Solvay TECHNYL® B 52 G1 MX 35 (XA 3004) PA66/6

Category Polymer , Thermoplastic , Nylon , Nylon 6/66
Manufacturer Solvay
Trade Name Technyl®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay TECHNYL® B 52 G1 MX 35 (XA 3004) PA66/6.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: TECHNYL B 52 G1 MX35 is a copolyamide 6.6/6 , with thermal protection, glow wire resistant and reinforced with mineral filler.Colors: GreyAvailable in: Latin AmericaMain Properties: ? Glow wire resistant, Dimensional stability, Stability at high temperatures, and Good finishing Applications: This product is indicated for pieces with low warping and good behavior at fire, as, for example, breakers and boxes of fusers.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 1.49 g/cc
0.0538 lb/in³
ISO 1183/A
Mechanical Properties Metric English Comments
Tensile Strength, Yield 75.0 MPa
10900 psi
ISO R 527
Elongation at Break 2.0 %
2.0 %
ISO R 527
Tensile Modulus 10.4 GPa
1510 ksi
ISO R 527
Flexural Strength 110 MPa
16000 psi
ISO 178
Flexural Modulus 6.00 GPa
870 ksi
ISO 178
Izod Impact, Notched (ISO) 3.00 kJ/m²
1.43 ft-lb/in²
ISO 180/1eA
Charpy Impact Unnotched 1.60 J/cm²
7.61 ft-lb/in²
ISO 179/1eU
Thermal Properties Metric English Comments
Melting Point 245 °C
473 °F
Glow Wire Test 960 °C

@Thickness 3.00 mm
1760 °F

@Thickness 0.118 in
CEI 695
Processing Properties Metric English Comments
Feed Temperature 260 - 270 °C
500 - 518 °F
Nozzle Temperature 250 - 270 °C
482 - 518 °F
Mold Temperature 60.0 - 100 °C
140 - 212 °F
Descriptive Properties Value Comments
Compression Zone 260-280°C
Mixing Zone 250-270°C