Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched (ISO) | 90.0 kJ/m² @Temperature 23.0 °C |
42.8 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP Faradex DS0026 PC (Europe-Africa-Middle East) LNP* Faradex* DS0026 is a compound based on Polycarbonate resin containing Flame Retardant, Stainless Steel Fiber. Added features include: EMI/RFI Shielding, Flame Retardant, Non-Brominated & Non-C.. |
|||
Izod Impact, Unnotched (ISO) | 90.0 - 96.0 kJ/m² @Temperature -30.0 - -30.0 °C |
42.8 - 45.7 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 92.0 kJ/m² Grade Count:3 |
Overview of materials for Nylon 66, 50% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 50% Glass Fiber Filled". Specific grades with glass content between 45% and 54% are included. .. |
|||
Izod Impact, Unnotched (ISO) | 90.0 kJ/m² | 42.8 ft-lb/in² | cond.; ISO 180-1U |
Lanxess Durethan® BKV 15 H2.0 DUS008 901510 Nylon 6, Glass Fiber Reinforced PA 6, 15% glass fibers, injection molding, heat-aging stabilizedInformation provided by LANXESS. |
|||
Izod Impact, Unnotched (ISO) | 90.0 kJ/m² | 42.8 ft-lb/in² | ISO 180/1eU |
Solvay TECHNYLSTARâ„¢ SX 216 V50 PA6, 50% glass filled, DRY Description: TECHNYLSTAR Polyamide, reinforced with 50% of glass fiber, characterized by a high fluidity of the melt, for injection molding.Available in: Asia Pacific, Europe and North America Produ.. |
|||
Izod Impact, Unnotched (ISO) | 90.0 kJ/m² | 42.8 ft-lb/in² | ISO 180/1eU |
Solvay TECHNYLSTARâ„¢ SX 216 V60 PA6, 60% glass filled, DRY Description: TECHNYL STAR TM Polyamide reinforced with 60% of glass fiber, for injection molding. Characterized by a high fluidity of the melt.Available in: Europe and North America Product Applicat.. |
|||
Izod Impact, Unnotched (ISO) | 90.0 kJ/m² | 42.8 ft-lb/in² | ISO 180/1eU |
Solvay TECHNYLSTARâ„¢ SX 218 V50 PA6, 50% glass filled, DRY Description: TECHNYLSTARâ„¢ SX 218 V50 is based on a patented high flow polyamide 6 resin (Technylstar), heat stabilized, reinforced with 50% of glass fiber, for injection molding. This product i.. |
|||
Izod Impact, Unnotched (ISO) | 90.0 kJ/m² | 42.8 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP STAT-KON DD200C PC (Asia Pacific) PTFE free polycarbonate compounds with ESD safety and good lubricating perfomrance , suitable for Semiconductor and Hard Disk Drive (HDD) and semicon industry. Added features of this material includ.. |
|||
Izod Impact, Unnotched (ISO) | 90.0 kJ/m² | 42.8 ft-lb/in² | ISO 180 |
Solvay Specialty Polymers Omnix® 4050 Polyamide, High Performance (HPPA) (Dry) Omnix® 4050 is a 50% glass-fiber reinforced, high-performance polyamide (HPPA). It is particularly suited for replacing die-cast metal in a variety of mechanical applications and components used .. |
|||
Izod Impact, Unnotched (ISO) | 90.0 kJ/m² | 42.8 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP PF00C PA 6 (Europe-Africa-Middle East) LNP* THERMOCOMP* PF00C is a compound based on PA6 resin containing Glass Fiber. |
|||
Izod Impact, Unnotched (ISO) | 90.0 kJ/m² @Temperature 23.0 °C |
42.8 ft-lb/in² @Temperature 73.4 °F |
ISO 180/A |
Styron CALIBREâ„¢ 301-10 Polycarbonate Resin Overview: CALIBREâ„¢ 300-10 polycarbonate resins offer exceptional impact resistance, heat distortion resistance and optical clarity as well as high melt strength for blow molding and sheet appli.. |
|||
Izod Impact, Unnotched (ISO) | 90.0 kJ/m² | 42.8 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP UF009AS PPA (Europe-Africa-Middle East) LNP* Thermocomp* UF009AS is a compound based on Polyphthalamide resin containing Glass Fiber. |
|||
Izod Impact, Unnotched (ISO) | 90.0 kJ/m² | 42.8 ft-lb/in² | ISO 180/1eU |
Solvay TECHNYLSTARâ„¢ SX 218 L2 V60 Black JA6A PA6, 60% glass filled, DRY Description: TECHNYLSTAR polyamide reinforced with 60% of glass fiber, heat and UV stabilized, characterized by a high fluidity of the melt, for injection molding.Available in: Europe Product Applic.. |
|||
Izod Impact, Unnotched (ISO) | 90.0 kJ/m² @Temperature 23.0 °C |
42.8 ft-lb/in² @Temperature 73.4 °F |
ISO 180/A |
Styron CALIBREâ„¢ 303-10 Polycarbonate Resin Overview: CALIBREâ„¢ 300-10 polycarbonate resins offer exceptional impact resistance, heat distortion resistance and optical clarity as well as high melt strength for blow molding and sheet appli.. |
|||
Izod Impact, Unnotched (ISO) | 90.0 kJ/m² | 42.8 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP PF00CS PA 6 (Europe-Africa-Middle East) LNP* THERMOCOMP* PF00CS is a compound based on PA6 resin containing Glass Fiber. |
|||
Izod Impact, Unnotched (ISO) | 90.0 kJ/m² @Temperature 23.0 °C |
42.8 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP Verton PV00A PA 6 (Europe-Africa-Middle East) LNP* Verton* PV00A is a compound based on Nylon 6 resin containing Long Glass Fiber.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Izod Impact, Unnotched (ISO) | 90.0 kJ/m² | 42.8 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP VERTON RV00AES PA 66 (Europe-Africa-Middle East) LNP VERTON* RV00AES is a compound based on PA 66 resin containing Long Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized. |
|||
Izod Impact, Unnotched (ISO) | 90.0 kJ/m² @Temperature 23.0 °C |
42.8 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP Verton RV00AESM PA 66 (Europe-Africa-Middle East) LNP* VERTON* RV00AESM is a compound based on PA66 resin containing Long Glass Fiber. Added features include: Easy Moldin, Heat Stabilized.This data was supplied by SABIC-IP for the Europe-Africa-Mid.. |
|||
Izod Impact, Unnotched (ISO) | 90.0 kJ/m² | 42.8 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP VERTON RV00AESP PA 66 (Europe-Africa-Middle East) LNP* VERTON* RV00AESP is a compound based on PA66 resin containing Long Glass Fiber. Added features include : Easy Molding, Heat Stabilized. |
|||
Izod Impact, Unnotched (ISO) | 90.0 kJ/m² | 42.8 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP VERTON RV00AESS PA 66 (Europe-Africa-Middle East) LNP* VERTON* RV00AESS is a compound based on PA 66 resin containing Long Glass Fiber. Added features include; Easy Molding, Heat Stabilized. |
|||
Izod Impact, Unnotched (ISO) | 90.0 kJ/m² | 42.8 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP VERTON RV00AEU PA 66 (Europe-Africa-Middle East) LNP* VERTON* RV00AEU is a compound based on PA 66 resin containing Long Glass Fiber. Added features include : Easy Molding, UV Stabilized. |
|||
Izod Impact, Unnotched (ISO) | 90.0 kJ/m² | 42.8 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP VERTON RV00AEX5 PA6.6 (Europe-Africa-Middle East) LNP* VERTON* Is a compound based on PA66 resin containing Long Glass Fiber. Added features include: Easy Molding, Heat Stabilized. |
|||
Izod Impact, Unnotched (ISO) | 90.0 kJ/m² | 42.8 ft-lb/in² | 50%RH; ISO 180/1U |
DuPont Performance Polymers Zytel® 70G33L NC010 Nylon 66
(Unverified Data**) 33% Glass Reinforced Polyamide 66Zytel 70G33L NC010 is a 33% glass fiber reinforced polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Izod Impact, Unnotched (ISO) | 90.0 kJ/m² @Temperature -30.0 °C |
42.8 ft-lb/in² @Temperature -22.0 °F |
DAM; ISO 180/1U |
DuPont Performance Polymers Zytel® 73G30L NC010 Nylon 6
(Unverified Data**) 30% Glass Reinforced Polyamide 6Zytel 73G30L NC010 is a 30% glass fiber reinforced polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Izod Impact, Unnotched (ISO) | 90.0 kJ/m² | 42.8 ft-lb/in² | DAM; ISO 180/1U |
DuPont Performance Polymers Zytel® 8018HS NC010 Nylon 66
(Unverified Data**) 14% Glass Reinforced Toughened Heat Stabilized Polyamide 66 Zytel 8018HS NC010 is a 14% glass reinforced heat stabilized toughened polyamide 66 resin.Information provided by DuPont Performance Polym.. |
|||
Izod Impact, Unnotched (ISO) | 90.0 kJ/m² @Temperature -30.0 °C |
42.8 ft-lb/in² @Temperature -22.0 °F |
DAM; ISO 180/1U |
DuPont Performance Polymers Zytel® 8018HS NC010 Nylon 66
(Unverified Data**) 14% Glass Reinforced Toughened Heat Stabilized Polyamide 66 Zytel 8018HS NC010 is a 14% glass reinforced heat stabilized toughened polyamide 66 resin.Information provided by DuPont Performance Polym.. |
|||
Izod Impact, Unnotched (ISO) | 90.0 kJ/m² | 42.8 ft-lb/in² | 80x10x4; ISO 180/1U |
Eurostar Staramide PF00AE PA6, 50% Glass Fiber Filled, Injection Molded Staramide PF00AE is a 50% Glass Fiber Reinforced, Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |
|||
Izod Impact, Unnotched (ISO) | 90.0 kJ/m² | 42.8 ft-lb/in² | 80x10x4; ISO 180/1U |
Eurostar Staramide PF00AS PA6, 50% Glass Fiber Filled, Injection Molded Staramide PF00AS is a 50% Glass Fiber Reinforced, Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |
|||
Izod Impact, Unnotched (ISO) | 90.0 kJ/m² | 42.8 ft-lb/in² | ISO 180/1C |
Chi Mei Polylac® PA-707 ABS High gloss, high rigid |
|||
Izod Impact, Unnotched (ISO) | 90.0 kJ/m² | 42.8 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP VERTON RX06097 PA 66 (Europe-Africa-Middle East) LNP* VERTON* RX06097 is a compound based on PA 66 resin containing Long Glass Fiber. Added features include; Easy Molding, UV-Stabilized. |