Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 22.0 kJ/m² | 10.5 ft-lb/in² | ISO 180 |
Polyplastic Armlen® PP MF 20-3IM Impact Modified Polypropylene Impact modified polypropylene composite materialInformation provided by PolyPlastic Group. |
|||
Izod Impact, Notched (ISO) | 22.0 kJ/m² | 10.5 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics Cycolac® MG47F ABS (Europe-Africa-Middle East) Multi-purpose, injection molding ABS providing a favorable balance of engineering properties. FDA compliant. |
|||
Izod Impact, Notched (ISO) | 22.0 kJ/m² | 10.5 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics Lexan® FST9436 PC Copolymer Medium viscosity opaque, low smoke, and OSU 65/65 compliant PC Copolymer |
|||
Izod Impact, Notched (ISO) | 22.0 kJ/m² @Temperature -30.0 °C |
10.5 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® HFD1212 PC Copolymer 18 MFR LEXAN High Flow Ductile Copolymer |
|||
Izod Impact, Notched (ISO) | 22.0 kJ/m² @Temperature -30.0 °C |
10.5 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® HFD1232 PC Copolymer (Asia Pacific) 18 MFR LEXAN High Flow Ductile Copolymer UV-stabilized, available in transparent colors only |
|||
Izod Impact, Notched (ISO) | 22.0 kJ/m² @Temperature -30.0 °C |
10.5 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Cycolac® EX58 ABS High impact ABS for sheet extrusion and blow molding applications. |
|||
Izod Impact, Notched (ISO) | 22.0 kJ/m² | 10.5 ft-lb/in² | ISO 180-1A |
Gromax BTE25-DN00N1 Nylon 6 (Dry) Information provided by Gromax Enterprises Corp. |
|||
Izod Impact, Notched (ISO) | 22.0 kJ/m² @Temperature 23.0 °C |
10.5 ft-lb/in² @Temperature 73.4 °F |
80x10x4mm, r=0.25; V-notch; ISO 180/1A |
SYNTHOS Forsan® 573 Acrylonitrile Butadiene Styrene (ABS) Increased heat resistant, glossy, good mechanical properties, suitable for electroplating.Applications: Electrotechnics, automotiveHousehold appliances, electric switches, car interior parts, profil.. |
|||
Izod Impact, Notched (ISO) | 22.0 kJ/m² | 10.5 ft-lb/in² | Low Temp; ISO 180 |
Solvay Technyl® A 246M Nylon 66, Impact Grade, EH0 Unreinforced and modified polyamide 66, with improved impact resistance, heat stabilized, for injection molding.Technyl A 246m offers an excellent notched impact resistance at low temperatures makin.. |
|||
Izod Impact, Notched (ISO) | 22.0 kJ/m² | 10.5 ft-lb/in² | ISO 180/1eA |
Solvay TECHNYL® C 548B V15 Black PA6, 15% glass filled, Conditioned Description: Polyamide PA6, reinforced with 15% of glass fiber, heat stabilized, height viscosity, for extrusion-blowing.Available in: Asia Pacific and North AmericaProduct Applications: TECHNYL C 5.. |
|||
Izod Impact, Notched (ISO) | 22.0 kJ/m² | 10.5 ft-lb/in² | ISO 180/1eA |
Solvay TECHNYLSTARâ„¢ SX 216 V50 PA6, 50% glass filled, Conditioned Description: TECHNYLSTAR Polyamide, reinforced with 50% of glass fiber, characterized by a high fluidity of the melt, for injection molding.Available in: Asia Pacific, Europe and North America Produ.. |
|||
Izod Impact, Notched (ISO) | 22.0 kJ/m² | 10.5 ft-lb/in² | ISO 180/1eA |
Solvay TECHNYLSTARâ„¢ SX 216 V60 PA6, 60% glass filled, Conditioned Description: TECHNYL STAR TM Polyamide reinforced with 60% of glass fiber, for injection molding. Characterized by a high fluidity of the melt.Available in: Europe and North America Product Applicat.. |
|||
Izod Impact, Notched (ISO) | 22.0 kJ/m² | 10.5 ft-lb/in² | ISO 180/1eA |
Solvay TECHNYLSTARâ„¢ SX 218 L2 V60 Black JA6A PA6, 60% glass filled, Conditioned Description: TECHNYLSTAR polyamide reinforced with 60% of glass fiber, heat and UV stabilized, characterized by a high fluidity of the melt, for injection molding.Available in: Europe Product Applic.. |
|||
Izod Impact, Notched (ISO) | 22.0 kJ/m² | 10.5 ft-lb/in² | ISO 180/1eA |
Solvay TECHNYLSTARâ„¢ SX 218 V50 PA6, 50% glass filled, Conditioned Description: TECHNYLSTARâ„¢ SX 218 V50 is based on a patented high flow polyamide 6 resin (Technylstar), heat stabilized, reinforced with 50% of glass fiber, for injection molding. This product i.. |
|||
Izod Impact, Notched (ISO) | 22.0 kJ/m² | 10.5 ft-lb/in² | ISO 180/1eA |
Solvay TECHNYLSTARâ„¢ SX 218 V60 Black Z PA6, 60% glass filled, Conditioned Description: TECHNYLSTAR Polyamide reinforced with 60% of glass fiber, heat stabilized, for injection molding. Characterized by a high fluidity of the melt. Available in: Asia Pacific, Europe and No.. |
|||
Izod Impact, Notched (ISO) | 22.0 kJ/m² | 10.5 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP THERMOTUF VF004S SUPER TOUGH NYLON (Europe-Africa-Middle East) LNP* THERMOTUF* VF004S is a compound based on Super Tough Nylon resin containing Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
Izod Impact, Notched (ISO) | 22.0 kJ/m² | 10.5 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics NORYL GTX GTX989 PPE+PA (Asia Pacific) NORYL GTX989 is a conductive and high heat material, especially designed for in- and on-line painted bodypanels and fenders in particular. This material combines impact performance with conductivity.. |
|||
Izod Impact, Notched (ISO) | 22.0 kJ/m² | 10.5 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics NORYL GTX GTX989 PPE+PA (Europe-Africa-Middle East) NORYL GTX989 is a conductive and high heat material, especially designed for in- and on-line painted bodypanels and fenders in particular. This material combines impact performance with conductivity.. |
|||
Izod Impact, Notched (ISO) | 22.0 kJ/m² | 10.5 ft-lb/in² | GB/T 1843-2008 |
Sichuan Deyang Haton® hXGR41 Polyphenylene Sulfide Injection molding, high strengthInformation provided by Sichuan Deyang Chemical Co., LTD |
|||
Izod Impact, Notched (ISO) | 22.0 kJ/m² | 10.5 ft-lb/in² | ASTM D 256 |
Lubrizol Telene 1620 A/BK Dicyclopentadiene (DCPD) Telene® is a two-component system based on extra-high purity dicyclopentadiene (DCPD). Telene® is processed using a standard high-pressure RIM Equipment (Reaction Injection Molding). Telene® resu.. |
|||
Izod Impact, Notched (ISO) | 22.0 kJ/m² | 10.5 ft-lb/in² | ISO 180 |
A. Schulman FORMION™ FI 394 Ionomer Information provided by A. Schulman. |
|||
Izod Impact, Notched (ISO) | 22.0 kJ/m² | 10.5 ft-lb/in² | ISO 180/1A |
Chi Mei Polylac® PA-746 ABS - High Flow High flow, medium impact |
|||
Izod Impact, Notched (ISO) | 22.0 kJ/m² | 10.5 ft-lb/in² | 50%RH; ISO 180/1A |
DuPont Performance Polymers Zytel® 73G30T BK261 Nylon 6
(Unverified Data**) 30% Glass Reinforced Toughened Polyamide 6 Zytel 73G30T BK261 is a 30% glass fiber reinforced toughened black polyamide 6 resin for injection molding.Information provided by DuPont Performance Polym.. |
|||
Izod Impact, Notched (ISO) | 22.0 kJ/m² | 10.5 ft-lb/in² | Conditioned; ISO 180/1A |
Addiplast Addinyl C2 V40 Nylon 66/6, 40% Glass Filled Glass fiber reinforced, high strengthInformation provided by Addiplast. |
|||
Izod Impact, Notched (ISO) | 22.0 kJ/m² | 10.5 ft-lb/in² | ISO 180/1A |
Chi Mei Polylac® PA-763A ABS - Flame Retardant F.R. High Heat |
|||
Izod Impact, Notched (ISO) | 22.0 kJ/m² | 10.5 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics NORYL PX1005X PPE+PS PPE+PS blend. Unfilled. Non-brominated, non-chlorinated FR system. UL94 V0/5VA rated. UL746C F1. Excelent dielectric strength. Suitable for E/E market in indoor/outdoor applications. |
|||
Izod Impact, Notched (ISO) | 22.0 kJ/m² | 10.5 ft-lb/in² | Conditioned; ISO 180/1A |
Addiplast Addinyl B2 ZV30 Nylon 6, 30% Glass Filled Glass fiber reinforced, increased thermal aging stabilityInformation provided by Addiplast. |
|||
Izod Impact, Notched (ISO) | 22.0 kJ/m² | 10.5 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP STAT-KON MFD03 PP LNP* STAT-KON* MFD03 is a compound based on Polypropylene resin containing 15% Glass Fiber. Added features of this material include: Electrically Conductive. |
|||
Izod Impact, Notched (ISO) | 22.0 kJ/m² | 10.5 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP STAT-KON MFD03 PP (Asia Pacific) LNP* Stat-kon* MFD03 is a compound based on Polypropylene resin containing Glass Fiber, Carbon Powder. Added features of this material include: Electrically Conductive. |
|||
Izod Impact, Notched (ISO) | 22.0 kJ/m² @Temperature -30.0 °C |
10.5 ft-lb/in² @Temperature -22.0 °F |
|
Polimeri Europa KOBLEND PCA 447F PC+ABS
(discontinued **) Symbol according to ISO 1043/1: PC+ABS Similar to KOBLEND PCA 447 with improved fluidity and release, suitable to mould complex items.Unfilled. Suitable for Injection Molding. Supplied as pellets.. |