Material Notes:
EMERGEâ„¢ PC 4630-10 advanced resin is formulated to supply both excellent ultraviolet stability and enhanced ignition resistance while maintaining excellent physical properties and processability. Applications: Information Technology Equipment Sockets, Plugs, and Switches Street Lights, Safety Lights, and Reflectors Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010.
Physical Properties Metric English Comments
Specific Gravity 1.20 g/cc
1.20 g/cc
ASTM D792
Linear Mold Shrinkage 0.0050 - 0.0070 cm/cm
0.0050 - 0.0070 in/in
ASTM D955
Melt Flow 10 g/10 min

@Load 1.20 kg,
Temperature 300 °C
10 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 123
123
ASTM D785
Tensile Strength, Ultimate 65.5 MPa
9500 psi
ASTM D638
Tensile Strength, Yield 60.7 MPa
8800 psi
ASTM D638
Elongation at Break 120 %
120 %
ASTM D638
Elongation at Yield 6.0 %
6.0 %
ASTM D638
Tensile Modulus 2.24 GPa
325 ksi
ASTM D638
Flexural Strength 100 MPa
14500 psi
ASTM D790
Flexural Modulus 2.41 GPa
350 ksi
ASTM D790
Izod Impact, Notched 8.76 J/cm
16.4 ft-lb/in
ASTM D256
Izod Impact, Unnotched NB
NB
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 68.4 µm/m-°C

@Temperature -40.0 - 82.2 °C
38.0 µin/in-°F

@Temperature -40.0 - 180 °F
ASTM D696
Hot Ball Pressure Test >= 125 °C
>= 257 °F
IEC 60335-1
Deflection Temperature at 0.46 MPa (66 psi) 144 °C
291 °F
annealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 127 °C
260 °F
unannealed; ASTM D648
140 °C
284 °F
annealed; ASTM D648
Vicat Softening Point 154 °C
309 °F
50°C/hr, 50N; ASTM D1525
UL RTI, Electrical 125 °C
257 °F
UL 746
UL RTI, Mechanical with Impact 105 °C
221 °F
UL 746
UL RTI, Mechanical without Impact 125 °C
257 °F
UL 746
Flammability, UL94 V-2
V-2
0.0625 in
V-0
V-0
0.125 in
Oxygen Index 41 %
41 %
ASTM D2863
Glow Wire Test 960 °C

@Thickness 2.00 mm
1760 °F

@Thickness 0.0787 in
IEC 60695-2-10
Optical Properties Metric English Comments
Transmission, Visible 84 - 88 %
84 - 88 %
ASTM D1003
Electrical Properties Metric English Comments
Dielectric Constant 3.0

@Frequency 100 - 1.00e+6 Hz
3.0

@Frequency 100 - 1.00e+6 Hz
ASTM D150
Dielectric Strength 16.7 kV/mm
425 kV/in
ASTM D149
Dissipation Factor 0.0010

@Frequency 100 Hz
0.0010

@Frequency 100 Hz
ASTM D150
0.0040

@Frequency 1e+6 Hz
0.0040

@Frequency 1e+6 Hz
ASTM D150
Comparative Tracking Index 250 V

@Thickness 2.00 mm
250 V

@Thickness 0.0787 in
IEC 60112