Processing Properties Metric English Comments
Front Barrel Temperature 240 - 250 °C
464 - 482 °F
NHEP Spectron™ E6046 Nylon 6, 15% Glass Fiber
Natural color. E6046 exhibits high rigidity and mechanical strength. It is suitable for wide range of applications. Property data measured at room temperature, 50% RH.Information provided by Bieglo..
Front Barrel Temperature 240 - 260 °C
464 - 500 °F
Celanese Celanex® 1632Z PBT, 15% Glass Reinforced  (Unverified Data**)
Celanex 1632Z is a general purpose, 15% fiberglass reinforced polybutylene terephthalate with a good balance of mechanical properties and processability.15% glass-fiber, improved impactInformation p..
Front Barrel Temperature 240 - 260 °C
464 - 500 °F
Celanese Celanex® 2003HR PBT  (Unverified Data**)
Celanex 2003HR is an unfilled polybutylene terephthalate which has an excellent hydrolysis resistance, mechanical properties and processabilityHydrolytically stable / injectionInformation provided b..
Front Barrel Temperature 240 - 260 °C
464 - 500 °F
Celanese Celanex® 2004-2 PBT  (Unverified Data**)
Celanex 2004-2 is an unfilled polyester that has an excellent combination of flowability and toughness. A typical application for Celanex 2004-2 is electrical connectors containing latches. Celanex ..
Front Barrel Temperature 240 - 260 °C
464 - 500 °F
Celanese Celanex® 2402 MT PBT, Medical Technology  (Unverified Data**)
Celanex 2402 MT Natural is an unreinforced PBT with improved flow that complies with the requirements of CFR 21 177.1660 of the Food and Drug Administration (FDA) and is listed in the Drug Master Fi..
Front Barrel Temperature 240 - 260 °C
464 - 500 °F
Celanese Celanex® 3300-2 PBT, 30% Glass Reinforced  (Unverified Data**)
Celanex 3300-2 is a general purpose, 30% glass reinforced, polybutylene terephthalate that offers a superior combination of mechanical, electrical, and thermal properties. This grade provides outsta..
Front Barrel Temperature 240 - 260 °C
464 - 500 °F
Celanese Vandar® 4612R PBT, 7% Glass Reinforced  (Unverified Data**)
Vandar 4612R is a high impact polyester alloy containing 7% glass. It possesses excellent impact properties as well as toughness and moldability. Dimensional stability, chemical resistance, and low ..
Front Barrel Temperature 240 - 260 °C
464 - 500 °F
Celanese Vandar® 4662Z PBT, 30% Glass Reinforced  (Unverified Data**)
Vandar 4662Zis a high impact polyester alloy which contains 30% glass fiber loading. It is characterized by toughness, dimensional stability, and high modulus. Good weatherability and moldability ar..
Front Barrel Temperature 240 - 250 °C
464 - 482 °F
Injection Molding
LG Chemical LUMAX GP5106FI PBT+ABS+GF10%, Flame Retardant
Description: Injection Molding Grade, PBT+ABS+GF10%, Flame Retardant, Impact Modified, Dimensional StabilityApplication: E&E (Switch)CAS: 9003-56-9, 68928-70-1, 65997-17-3, 24968-12-5, 9003-54-7 an..
Front Barrel Temperature 240 - 250 °C
464 - 482 °F
LG Chemical LUMAX HF-5306F High Flow PBT, 30% Polymer Alloy, Weather Resistant, Flame Retardant
LUMAX resins are a family of thermoplastic blends of polybutyleneterephthalate(PBT) and styrenic resins that combine the most desirable properties of both resins and fillers. They offer high heat r..
Front Barrel Temperature 240 - 250 °C
464 - 482 °F
LG Chemical Lupox® PBT-GP-2150 15% GFR PBT
Information provided by US distributor Polymer Technology and Services, LLC (PTS).
Front Barrel Temperature 240 °C
464 °F
Kraiburg TPE For-Tec E OC8OAN Thermoplastic Elastomer, Adhesion to PA
The AD/PAX/MR Series is recommended for two-component-seals in electronic applications and soft touch grips and handles of machine tools. The material provides an excellent resistance to skin oils, ..
Front Barrel Temperature 240 °C
464 °F
Kraiburg TPE THERMOLAST® K TC3MSB Thermoplastic Elastomer, Adhesion to PC, ABS, low hardness
The AD1 Series is recommended for applications with excellent adhesion to polar thermoplastics such as ABS, PC and PC/ABS. The compounds are available in natural and black colors. Typical applicatio..
Front Barrel Temperature 240 °C
464 °F
Kraiburg TPE THERMOLAST® K TC4MSZ Thermoplastic Elastomer, Adhesion to PC, ABS, low hardness
The AD1 Series is recommended for applications with excellent adhesion to polar thermoplastics such as ABS, PC and PC/ABS. The compounds are available in natural and black colors. Typical applicatio..
Front Barrel Temperature 240 °C
464 °F
Kraiburg TPE THERMOLAST® K TC6HAZ Thermoplastic Elastomer
The AD/POM Series is recommended for applications with excellent adhesion to POM. The compounds are available in natural and black colors. Typical applications: BumpersFunction and design elementsGr..
Front Barrel Temperature 240 °C
464 °F
Kraiburg TPE THERMOLAST® K TC6HBZ Thermoplastic Elastomer
The AD/POM Series is recommended for applications with excellent adhesion to POM. The compounds are available in natural and black colors. Typical applications: BumpersFunction and design elementsGr..
Front Barrel Temperature 240 °C
464 °F
Kraiburg TPE THERMOLAST® K TC8MLB Thermoplastic Elastomer, Adhesion to PC, ABS, low hardness
The AD1 Series is recommended for applications with excellent adhesion to polar thermoplastics such as ABS, PC and PC/ABS. The compounds are available in natural and black colors. Typical applicatio..
Front Barrel Temperature 240 °C
464 °F
Kraiburg TPE THERMOLAST® K TF5FMA Thermoplastic Elastomer, adhesion to PC, ABS, PETG
The FC/AD1 Series is recommended for applications with food contact providing excellent adhesion to polar thermoplastics such as PC, ABS and PETG. Typical applications:Function and design elementsGr..
Front Barrel Temperature 240 °C
464 °F
Kraiburg TPE THERMOLAST® K TF6FMA Thermoplastic Elastomer, adhesion to PC, ABS, PETG
The FC/AD1 Series is recommended for applications with food contact providing excellent adhesion to polar thermoplastics such as PC, ABS and PETG. Typical applications:Function and design elementsGr..
Front Barrel Temperature 240 °C
464 °F
Injection
Kraiburg TPE THERMOLAST® K TP6VCZ Thermoplastic Elastomer, Adhesion to PC, ABS, PETG, optimized compression set
The AD1/CS Series is recommended for applications with excellent adhesion to polar thermoplastics such as ABS, PC and PC/ABS as well as excellent compression set. The compounds are available in natu..
Front Barrel Temperature 240 °C
464 °F
Kraiburg TPE THERMOLAST® M TM5ADT Thermoplastic Elastomer, for medical and pharmaceutical technology
The MC/AD1 Series is recommended for applications requiring basic medical approvals such as USP Class VI, USP 661 and ISO 10993-4, -5, -10, -11. The series is characterized by excellent adhesion pro..
Front Barrel Temperature 240 °C
464 °F
Kraiburg TPE THERMOLAST® K TC4MSB Thermoplastic Elastomer, Adhesion to PC, ABS, low hardness
The AD1 Series is recommended for applications with excellent adhesion to polar thermoplastics such as ABS, PC and PC/ABS. The compounds are available in natural and black colors. Typical applicatio..
Front Barrel Temperature 240 - 250 °C
464 - 482 °F
Solvay Technyl® C 218 V50 50% Glass Filled, Heat Stabilized Nylon 6
Information provided by Rhodia; Rhodia has been acquired by Solvay.
Front Barrel Temperature 240 - 255 °C
464 - 491 °F
Solvay TECHNYL® C 30H1 V30 Natural/F PA6, 30% glass fiber, DRY
Description: Flame retardant polyamide PA6, reinforced with 30% of glass fiber, for injection molding.Available in: Asia Pacific, Europe, Latin America and North AmericaProduct Applications: This gr..
Front Barrel Temperature 240 - 255 °C
464 - 491 °F
Solvay TECHNYL® C 548B V15 Black PA6, 15% glass filled, DRY
Description: Polyamide PA6, reinforced with 15% of glass fiber, heat stabilized, height viscosity, for extrusion-blowing.Available in: Asia Pacific and North AmericaProduct Applications: TECHNYL C 5..
Front Barrel Temperature 240 - 250 °C
464 - 482 °F
Solvay Technyl® C216V25 25% Glass Filled Nylon 6
Information provided by Rhodia; Rhodia has been acquired by Solvay.
Front Barrel Temperature 240 - 270 °C
464 - 518 °F
Zone 3
Eurostar Staramide BG5 PA6, 25% Glass Filled, Injection Molded
BG5 is a 25% Glass Fiber Reinforced Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier.
Front Barrel Temperature 240 - 270 °C
464 - 518 °F
Zone 3
Eurostar Staramide PF004EUC PA6, 20% Glass Filled, Injection Molded
PF004EUC is a 20% Glass Fiber Reinforced Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier.
Front Barrel Temperature 240 - 260 °C
464 - 500 °F
Celanese Celanex® 3100 7.5% Fiberglass Reinforced Polybutylene Terephthalate
Description: Celanex 3100 is a general purpose, 7.5% glass reinforced polybutylene terephthalate with a good balance of mechanical properties and processability. Celanex 3100 is a high flow material..
Front Barrel Temperature 240 - 255 °C
464 - 491 °F
Celanese Celanex® 3214 15% Fiberglass Reinforced Polybutylene Terephthalate
Description: Celanex 3214 is a non-exuding (UL approved V-0 at 1/32 inch), 15% fiberglass reinforced polybutylene terephthalate which has an excellent balance of mechanical properties and processabi..
Copyright © lookpolymers.com All Rights Reserved