Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Solvay TECHNYL® A 218 V35 Black 34 NG PA66, 35% glass fiber, Conditioned

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 40% Glass Fiber Filled
Manufacturer Solvay
Trade Name Technyl®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay TECHNYL® A 218 V35 Black 34 NG PA66, 35% glass fiber, Conditioned.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: TECHNYL® A 218 V35 Black 34 NG is a polyamide 66, reinforced with 35% of glass fiber, heat stabilized, for injection molding. The product is available in black color.Benefits: This product has been specially designed to improve its resistance to automotive cooling liquids, increasing lifetime of parts in permanent contact with such liquids.Available in: Europe and North AmericaRegulations compliance: Grades produced or imported in Europe comply with directive 453/2010/EC, which amends REACH directive 1907/2006/EC. This grade complies with RoHS directive 2002/95/EC. Unless specified, this grade is not suitable for food contact, medical devices or toy applicationsApplications: Cooling and heating radiator systems, header tanks, thermostat components, inlet & outlet pipes…Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 1.41 g/cc
0.0509 lb/in³
ISO 1183/A
Mechanical Properties Metric English Comments
Tensile Strength at Break 150 MPa
21800 psi
ISO 527 Type 1A
Elongation at Break 4.0 %
4.0 %
ISO 527 Type 1A
Tensile Modulus 8.70 GPa
1260 ksi
ISO 527 Type 1A
Izod Impact, Notched (ISO) 18.0 kJ/m²
8.57 ft-lb/in²
ISO 180/1eA
Charpy Impact Unnotched 10.0 J/cm²
47.6 ft-lb/in²
ISO 179/1eU
Charpy Impact, Notched 1.85 J/cm²
8.80 ft-lb/in²
ISO 179/1eA
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+13 ohm-cm
1.00e+13 ohm-cm
IEC 60093
Surface Resistance 1.00e+12 ohm
1.00e+12 ohm
IEC 60093
Dielectric Strength 29.0 kV/mm
737 kV/in
IEC 60243
Dissipation Factor 0.11
0.11
IEC 60250
Comparative Tracking Index 600 V
600 V
Solution A; IEC 60112
Processing Properties Metric English Comments
Moisture Content <= 0.20 %
<= 0.20 %
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved