Solvay TECHNYL® B 50 H1 PA66/6, Conditioned

Category Polymer , Thermoplastic , Nylon , Nylon 6/66
Manufacturer Solvay
Trade Name Technyl®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay TECHNYL® B 50 H1 PA66/6, Conditioned.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: TECHNYL® B 50H1 is an unreinforced melamine cyanurate flame retarded copolyamide 66/6. This product has been heat stabilized and is suitable for injection molding. This product is available in natural, black, and in other colors upon request. Benefits: This phosphorus and halogen free flame retardant grade, UL94 V0 at 0.4mm, offers excellent filling qualities together with good stiffness.Available in: Asia Pacific, Europe, Latin America and North AmericaRegulations compliance: Grades produced or imported in Europe comply with directive 453/2010/EC, which amends REACH directive 1907/2006/EC. This grade complies with RoHS directive 2002/95/EC. Unless specified, this grade is not suitable for food contact, medical devices or toy applications.Applications: Connectivity- junction blocks, terminal blocks, connectors…Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 1.16 g/cc
0.0419 lb/in³
ISO 1183/A
Mechanical Properties Metric English Comments
Tensile Strength at Break 40.0 MPa
5800 psi
ISO 527 Type 1A
Tensile Strength, Yield 40.0 MPa
5800 psi
ISO 527 type 1 A
Elongation at Break 100 %
100 %
ISO 527 Type 1A
Elongation at Yield 5.0 %
5.0 %
ISO 527 type 1 A
Tensile Modulus 2.20 GPa
319 ksi
ISO 527 Type 1A
Flexural Strength 70.0 MPa
10200 psi
ISO 178
Izod Impact, Notched (ISO) 6.50 kJ/m²
3.09 ft-lb/in²
ISO 180/1eA
Charpy Impact Unnotched NB
NB
ISO 179/1eU
Charpy Impact, Notched 0.550 J/cm²
2.62 ft-lb/in²
ISO 179/1eA
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
IEC 60093
Surface Resistance 1.00e+12 ohm
1.00e+12 ohm
IEC 60093
Dielectric Constant 4.0
4.0
IEC 60250
Dielectric Strength 30.0 kV/mm
762 kV/in
IEC 60243
Dissipation Factor 0.060
0.060
IEC 60250
Comparative Tracking Index 600 V
600 V
Solution A; IEC 60112
600 V
600 V
Solution B; IEC 60112
Processing Properties Metric English Comments
Moisture Content <= 0.20 %
<= 0.20 %