Material Notes:
Description: TECHNYL® A 218 V35 Black 34 NG is a polyamide 66, reinforced with 35% of glass fiber, heat stabilized, for injection molding. The product is available in black color.Benefits: This product has been specially designed to improve its resistance to automotive cooling liquids, increasing lifetime of parts in permanent contact with such liquids.Available in: Europe and North AmericaRegulations compliance: Grades produced or imported in Europe comply with directive 453/2010/EC, which amends REACH directive 1907/2006/EC. This grade complies with RoHS directive 2002/95/EC. Unless specified, this grade is not suitable for food contact, medical devices or toy applicationsApplications: Cooling and heating radiator systems, header tanks, thermostat components, inlet & outlet pipes…Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 1.41 g/cc
0.0509 lb/in³
ISO 1183/A
Water Absorption 0.75 %

@Temperature 23.0 °C,
Time 86400 sec
0.75 %

@Temperature 73.4 °F,
Time 24.0 hour
ISO 62
Mechanical Properties Metric English Comments
Tensile Strength at Break 210 MPa
30500 psi
ISO 527 Type 1A
Elongation at Break 3.0 %
3.0 %
ISO 527 Type 1A
Tensile Modulus 12.0 GPa
1740 ksi
ISO 527 Type 1A
Izod Impact, Notched (ISO) 13.0 kJ/m²
6.19 ft-lb/in²
ISO 180/1eA
Charpy Impact Unnotched 9.50 J/cm²
45.2 ft-lb/in²
ISO 179/1eU
Charpy Impact, Notched 1.35 J/cm²
6.42 ft-lb/in²
ISO 179/1eA
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 22.0 µm/m-°C

@Temperature 23.0 - 85.0 °C
12.2 µin/in-°F

@Temperature 73.4 - 185 °F
ISO 11359
Melting Point 260 °C
500 °F
ISO 11357
Deflection Temperature at 1.8 MPa (264 psi) 255 °C
491 °F
ISO 75/Af
Flammability, UL94 HB

@Thickness 0.800 mm
HB

@Thickness 0.0315 in
1210
Oxygen Index 23 %
23 %
ISO 4589
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
IEC 60093
Surface Resistance 6.00e+14 ohm
6.00e+14 ohm
IEC 60093
Dielectric Strength 34.0 kV/mm
864 kV/in
IEC 60243
Dissipation Factor 0.010
0.010
IEC 60250
Comparative Tracking Index 600 V
600 V
Solution A; IEC 60112
Processing Properties Metric English Comments
Feed Temperature 260 - 270 °C
500 - 518 °F
Mold Temperature 70.0 - 100 °C
158 - 212 °F
Drying Temperature 80.0 °C
176 °F
Moisture Content <= 0.20 %
<= 0.20 %
Descriptive Properties Value Comments
Compression Zone 270-280°C
Mixing Zone 280-290°C