Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Solvay TECHNYLSTARâ„¢ SX 216 V60 PA6, 60% glass filled, DRY

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, 60% Glass Fiber Filled
Manufacturer Solvay
Trade Name TECHNYLSTAR™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay TECHNYLSTARâ„¢ SX 216 V60 PA6, 60% glass filled, DRY.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: TECHNYL STAR TM Polyamide reinforced with 60% of glass fiber, for injection molding. Characterized by a high fluidity of the melt.Available in: Europe and North America Product Applications: TECHNYLSTAR TM SX 216 V60 is suitable for all applications where a high rigidity is required. Due to its outstanding flow properties, the material easily fills the mould and the surface aspect of the finished part is excellent. This product is available in natural.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 1.65 g/cc
0.0596 lb/in³
ISO 1183/A
Water Absorption 0.55 %

@Temperature 23.0 °C,
Time 86400 sec
0.55 %

@Temperature 73.4 °F,
Time 24.0 hour
ISO 62
Mechanical Properties Metric English Comments
Tensile Strength at Break 240 MPa
34800 psi
ISO 527 Type 1A
Elongation at Break 2.5 %
2.5 %
ISO 527 Type 1A
Tensile Modulus 21.0 GPa
3050 ksi
ISO 527 Type 1A
Flexural Modulus 19.0 GPa
2760 ksi
ISO 178
Izod Impact, Notched (ISO) 15.2 kJ/m²
7.23 ft-lb/in²
ISO 180/1eA
Izod Impact, Unnotched (ISO) 90.0 kJ/m²
42.8 ft-lb/in²
ISO 180/1eU
Charpy Impact Unnotched 8.50 J/cm²
40.4 ft-lb/in²
ISO 179/1eU
Charpy Impact, Notched 1.50 J/cm²
7.14 ft-lb/in²
ISO 179/1eA
Thermal Properties Metric English Comments
Melting Point 222 °C
432 °F
ISO 11357
Processing Properties Metric English Comments
Feed Temperature 220 - 225 °C
428 - 437 °F
Front Barrel Temperature 240 - 245 °C
464 - 473 °F
Mold Temperature 80.0 °C
176 °F
Drying Temperature 80.0 °C
176 °F
Moisture Content <= 0.20 %
<= 0.20 %
Descriptive Properties Value Comments
Compression Zone 235-240°C
Users viewing this material also viewed the following: