Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 11.6 GPa @Temperature 23.0 °C |
1680 ksi @Temperature 73.4 °F |
ISO 527-2/1 |
PolyOne Bergamid™ A70 G30 U Polyamide 66 (Nylon 66) Information provided by PolyOne |
|||
Tensile Modulus | 11.6 GPa @Temperature 23.0 °C |
1680 ksi @Temperature 73.4 °F |
DAM; ISO 527 |
DuPont Performance Polymers Zytel® HTN 52G35HSL BK083 Polyphthalamide (PPA)
(Unverified Data**) Zytel® HTN52G35HSL BK083 is a 35% glass reinforced, heat stabilized, lubricated high performance polyamide resin that can be molded in water heated molds. It is also a PPA resin.Information provid.. |
|||
Tensile Modulus | 11.6 GPa | 1680 ksi | ISO 527 |
Solvay Specialty Polymers Amodel® A-1340 HS Polyphthalamide (PPA) Resin, 40% Mineral/Glass Reinforced, Dry as Molded
&a AMODEL® A-1340 HS is a 40% mineral/glass reinforced, heat stabilized polyphthalamide (PPA) which exhibits a high deflection temperature, high flexural modulus, high tensile strength and low warpage.. |
|||
Tensile Modulus | 11.6 GPa | 1680 ksi | |
Idemitsu Kosan Xarec® EA 537 SPS, 30% Glass Filled Crystalline Polymer, Glass Filled, Ignition Resistant, Impact Modified. Used in Electronic and Electrical applications |
|||
Tensile Modulus | 11.6 GPa | 1680 ksi | ISO 527-1/-2 |
Kuraray Genestarâ„¢ G1352A-M41 Nylon, 35% Glass Filled Low friction reinforced injection grade.Main Features:Low friction coefficientAbrasion resistanceExamples of applications:Friction and wear applicationGear and wheel |
|||
Tensile Modulus | 11.6 GPa | 1680 ksi | ISO 527 Type 1A |
Solvay TECHNYLSTARâ„¢ SX 216 V50 PA6, 50% glass filled, Conditioned Description: TECHNYLSTAR Polyamide, reinforced with 50% of glass fiber, characterized by a high fluidity of the melt, for injection molding.Available in: Asia Pacific, Europe and North America Produ.. |
|||
Tensile Modulus | 11.6 GPa | 1680 ksi | ISO 527 Type 1A |
Solvay TECHNYLSTARâ„¢ SX 218 V50 PA6, 50% glass filled, Conditioned Description: TECHNYLSTARâ„¢ SX 218 V50 is based on a patented high flow polyamide 6 resin (Technylstar), heat stabilized, reinforced with 50% of glass fiber, for injection molding. This product i.. |
|||
Tensile Modulus | 11.6 GPa | 1680 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics ULTEM SF2350 PEI Blend High flow Ultem blends for thin wall application |
|||
Tensile Modulus | 11.6 GPa | 1680 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics ULTEM SF2350 PEI Blend (Asia Pacific) High flow Ultem blends for thin wall application |
|||
Tensile Modulus | 11.6 GPa | 1680 ksi | 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Ultem SF2350 PEI Blend (Europe-Africa-Middle East) High flow Ultem blends for thin wall applicationThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Tensile Modulus | 11.6 GPa | 1680 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Valox® ENH4565 PBT (Asia Pacific) 33% GF reinforced, Non-Brominated & Non-Chlorinated Flame Retardant, PBT resin, Good thermal shock resistance and low CTE. |
|||
Tensile Modulus | 11.6 GPa | 1680 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Valox® ENH4565 PBT (Europe-Africa-Middle East) 33% GF reinforced, Non-Brominated & Non-Chlorinated Flame Retardant, PBT resin, Good thermal shock resistance and low CTE. |
|||
Tensile Modulus | 11.6 GPa | 1680 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP UF006AS PPA LNP THERMOCOMP* UF006AS is a compound based on Polyphthalamide resin containing 30% Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
Tensile Modulus | 11.6 GPa | 1680 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Valox® EXVX1403 PBT (Asia Pacific) 33% GF reinforced, Non-Brominated & Non-Chlorinated Flame Retardant, PBT resin, Good thermal shock resistance and low CTE. |
|||
Tensile Modulus | 11.6 GPa | 1680 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP PF008QS PA 6 LNP THERMOCOMP* PF008QS is a compound based on Nylon 6 resin containing 40% Glass Fiber. Added features of this material include: Heat Stabilized, Reduced Moisture. |
|||
Tensile Modulus | 11.6 GPa | 1680 ksi | ASTM D638 |
Plenco 1501 Polyester, Briquette, Transfer Molded PLENCO 01501 is a general purpose, mineral filled granular polyester molding compound, offering excellent arc and track resistance properties, low post shrinkage, and improved mechanical strength va.. |
|||
Tensile Modulus | 11.6 GPa | 1680 ksi | ASTM D638 |
Plenco 3303 Phenolic, Granular, Compression Molded Plenco 03303 is a renumber of Plaslok 5303. Plenco 03303 is a two-stage, mineral and flock-filled phenolic molding compound offering excellent electrical insulating properties. It can be processed b.. |
|||
Tensile Modulus | 11.6 GPa | 1680 ksi | ASTM D638 |
Westlake Plastics Zelux® 40% GF Polycarbonate 40% Glass Filled Zelux polycarbonate is a transparent engineering plastic with excellent dimensional stability and good mechanical and electrical properties. It is used for structural applications when clarity and .. |
|||
Tensile Modulus | 11.6 GPa | 1680 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® BG-40 S PA6-GF40 Product description: Grilon BG-40 S is a normal viscosity PA 6 injection molding type with 40% glass fibers. Grilon BG-40 S has the following important properties: High stiffnessExcellent surface fi.. |
|||
Tensile Modulus | 11.6 GPa | 1680 ksi | ISO 527-1/-2 |
DuPont Performance Polymers Crastin® SK695FR NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**)&l 30% Glass Reinforced Flame Retardant Polybutylene Terephthalate Crastin® SK695FR is a 30% glass reinforced flame retardant polybutylene terephthalate for injection moulding.Information provided b.. |
|||
Tensile Modulus | 11.6 GPa | 1680 ksi | 1 mm/min; ISO 527 |
Eurostar Starflam PF0023E PA6, Glass Fiber Filled, Flame Retardant, Injection Molded Starflam PF0023E is a Mineral Flame Retardant, Halogen Free, Red Phosphorous Free, Glass Fiber Reinforced, Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |
|||
Tensile Modulus | 11.6 GPa @Temperature -40.0 °C |
1680 ksi @Temperature -40.0 °F |
ISO Data |
BASF Ultramid® 8233G HS 33% Glass Filled PA6 (Conditioned) Ultramid 8233G HS is a heat stabilized, 33% glass fiber reinforced nylon 6 molding compound offering excellent strength, stiffness, high temperature performance and dimensional stability. It is also.. |
|||
Tensile Modulus | 11.6 GPa | 1680 ksi | ISO 527-2 |
Ascend Performance Materials Vydyne® R535 Nylon 66, 35% Glass Reinforced, DAM Vydyne® R535 is general-purpose, hydrolysis-resistant, 35% glass-fiber reinforced PA66 resin. This product is lubricated for improved flow and offers superior surface appearance. Glass-reinforced V.. |
|||
Tensile Modulus | 11.6 GPa | 1680 ksi | ISO 527-2 |
Ascend Performance Materials Vydyne® R535H NT651 Nylon 66, 35% Glass Reinforced, DAM Vydyne® R535H NT651 is 35% glass-fiber reinforced PA66 resin. Available in natural, it is heat-stabilized with an electrically neutral heat stabilizer. It is designed specially for electrical appli.. |
|||
Tensile Modulus | 11.6 GPa | 1680 ksi | 1[mm/min]; ISO 527-1/2 |
Akro-Plastic Akromid® A3 GF 35 (2421) PA 6.6 Dry, 35% Glass Filled AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat.. |
|||
Tensile Modulus | 11.6 GPa | 1680 ksi | DAM; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® HTN 52G35HSL BK083 Polyphthalamide (PPA)
(Unverified Data**) 35% Glass Reinforced PPA High Performance Polyamide Zytel HTN52G35HSL BK083 is a 35% glass reinforced heat stabilized lubricated high performance polyamide resin that can be molded in water heated m.. |
|||
Tensile Modulus | 11.6 GPa | 1680 ksi | ASTM D638 |
LNP Thermocomp® UF-1006 A HS Polyphthalamide, Glass Fiber Reinforcement
(discontinued **) Features: Heat StabilizedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are sti.. |
|||
Tensile Modulus | 11.58 GPa | 1680 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP 2X04505 ETFE LNP* THERMOCOMP* 2X04505 is a compound based on ETFE resin containing Proprietary Filler(s). |