Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 245 °C | 473 °F | ISO 1135 7-1-3 |
Radici Radilon® CAHS (dry) Copolyamide 66/6 General purposeInformation provided by Radici group. |
|||
Melting Point | 245 °C | 473 °F | ISO 1135 7-1-3 |
Radici Radilon® CARV300 L (dry) Copolyamide 66/6 Glass-fiber reinforcedInformation provided by Radici group. |
|||
Melting Point | 245 °C | 473 °F | ISO 11357-1 |
Murtfeldt Murylat® Polyethylene Terephthalate Thanks to its extremely low absorption of moisture and low expansion coefficient, Murylat® is ideally suited for the processing of precision parts. Murylat® has an extremely high hardness grade an.. |
|||
Melting Point | 245 °C | 473 °F | Crystalline Peak Melting Point; ASTM D3418 |
Eastman Aqua 18696 PET
(discontinued **) Voridian Aqua thermoplastic polyesters are condensation polymers produced by a continuous melt-phase polymerization process followed by a solid-state polymerization process. Containers made from 186.. |
|||
Melting Point | 245 °C | 473 °F | ASTM D3418 |
Custom Resins Vexel™ E20GF45 , 45% Glass Reinforced PET
(discontinued **) Description: Vexel™ E20GF45 is a 45% glass fiber reinforced, general purpose PET. Information provided by Custom Resins. |
|||
Melting Point | 245 °C | 473 °F | ASTM D3418 |
Custom Resins Vexel™ E20MG35 , 35% Glass/Mica Reinforced PET
(discontinued **) Description: Vexel™ E20MG35 is a 20% glass fiber / 15% mica reinforced PET. Information provided by Custom Resins. |
|||
Melting Point | 245 °C | 473 °F | ASTM D3418 |
Custom Resins Vexel™ E20GF45 FR , 45% Glass Reinforced, Flame Retardant PET
(discontinued **) Description: Vexel™ E20GF45 FR is a 45% glass fiber reinforced, flame retardant PET. Information provided by Custom Resins. |
|||
Melting Point | 245 - 275 °C | 473 - 527 °F | Average value: 264 °C Grade Count:10 |
Overview of materials for Fluorinated Ethylene Propylene (FEP), Molded/Extruded This property data is a summary of similar materials in the MatWeb database for the category "Fluorinated Ethylene Propylene (FEP), Molded/Extruded". Each property range of values reported is minimu.. |
|||
Melting Point | 245 °C | 473 °F | 10°C/min; DAM; ISO 11357-1/-3 |
DuPont Performance Polymers Zytel® FE270038 BK267 Nylon 66
(Unverified Data**) Zytel® FE270038 is a 40% glass fiber/mineral reinforced, heat stabilized polyamid 66 for injection molding. It is well suited for water injection technology.Information provided by DuPont Performan.. |
|||
Melting Point | 245 °C | 473 °F | |
Solvay TECHNYL® B 52 G1 MX 35 (XA 3004) PA66/6 Description: TECHNYL B 52 G1 MX35 is a copolyamide 6.6/6 , with thermal protection, glow wire resistant and reinforced with mineral filler.Colors: GreyAvailable in: Latin AmericaMain Properties: ? G.. |
|||
Melting Point | 245 - 247 °C | 473 - 477 °F | |
SK Chemicals SKYPET® BL8050 Specially Formulated PET Copolymer Resin SKYPET-BL8050 is a specially formulated PET copolymer resin for PET bottles and extruded sheet. SKYPET-BL8050 provides excellent processability in injection molding and blow molding processes, offe.. |
|||
Melting Point | 245 °C | 473 °F | ISO 3146 |
Wellman Wellpet® PR109-N1 Unfilled PET Description: Unfilled PETInformation provided by Wellman. |
|||
Melting Point | <= 245 °C | <= 473 °F | Peak Melting Point; ExxonMobil method |
ExxonMobil Exceed™ 1018HA Metallocene Polyethylene Resin Product Description: Exceed 1018HA is a metallocene ethylene-hexene copolymer. Films made from Exceed 1018HA have outstanding tensile, impact strength and puncture. These superior strength propertie.. |
|||
Melting Point | <= 245 °C | <= 473 °F | Peak Melting Point; ExxonMobil method |
ExxonMobil Exceed™ 1018HA Metallocene Polyethylene Resin (European Grade) Product Description: Exceed 1018HA is a metallocene ethylene-hexene copolymers. Films are made of Exceed 1018HA have outstanding tensile, impact strength and puncture. These superior strength proper.. |
|||
Melting Point | 245 - 255 °C | 473 - 491 °F | |
Daikin NEOFLON NP-3000 FEP Pellets NEOFLON FEP molding materials are supplied as translucent white pellets for melt flow processes.Processing Methods: Extrusion.Applications: Ultra high speed wire and cable coatings.Information provi.. |
|||
Melting Point | 245 °C | 473 °F | 10 K/min |
BASF Petra® 110 BK-112 15% Glass Filled PET Petra 110 is a 15% glass fiber reinforced, black pigmented, polyethylene terephthalate injection molding compound. It exhibits a good combination of performance properties including good strength a.. |
|||
Melting Point | 245 °C | 473 °F | ASTM Test |
BASF Petra® 130 30% Glass Filled PET Petra 130 is a 30% glass fiber reinforced polyethylene terephthalate (PET) for injection molding applications. It exhibits a good combination of performance properties including high strength and s.. |
|||
Melting Point | 245 °C | 473 °F | 10 K/min |
BASF Petra® 130 BK-112 30% Glass Filled PET Petra 130 BK-112 is a 30% glass fiber reinforced, black pigmented polyethylene terephthalate injection molding compound. It exhibits a combination of performance properties including good strength .. |
|||
Melting Point | 245 °C | 473 °F | ASTM Test |
BASF Petra® 130 BK-112 30% Glass Filled PET Petra 130 BK-112 is a 30% glass fiber reinforced, black pigmented polyethylene terephthalate injection molding compound. It exhibits a combination of performance properties including good strength .. |
|||
Melting Point | 245 °C | 473 °F | 10 K/min |
BASF Petra® 130 FR 30% Glass Filled PET Petra 130 FR is a 30% glass fiber reinforced, flame retardant injection molding polyethylene terephthalate feedstocks. It is recognized as UL 94V-0/5VA by Underwriters Laboratories. It is also avail.. |
|||
Melting Point | 245 °C | 473 °F | ASTM Test |
BASF Petra® 130 FR BK-112 30% Glass Filled PET Petra 130 FR BK-112 is a 30% glass fiber reinforced, black pigmented, flame retardant injection molding compound based on post-consumer and post-industrial recycle polyethylene erephthalate feedstoc.. |
|||
Melting Point | 245 °C | 473 °F | ASTM Test |
BASF Petra® 140 45% Glass Filled PET Petra 140 is a 45% glass reinforced injection molding polyethylene terephthalate (PET) offering an increased level of strength, stiffness, high temperature performance and dimensional stability. Ex.. |
|||
Melting Point | 245 °C | 473 °F | 10 K/min |
BASF Petra® 140 BK-112 45% Glass Filled PET Petra 140 BK-112 is a 45% glass reinforced, pigmented black, polyethylene terephthalate (PET) injection molding compound offering an increased level of strength, stiffness, high temperature performa.. |
|||
Melting Point | 245 °C | 473 °F | ASTM D3418 |
BASF Petra® 7010 WT 7729 15% Glass Filled PET Description: Petra 7010 WT7729 is a 15% glass fiber reinforced, pigmented white injection molding compound based on post-consumer recycle polyethylene terephthalate. Formulated for superior surface .. |
|||
Melting Point | 245 °C | 473 °F | ASTM Test |
BASF Petra® 7030 GY6128 30% Glass Filled PET Petra 7030 GY6128 is a grey pigmented, high flow 30% glass fiber reinforced injection molding compound based on post-consumer and post-industrial recycled polyethylene terephthalate feedstock. It o.. |
|||
Melting Point | 245 °C | 473 °F | ISO 11357-1 |
Murtfeldt Murylat® SP Polyethylene Terephthalate Murylat® SP combines the properties of Murylat® with improved wear and friction characteristics. It also has increased dynamic resilience which, for example, significantly reduces the required dri.. |
|||
Melting Point | 245 °C | 473 °F | 10 K/min |
BASF Petra® 230 BK-112 22/13% Glass/Mineral Filled PET Petra 230 BK-112 is a 35% mineral and glass fiber reinforced, black pigmented, polyethylene terephthalate injection molding compound. It exhibits a very good combination of performance properties in.. |
|||
Melting Point | 245 °C | 473 °F | ASTM D3418 |
Ashley Polymers Ashlene® PE128 PET Polyester, 45% Glass Reinforced PET Polyester, with 45% glass reinforcement.Data provided by the manufacturer |
|||
Melting Point | 245 °C | 473 °F | ASTM D3418 |
Custom Resins Vexel™ E20GF30 FR , 30% Glass Reinforced, Flame Retardant PET
(discontinued **) Description: Vexel™ E20GF30 FR is a 30% glass fiber reinforced, flame retardant PET. Information provided by Custom Resins. |