner Gloss, 60°