Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Solvay TECHNYLSTARâ„¢ SX 218 V50 PA6, 50% glass filled, Conditioned

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, 50% Glass Fiber Filled
Manufacturer Solvay
Trade Name TECHNYLSTAR™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay TECHNYLSTARâ„¢ SX 218 V50 PA6, 50% glass filled, Conditioned.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: TECHNYLSTARâ„¢ SX 218 V50 is based on a patented high flow polyamide 6 resin (Technylstar), heat stabilized, reinforced with 50% of glass fiber, for injection molding. This product is available in black color.Benefits: Due to its outstanding flow characteristics, the product allows more freedom in mould and part design versus a standard polyamide solutions.Available in: Asia Pacific, Europe and North AmericaRegulations compliance: Grades produced or imported in Europe comply with directive 453/2010/EC, which amends REACH directive 1907/2006/EC. This grade complies with RoHS directive 2002/95/EC. Unless specified, this grade is not suitable for food contact, medical devices or toy applications.Applications: It is used in a wide variety of industries. The product is particularly suitable for all applications where a high rigidity is required.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 1.55 g/cc
0.0560 lb/in³
ISO 1183/A
Mechanical Properties Metric English Comments
Tensile Strength at Break 162 MPa
23500 psi
ISO 527 Type 1A
Elongation at Break 4.0 %
4.0 %
ISO 527 Type 1A
Tensile Modulus 11.6 GPa
1680 ksi
ISO 527 Type 1A
Flexural Modulus 10.0 GPa
1450 ksi
ISO 178
Izod Impact, Notched (ISO) 22.0 kJ/m²
10.5 ft-lb/in²
ISO 180/1eA
Izod Impact, Unnotched (ISO) 100 kJ/m²
47.6 ft-lb/in²
ISO 180/1eU
Charpy Impact Unnotched 9.50 J/cm²
45.2 ft-lb/in²
ISO 179/1eU
Charpy Impact, Notched 2.00 J/cm²
9.52 ft-lb/in²
ISO 179/1eA
Processing Properties Metric English Comments
Moisture Content <= 0.20 %
<= 0.20 %