Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 6.50 kJ/m² @Temperature 23.0 °C |
3.09 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1A |
DuPont Performance Polymers Crastin® LW9320 BK851 PBT
(Unverified Data**) Crastin® LW9320 BK851 is a 20% glass fiber reinforced, black polybutylene terephthalate alloy for injection molding. It has improved surface aesthetics, excellent dimensional stability and low warp.. |
|||
Izod Impact, Notched (ISO) | 6.50 kJ/m² | 3.09 ft-lb/in² | ISO 180/A |
Victrex® HT™ P45 Polyetherketone Product Description: High performance thermoplastic material, unreinforced PolyEtherKetone (PEK), semi crystalline, coarse powder for extrusion
compounding, low flow, FDA food contact compliant, co.. |
|||
Izod Impact, Notched (ISO) | 6.50 kJ/m² @Temperature 23.0 °C |
3.09 ft-lb/in² @Temperature 73.4 °F |
ISO 180/A |
Victrex® PEEK 150FW30 PEEK, 30% Carbon Fibre/PTFE Reinforced Product Description:High performance thermoplastic material, 30% reinforced with carbon fibre / PTFE Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, easy flow, FDA fo.. |
|||
Izod Impact, Notched (ISO) | 6.50 kJ/m² | 3.09 ft-lb/in² | ISO 180 |
Iran Petrochemical (PCC) EPD 60 R Polypropylene EPD 60 R has a high molecular weight giving it superior toughness even at low temperature. It has excellent heat and detergent resistance.Applications: extrusion blow molding applications include t.. |
|||
Izod Impact, Notched (ISO) | 6.50 kJ/m² | 3.09 ft-lb/in² | ISO 180 |
Iran Petrochemical (PCC) S 30 S Polypropylene This grade is for general injection molding applications.Applications: textile bobbins ,wheels ,fittings ,closures ,caps.Information provided by Iran Petrochemical Commercial Co. |
|||
Izod Impact, Notched (ISO) | 6.50 kJ/m² | 3.09 ft-lb/in² | Sample Type A; ISO 180:2000 |
Global EPP PA 612 Copolymer Cast Polyamide 612 Cast nylons are generally accepted as the primary engineering polymer, suitable for virtually any plain bearing application. By varying the conditions of polymerisation the mechanical properties of .. |
|||
Izod Impact, Notched (ISO) | 6.50 kJ/m² | 3.09 ft-lb/in² | ISO 180 |
Iran Petrochemical (PCC) S 30 G Polypropylene The grade has combined excellent process ability with high stiffness.Applications: bags, mats, packing twines and ropes, drinking beakers packaging for dairy products.Information provided by Iran Pe.. |
|||
Izod Impact, Notched (ISO) | 6.50 kJ/m² | 3.09 ft-lb/in² | Type 1, Notch A; ISO 180 |
Solvay Specialty Polymers Amodel® AS-1566 HS Polyphthalamide (PPA), 65% GlassMineral (Dry) Amodel® AS-1566 HS resin is a 65% glass and mineral reinforced polyphthalamide (PPA) resin that exhibits a high deflection temperature and high flexural modulus. This grade was designed specifica.. |
|||
Izod Impact, Notched (ISO) | 6.50 kJ/m² | 3.09 ft-lb/in² | ISO 180/1A |
Solvay TECHNYL® A 218 MT15 V 25 Black 21N PA66, 25/15% glass/mineral fiber, Conditioned Description: Polyamide 66, reinforced with 25% of glass fiber and 15% of mineral filler, heat stabilized, for injection molding.Available in: Asia PacificProduct Applications: TECHNYL® A 218 MT15.. |
|||
Izod Impact, Notched (ISO) | 6.50 kJ/m² | 3.09 ft-lb/in² | ISO 180/1eA |
Solvay TECHNYL® B 50 H1 PA66/6, Conditioned Description: TECHNYL® B 50H1 is an unreinforced melamine cyanurate flame retarded copolyamide 66/6. This product has been heat stabilized and is suitable for injection molding. This product is av.. |
|||
Izod Impact, Notched (ISO) | 6.50 kJ/m² | 3.09 ft-lb/in² | ISO 180 |
Polyram PlusTek PA350M4 Nylon 6.6 for Injection Molding, 20% Mineral Reinforced 20% Mineral Reinforced Nylon 6.6 for injection molding applications.Information provided by Polyram. |
|||
Izod Impact, Notched (ISO) | 6.50 kJ/m² | 3.09 ft-lb/in² | ISO 180-93 |
Wellman Wellamid® GF25-66 XE-NBK1 25% Glass Fiber Reinforced, Engineering Grade Nylon 66 Description: Glass Fiber Reinforced, Engineering Grade Nylon 66Information provided by Wellman. |
|||
Izod Impact, Notched (ISO) | 6.50 kJ/m² | 3.09 ft-lb/in² | ASTM D256 |
Total PSI 2451 High Heat Resistance Impact Polystyrene Total Petrochemicals Polystyrene 2451 is a high heat resistance, impact polystyrene for injection blow molding, thermoforming. It is recommended for the manufacturing of articles which require good.. |
|||
Izod Impact, Notched (ISO) | 6.50 kJ/m² | 3.09 ft-lb/in² | ISO 180 |
Polyram RamTough PZ303G2 Polycarbonate, 10% Glass Fiber 10% glass fiber reinforced polycarbonate for injection molding applications.Information provided by Polyram. |
|||
Izod Impact, Notched (ISO) | 6.50 kJ/m² | 3.09 ft-lb/in² | ISO 180/1A |
DuPont Performance Polymers Crastin® LW9320 BK851 PBT+SAN
(Unverified Data**) 20% Glass Reinforced Polybutylene Terephthalate Blend with Low Warpage Characteristics Crastin LW9320 BK851 is a 20% glass fiber reinforced black polybutylene terephthalate blend for injection mold.. |
|||
Izod Impact, Notched (ISO) | 6.50 kJ/m² | 3.09 ft-lb/in² | ISO 180/1A |
Addiplast Addilene H 211 V20 Polypropylene Homopolymer Glass fiber reinforced, high modulus and improved stiffnessInformation provided by Addiplast. |
|||
Izod Impact, Notched (ISO) | 6.50 kJ/m² | 3.09 ft-lb/in² | ISO 180/1A |
Addiplast Addilene J 520 M20 Polypropylene Copolymer Mineral reinforced, improved rigidityInformation provided by Addiplast. |
|||
Izod Impact, Notched (ISO) | 6.50 kJ/m² | 3.09 ft-lb/in² | ISO 180/1A |
Addiplast Addilene J 522 M20 Polypropylene Copolymer Mineral reinforced, improved rigidityInformation provided by Addiplast. |
|||
Izod Impact, Notched (ISO) | 6.50 kJ/m² | 3.09 ft-lb/in² | ISO 180/A |
BASF Ultraform H 4320 Q600 POM Ultraform H4320 Q600 is an extrusion POM high molecular weight grade. This grade enables high extrusion rates with thick-walled product. It also exhibits high thermal stability and a low tendency .. |
|||
Izod Impact, Notched (ISO) | 6.50 kJ/m² | 3.09 ft-lb/in² | ISO Test |
BASF Ultraform N 2320 U03 UNC Q600 POM Ultraform N2320 U03 UNC Q600 is a rapidly freezing UV stabilized general-purpose injection molding grade. |
|||
Izod Impact, Notched (ISO) | 6.50 kJ/m² @Temperature 23.0 °C |
3.09 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1A |
BASF Ultramid® B3M6 BK 23213 30% Mineral Filled PA6 (Dry) Description: 30% Mineral-filled injection molding grade for high impact industrial items having very high dimensional stability, such as automobile wheel covers.Information provided by BASF |
|||
Izod Impact, Notched (ISO) | 6.50 kJ/m² | 3.09 ft-lb/in² | ISO 180/A |
BASF Ultrason® E 2010 G4 MR SW 15102 20% Glass Filled PESU Information provided by BASF |
|||
Izod Impact, Notched (ISO) | 6.50 kJ/m² | 3.09 ft-lb/in² | ISO 180/1A |
Addiplast Addinyl PMD 20117 Flame Retardant Nylon, Glass Filled Flame retardant, glass fiver reinforced, friction resistantInformation provided by Addiplast. |
|||
Izod Impact, Notched (ISO) | 6.50 kJ/m² | 3.09 ft-lb/in² | ISO 180/A |
BASF Ultrason E 2010 G4 20% Glass Filled PES Ultrason E 2010 G4 is a 20% glass reinforced, medium viscosity injection molding PES grade with high rigidity and strength. |
|||
Izod Impact, Notched (ISO) | 6.50 kJ/m² @Temperature -30.0 °C |
3.09 ft-lb/in² @Temperature -22.0 °F |
ISO 180/A |
BASF Ultrason E 2010 G4 20% Glass Filled PES Ultrason E 2010 G4 is a 20% glass reinforced, medium viscosity injection molding PES grade with high rigidity and strength. |
|||
Izod Impact, Notched (ISO) | 6.50 kJ/m² | 3.09 ft-lb/in² | ISO 180/A |
BASF Ultrason E 2010 PES Ultrason E 2010 is an unreinforced, medium viscosity standard injection molding PES grade. It flows readily and offers outstanding heat resistance and dimensional stability. It conforms to FDA req.. |
|||
Izod Impact, Notched (ISO) | 6.50 kJ/m² | 3.09 ft-lb/in² | ISO 180/1A |
Addiplast Addinyl B2 ZM30 Nylon 6, 30% Mineral Filled Mineral filled, increased thermal aging stabilityInformation provided by Addiplast. |
|||
Izod Impact, Notched (ISO) | 6.50 kJ/m² | 3.09 ft-lb/in² | ISO 180 |
BASF Nypel® 6030G HS DB BK 5830 30% Glass Filled PA6 (Dry) Description: Nypel® 6030G HS DB BK5830 is a 30% glass fiber reinforced, heat stabilized, black pigmented, injection molding compound based on recycled PA6..Application: Nypel® 6030G HS DB BK5830.. |
|||
Izod Impact, Notched (ISO) | 6.50 kJ/m² | 3.09 ft-lb/in² | ISO 180/A |
BASF Ultramid® B3M6 BK60564 30% Mineral Filled PA6 (Dry) ultramid B3M6 BK60564 is a 30% mineral reinforced, pigmented black injection molding PA6 grade for industrial items requiring high impact strength and very high dimensional stability, excellent lase.. |