Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Solvay Technyl® C 217 Unfilled, Heat Stabilized, Impact Modified Nylon 6

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Heat Stabilized
Manufacturer Solvay
Trade Name Technyl®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Technyl® C 217 Unfilled, Heat Stabilized, Impact Modified Nylon 6.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Rhodia; Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 1.14 g/cc
0.0412 lb/in³
ISO 1183-A
Water Absorption 1.3 %
1.3 %
24 Hr.; ISO 62
Mechanical Properties Metric English Comments
Tensile Strength, Yield 85.01 MPa
12330 psi
ISO 527
Elongation at Break 100 %
100 %
ISO 527
Tensile Modulus 2.95 GPa
428 ksi
ISO 527
Flexural Strength 115 MPa
16700 psi
ISO 178
Flexural Modulus 2.90 GPa
421 ksi
ISO 178
Izod Impact, Notched (ISO) 4.49 kJ/m²
2.14 ft-lb/in²
ISO 180
Thermal Properties Metric English Comments
Melting Point 222 °C
432 °F
ISO 3146-C
Deflection Temperature at 1.8 MPa (264 psi) 80.0 °C
176 °F
ISO 75-2
Processing Properties Metric English Comments
Drying Temperature 80.0 °C
176 °F
Dehumidifying Dryer
Dry Time 3 - 4 hour
3 - 4 hour
Users viewing this material also viewed the following: