Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 210 MPa | 30500 psi | |
Plastcom SLOVAMID 6 GF 50 LS PA6, 50% glass fibre, light stability FeaturesPA 6 for injection moulding, chemically strengthened with 50% of glass fibre, for mouldings with high strength and toughness used in the automotive, electrical, engineering and consumer-good.. |
|||
Tensile Strength at Break | 210 MPa | 30500 psi | STN EN ISO 527-2 |
Plastcom SLOVAMID 6 GF 60 Polyamide 6, 60% Glass Fiber FeaturesPA 6 for injection moulding, chemically strengthened with 60% of glass fiber, for mouldings with high strength and toughness used in the automotive, electrical, engineering and consumer-good.. |
|||
Tensile Strength at Break | 210 MPa | 30500 psi | ISO 527 |
Nilit FRIANYL A63 GV35 Nylon 6.6 for injection molding, 35% glass fiber reinforced Nylon 6.6 for injection moldingInformation provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Tensile Strength at Break | <= 210 MPa | <= 30500 psi | ISO/R527 |
Polykemi AB SCANAMID 66 A12^ F50 Nylon 66, Glass Fiber Reinforced Information provided by Polykemi AB |
|||
Tensile Strength at Break | 210 MPa | 30500 psi | STN EN ISO 527-2 |
Plastcom SLOVAMID 6 GF 50 Polyamide 6, 50% Glass Fiber FeaturesPA 6 for injection moulding, chemically strengthened with 50% of glass fiber, for mouldings with high strength and toughness used in the automotive, electrical, engineering and consumer-good.. |
|||
Tensile Strength at Break | 210 MPa | 30500 psi | ISO 527 Type 1A |
Solvay TECHNYL® A 218 V35 PA66, 35% glass fiber, DRY Description: TECHNYL® A 218 V35 is a polyamide 66, reinforced with 35% of glass fiber, heat stabilized, for injection molding. This product is available in natural and black colors.Benefits: The .. |
|||
Tensile Strength at Break | 210 MPa | 30500 psi | |
SGL Carbon Group PANOX® FM C063 SSC Oxidized Textile Fiber, Crimped staple fiber, For felts and non-wovens PANOX® is the industry standard when it comes to fire-retardant textile fibers. As an oxidized, thermally stabilized polyacrylonitrile (PAN) fiber that will not burn, melt, soften or drip, PANOX .. |
|||
Tensile Strength at Break | 210 MPa | 30500 psi | |
SGL Carbon Group PANOX® SM T320 EEA Oxidized Textile Fiber, Continuous Tow with 320k filaments, For carbon/carbon and spinning PANOX® is the industry standard when it comes to fire-retardant textile fibers. As an oxidized, thermally stabilized polyacrylonitrile (PAN) fiber that will not burn, melt, soften or drip, PANOX .. |
|||
Tensile Strength at Break | 210 MPa | 30500 psi | ISO 527-2 |
Solvay Specialty Polymers Amodel® AE-4133 Polyphthalamide (PPA), 33% Glass Fiber (Dry) Amodel® AE-4133 is a 33% glass reinforced, hot-water moldable polyphthalamide (PPA) designed to work in the modern automotive electrical environment. Features: Good Chemical Resistance; Good Cree.. |
|||
Tensile Strength at Break | 210 MPa | 30500 psi | ISO 527-2 |
Solvay Specialty Polymers Amodel® AS-1935 HS Polyphthalamide (PPA), 35% Glass Fiber Amodel® AS-1935 HS is a 35% glass reinforced grade of polyphthalamide (PPA) resin developed specifically for improved performance in a 50/50 ethylene glycol and water environment. This material e.. |
|||
Tensile Strength at Break | 210 MPa | 30500 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Thermocomp RF00AES PA 66 (Europe-Africa-Middle East) LNP THERMOCOMP* RF00AES is a compound based on PA66 resin containing Glass Fiber, Mold Release.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Tensile Strength at Break | 210 MPa | 30500 psi | ISO 527-1/-2 |
DSM Stanyl® TW200F6 (DAM) Nylon 46 30% Glass Reinforced, Heat Stabilized (North America) Information provided by DSM Engineering Plastics. |
|||
Tensile Strength at Break | 210 MPa | 30500 psi | ISO 527-1/-2 |
DSM Stanyl® TW241F6 Nylon 46-30% Glass Reinforced, Heat Stabilized, Lubricated (Asian Grade) (Dry) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Tensile Strength at Break | 210 MPa | 30500 psi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® HTV-4H1 black 9205 PA6T/6I-GF40 Product description: Grivory HTV-4H1 black 9205 is a 40% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Acc. to ISO: PA 6T/6I... |
|||
Tensile Strength at Break | 210 MPa | 30500 psi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® XE 4105 nat PA610-GF50 Product description: Grilamid XE 4105 natural is a 50% glass fiber reinforced, heat stabilized polyamide 610 (PA610) injection molding grade. This product is to a large extent based on renewable raw.. |
|||
Tensile Strength at Break | 210 MPa | 30500 psi | DAM; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® 70G35HSRX BK099 Nylon 66
(Unverified Data**) 35% Glass Reinforced Heat Stabilized Polyamide 66 Zytel 70G35HSRX BK099 a 35% glass reinforced heat stabilized hydrolysis resistant PA66 for injection molding. Developed for applications designed fo.. |
|||
Tensile Strength at Break | 210 MPa | 30500 psi | 50%RH; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® 70G50HSLA BK039B Nylon 66
(Unverified Data**) 50% Glass Reinforced Heat Stabilized Polyamide 66 Information provided by DuPont Performance Polymers |
|||
Tensile Strength at Break | 210 MPa | 30500 psi | 50%RH; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® HTN 53G50LWSF BK702A Polyphthalamide (PPA)
(Unverified Data**) 50% Glass Reinforced High Performance Polyamide with Low Warpage and High Stiffness Information provided by DuPont Performance Polymers |
|||
Tensile Strength at Break | 210 MPa | 30500 psi | 5 mm/min; ISO 527 |
Eurostar Staramide AG10 PA66, 50% Glass Filled, Injection Molded AG10 is a 50% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
Tensile Strength at Break | 210 MPa | 30500 psi | ISO 527 |
Eurotec® Tecomid® NA40 GR40 NL HS PA6.6, 40% glass fiber reinforced, heat stabilized, natural Information provided by Eurotec® |
|||
Tensile Strength at Break | 210 MPa | 30500 psi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® GV-4H PA*-GF40 Product description: Grivory GV-4H natural is a 40% glass-fiber reinforced engineering thermoplastic material based on a combination of semicrystalline Polyamide with partially aromatic copolyamide... |
|||
Tensile Strength at Break | 210 MPa | 30500 psi | ISO R 527 |
Addiplast Addinyl A2 ZV40 Nylon 66, 40% Glass Filled Glass fiber reinforced, increased thermal aging stabilityInformation provided by Addiplast. |
|||
Tensile Strength at Break | 210 MPa | 30500 psi | 5 [mm/min]; ISO 527-2/5 |
Akro-Plastic Akromid® B3 GF 50 RM-M (3146) PA 6 Dry, 50% Glass Filled In all, the construction relevant features show that the significantly reduced moisture absorption of AKROMID B3 GF 30 RM leads to increasing rigidities and strengths as already expected. Neverthele.. |
|||
Tensile Strength at Break | 210 MPa | 30500 psi | 5 [mm/min]; ISO 527-1/2 |
Akro-Plastic Akromid® T1 GF 30 9 (3498) PPA Dry, 30% Glass Filled The new AKROMID® T is characterized primarily by high heat resistance and the lowest moisture absorption of the three PA grades, making it particularly well-suited in the automotive sector for high.. |
|||
Tensile Strength at Break | 210 MPa @Temperature -40.0 °C |
30500 psi @Temperature -40.0 °F |
ISO Data |
BASF Petra® 130 30% Glass Filled PET Petra 130 is a 30% glass fiber reinforced polyethylene terephthalate (PET) for injection molding applications. It exhibits a good combination of performance properties including high strength and s.. |
|||
Tensile Strength at Break | 210 MPa @Temperature -40.0 °C |
30500 psi @Temperature -40.0 °F |
ISO Data |
BASF Ultramid® 8233G HS BK-106 33% Glass Filled PA6 (Dry) Ultramid 8233G HS BK-106 is a heat stabilized, weather resistant, 33% glass fiber reinforced PA6 injection molding compound offering excellent strength, stiffness, high temperature
performance and .. |
|||
Tensile Strength at Break | 210 MPa | 30500 psi | 5 [mm/min]; ISO 527-2/5 |
Akro-Plastic Akromid® B3 GF 50 9 RM-M (3147) PA 6 Dry, 50% Glass Filled In all, the construction relevant features show that the significantly reduced moisture absorption of AKROMID B3 GF 30 RM leads to increasing rigidities and strengths as already expected. Neverthele.. |
|||
Tensile Strength at Break | 210 MPa | 30500 psi | ISO 527-1/-2 |
DSM Akulon® K224-HG8 (Dry) 40% Glass Reinforced Nylon 6 (North America)
(discontinued **) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
Tensile Strength at Break | 210 MPa | 30500 psi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® GV-4H black PA*-GF40 Product description: Grivory GV-4H black 9915 is a 40% glass fiber reinforced engineering thermoplastic material based on a combination of semicrystalline Polyamide with partially aromatic copolyami.. |
|||
Tensile Strength at Break | 210 MPa | 30500 psi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® HT1V-4 FWA nat PA6T/6I-GF40 Product description: Grivory HT1V-4 FWA natural is a 40 wt.-% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Acc. to ISO: PA 6.. |